Author: Subject: Getting the Last of the Toluene out of the Product
JJay
International Hazard
*****




Posts: 3440
Registered: 15-10-2015
Member Is Offline


biggrin.gif posted on 9-2-2018 at 13:25
Getting the Last of the Toluene out of the Product


What is the best way to get toluene out of anhydrous oxalic acid? Ideally, I'd like to just stick it in my vacuum desiccator, but I have no idea what desiccant would absorb toluene, and it's kind of hard on the pump to run it for hours to pump off the toluene vapor.



View user's profile View All Posts By User
Cryolite.
Hazard to Others
***




Posts: 269
Registered: 28-6-2016
Location: CA
Member Is Offline

Mood: No Mood

[*] posted on 9-2-2018 at 14:34


Maybe try washing out the toluene in something that doesn't dissolve oxalic acid (DCM maybe) and then evap off the volatile wash? Kind of wasteful though.

View user's profile View All Posts By User
Texium
Administrator
********




Posts: 4738
Registered: 11-1-2014
Location: Salt Lake City
Member Is Offline

Mood: Seeking gainful employment

[*] posted on 9-2-2018 at 14:39


Pull a direct vacuum on it in a flask while gently heating with a heat gun or hot plate. Use a cold trap in between the flask and the pump.



Come check out the Official Sciencemadness Wiki
They're not really active right now, but here's my YouTube channel and my blog.
View user's profile Visit user's homepage View All Posts By User
j_sum1
Administrator
********




Posts: 6468
Registered: 4-10-2014
Location: At home
Member Is Offline

Mood: Most of the ducks are in a row

[*] posted on 9-2-2018 at 14:42


My inclination would be to crush it up and leave it in thae hot Australian sun for a while. Maybe double the time for the smell to be indiscernable. But, I confess I have no practical experience of this particular problem.

You are welcome to pop over and borrow some sun. It looks like we will have too much over the next few days.




View user's profile View All Posts By User
UC235
National Hazard
****




Posts: 565
Registered: 28-12-2014
Member Is Offline

Mood: No Mood

[*] posted on 9-2-2018 at 14:49


I believe shredded parrafin wax is the recommended "dessicant" for nonpolar hydrocarbon solvents.
View user's profile View All Posts By User
JJay
International Hazard
*****




Posts: 3440
Registered: 15-10-2015
Member Is Offline


[*] posted on 9-2-2018 at 15:07


Quote: Originally posted by UC235  
I believe shredded parrafin wax is the recommended "dessicant" for nonpolar hydrocarbon solvents.


Oh, thank you! I was considering shredded rubber, but I wasn't sure if that would work and didn't have any immediately available. Shredded wax sounds like an excellent idea!




View user's profile View All Posts By User
AvBaeyer
National Hazard
****




Posts: 659
Registered: 25-2-2014
Location: CA
Member Is Offline

Mood: No Mood

[*] posted on 9-2-2018 at 19:03


UC235 is correct. Shredded paraffin in a desiccator is very efficient for removing residual volatile hydrocarbons. I use this quite frequently for hexane and toluene. It does not really require a vacuum, just a bit of time.

AvB

[Edited on 10-2-2018 by AvBaeyer]
View user's profile View All Posts By User