Chemcraft - 16-8-2021 at 02:43
We offer Potassium metal 99.9% for sale. Packed in vacuum plastic bags.
Packing sizes from 10g to 2000g
Price for 100 gr - 28 USD
1 kg - 250 USD
Worldwide shipping (excluding Latin American countries)
Impurities content (weight %)
Chlorides (Cl-) <0.003
Sulfates (SO42-) <0.004
Iron (Fe) <0.001
Calcium (Ca) <0.02
Sodium (Na) <0.02
Silicon dioxide (SiO2) <0.015
Heavy metals (Pb) <0.001
Link to our internet store:
https://chemcraft.su
![k_kuski_-3.png - 350kB](https://www.sciencemadness.org/whisper/files.php?pid=664110&aid=89835)