Hello everybody!
Assume I need a halocarbon with one halogen atom, that is liquid in room temperature. Chloroprene seems to fulfil this requirements. I wonder, if I
could try pyrolysis (depolymerization) of neoprene or whatever to obtain it.
|
|
blogfast25
International Hazard
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
Anaerobic depolymerisation by pyrolysis is likely to yield stinky mess of chlorinated cyclics and aromatics with very little actual chloroprene.
|
|