I am looking to make silver nitrate with purity over 99.9%. I don't know much about the processes taken for making reagents of high purity in a lab and what measures must be taken. I am starting with a silver coin that I have with declared purity of .9999 (4nine pure), I let it sit in 30% HCl for 5 minutes to remove the surface tarnish, and then rinsed well. I make the nitric acid at home by distilling from sulfuric and a nitrate salt inside a retort and then diluted to 60% with distilled water.

My question is this. The most I have done for cleaning glassware is maybe rinsing with HCl, hot water or ethanol/acetone and then finally rinsing with distilled water and allowing to air dry. Using pure and clean silver and nitric acid (distilled) my end product should be at least 99.9% pure, using clean utensils and such, correct?


[Edited on 25-1-2014 by Turner]
View user's profile View All Posts By User
BromicAcid
International Hazard
*****




Posts: 3237
Registered: 13-7-2003
Location: Wisconsin
Member Is Offline

Mood: Rock n' Roll

[*] posted on 25-1-2014 at 16:05


99.9% pure by what? Metals?



Shamelessly plugging my attempts at writing fiction: http://www.robvincent.org
View user's profile Visit user's homepage View All Posts By User
Turner
Hazard to Others
***




Posts: 197
Registered: 2-12-2013
Member Is Offline

Mood: No Mood

[*] posted on 25-1-2014 at 16:58


99.9% pure by weight of silver nitrate.
View user's profile View All Posts By User
elementcollector1
International Hazard
*****




Posts: 2684
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline

Mood: Molten

[*] posted on 25-1-2014 at 17:09


Yes. However, extra steps such as recrystallization couldn't hurt.