TheGhostKing
Harmless
Posts: 13
Registered: 14-9-2013
Location: Texas, Dallas
Member Is Offline
Mood: Lazy
|
|
Nitric Acid and plastic?
Does nitric acid dissolve plastic soda bottles? I want to make sure before i synthesis a dilute amount of it.
I seem to have difficulty referencing my hobbies as "safe".
|
|
Oscilllator
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 659
Registered: 8-10-2012
Location: The aqueous layer
Member Is Offline
Mood: No Mood
|
|
Depends what you mean by "plastic". Polyethylene, PVC, polyester? Go do some research on what particular plastic your soda bottle is, and whether or
not it is resistant to acid.
Most plastics are resistant to dilute nitric acid. As far as I know, only fluoropolymers are immune to concentrated acid.
|
|
Mesa
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 264
Registered: 2-7-2013
Member Is Offline
Mood: No Mood
|
|
http://en.wikipedia.org/wiki/Resin_identification_code
And
http://www.vp-scientific.com/Chemical_Resistance_Chart.htm
should answer your query
|
|
bfesser
|
Thread Moved 2-2-2014 at 06:14 |