thesmug
Hazard to Others
 
Posts: 370
Registered: 17-1-2014
Location: Chicago, Il (USA)
Member Is Offline
Mood: No Mood
|
|
Yellow gas from iron sulfide
Excuse this extremely beginner question but earlier today I was making some iron sulfide and as the reaction proceeded there was a yellow gas being
evolved. I know it's not sulfur dioxide or hydrogen sulfide so what was it?
|
|
plante1999
International Hazard
   
Posts: 1936
Registered: 27-12-2010
Member Is Offline
Mood: Mad as a hatter
|
|
vapors of sulphur.
I never asked for this.
|
|
Bert
Super Administrator
       
Posts: 2821
Registered: 12-3-2004
Member Is Offline
Mood: " I think we are all going to die. I think that love is an illusion. We are flawed, my darling".
|
|
How about a complete lab description? I have NO IDEA what chemicals you used or how your process was conducted?
Rapopart’s Rules for critical commentary:
1. Attempt to re-express your target’s position so clearly, vividly and fairly that your target says: “Thanks, I wish I’d thought of putting it
that way.”
2. List any points of agreement (especially if they are not matters of general or widespread agreement).
3. Mention anything you have learned from your target.
4. Only then are you permitted to say so much as a word of rebuttal or criticism.
Anatol Rapoport was a Russian-born American mathematical psychologist (1911-2007).
|
|
thesmug
Hazard to Others
 
Posts: 370
Registered: 17-1-2014
Location: Chicago, Il (USA)
Member Is Offline
Mood: No Mood
|
|
Sorry Bert, I mixed equal stoichiometric quantities of sulfur and iron filings. They were mixed thoroughly and put in a porcelain dish. The mixture
was heated by an alcohol flame until the sulfur melted. Heating was removed when the mixture began to glow. The mixture was cooled and collected until
testing could be done.
|
|
Zyklon-A
International Hazard
   
Posts: 1547
Registered: 26-11-2013
Member Is Offline
Mood: Fluorine radical
|
|
It's almost certainly airborne sulfur particles and vapors of sulfur.
[Edited on 13-4-2014 by Zyklonb]
|
|
elementcollector1
International Hazard
   
Posts: 2689
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline
Mood: Molten
|
|
Yep, sulfur. I remember seeing this stuff when I was working a blacksmithing forge that used genuine anthracite as a fuel source. We'd make so much
smoke that the archery range 100 feet upwind would complain of being blind.
Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
|
|