Author: Subject: Is that alumina or what ?
Hel
Harmless
*




Posts: 2
Registered: 23-2-2014
Member Is Offline

Mood: No Mood

[*] posted on 23-2-2014 at 11:26
Is that alumina or what ?


Hi, I'm new here, please be patient with me because I'm not an expert :)
Recently I dissolved some scrap Al in NaOH to make some sodium aluminate for
other experiments. When the mix cooled down I removed the excess unreacted Al
and I was left with a clear liquid (which should be a solution of NaAlO2) but also a lot of
very fine white powder as precipitate. I carefully filtered and collected the two
compounds and I dried the precipitate. I suppose it is alumina, but strangely enough
this powder does not react at all neither with strong HCl nor H2SO4, not even
with heat. Same thing by adding excess NaOH, it doesn't react. Any idea ???
I would like to make something useful out of it or understand what compound it
actually is... thanks !
View user's profile View All Posts By User
bfesser
Resident Wikipedian
Thread Moved
23-2-2014 at 14:09
Metacelsus
International Hazard
*****




Posts: 2537
Registered: 26-12-2012
Location: Boston, MA
Member Is Offline

Mood: Double, double, toil and trouble

[*] posted on 23-2-2014 at 14:17


What was your source of aluminum?



As below, so above.

My blog: https://denovo.substack.com
View user's profile View All Posts By User
Hel
Harmless
*




Posts: 2
Registered: 23-2-2014
Member Is Offline

Mood: No Mood

[*] posted on 24-2-2014 at 05:55


Quote: Originally posted by Cheddite Cheese  
What was your source of aluminum?


Cuts from anodized aluminium profiles no longer useable
View user's profile View All Posts By User