Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: copper (II) chloride
hello402
Harmless
*




Posts: 2
Registered: 10-5-2007
Member Is Offline

Mood: No Mood

[*] posted on 10-5-2007 at 21:41
copper (II) chloride


can copper (II) chloride solution oxidize a piece of bright copper wire?
View user's profile View All Posts By User
woelen
Super Administrator
*********




Posts: 8014
Registered: 20-8-2005
Location: Netherlands
Member Is Online

Mood: interested

[*] posted on 10-5-2007 at 22:44


Yes, it can, but only at high concentration of chloride ions.

At high concentration of chloride ions, you obtain the complex CuCl4(2-). This reacts with copper metal as follows:

Cu + CuCl4(2-) ---> 2CuCl2(-)

The CuCl2(-) ion is a colorless ion. The solutions, however, become very dark, due to a secondary reaction between the copper(I) and copper(II) species in solution, giving some dark mixed oxidation state complex.




The art of wondering makes life worth living...
Want to wonder? Look at https://woelen.homescience.net
View user's profile Visit user's homepage View All Posts By User
12AX7
Post Harlot
*****




Posts: 4803
Registered: 8-3-2005
Location: oscillating
Member Is Offline

Mood: informative

[*] posted on 11-5-2007 at 14:13


In response to elements of your OTHER thread, yes. The balanced reaction is CuCl2 + Cu = Cu2Cl2 (cuprous chloride, insoluble and white). At first, most of this is able to dissolve (darkening the solution as Woelen says), but eventually it saturates and Cu2Cl2 precipitates on the metal.

Tim




Seven Transistor Labs LLC http://seventransistorlabs.com/
Electronic Design, from Concept to Layout.
Need engineering assistance? Drop me a message!
View user's profile Visit user's homepage View All Posts By User This user has MSN Messenger
209
Harmless
*




Posts: 20
Registered: 23-1-2007
Member Is Offline

Mood: No Mood

[*] posted on 7-6-2007 at 11:32


The reaction is very slow. The trick is to speed it up. Use some H202 and add enough HCl to cover the copper chips and leave it overnight. Use some tweezers, pull out any remaining copper chips and simmer off the now dark greeny/black liquid. let the brown powder sit and it will gain moisture from the air on its own.
View user's profile View All Posts By User

  Go To Top