Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: Potassium metal 99.9% (pure p.a.) for sale
Chemcraft
Hazard to Self
**




Posts: 98
Registered: 8-6-2017
Location: Russia
Member Is Offline

Mood: No Mood

[*] posted on 16-8-2021 at 02:43
Potassium metal 99.9% (pure p.a.) for sale


We offer Potassium metal 99.9% for sale. Packed in vacuum plastic bags.
Packing sizes from 10g to 2000g

Price for 100 gr - 28 USD
1 kg - 250 USD

Worldwide shipping (excluding Latin American countries)

Impurities content (weight %)
Chlorides (Cl-) <0.003
Sulfates (SO42-) <0.004
Iron (Fe) <0.001
Calcium (Ca) <0.02
Sodium (Na) <0.02
Silicon dioxide (SiO2) <0.015
Heavy metals (Pb) <0.001

Link to our internet store:
https://chemcraft.su