Of the 'branded' glassware that I have,
I consider the order of quality to be;
Pyrex/Quickfit, (excellent but not perfect)
Kimble/Simax (good)
Bomex, (O.K. but thin glass)
GG-17, (prettiest Chinese glassware so far)
Lab Glass, (similar to Bomex)
Generic Chinese.
Based on almost no evidence, just my own perception,
I'd rather buy used Pyrex than new Bomex.
|