Assume I need a halocarbon with one halogen atom, that is liquid in room temperature. Chloroprene seems to fulfil this requirements. I wonder, if I
could try pyrolysis (depolymerization) of neoprene or whatever to obtain it.
blogfast25 - 9-6-2015 at 04:53
Anaerobic depolymerisation by pyrolysis is likely to yield stinky mess of chlorinated cyclics and aromatics with very little actual chloroprene.