Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: explanation of chemical symbols
Traveller
Hazard to Self
**




Posts: 98
Registered: 29-9-2012
Location: western Canada
Member Is Offline

Mood: inquisitive

[*] posted on 14-2-2013 at 09:45
explanation of chemical symbols


This is an excerpt from the book "Advances in Gold Ore Processing" by M.D. Adams:

"Laboratory-scale tests were conducted on 20% solids slurry containing 25 g/L NaOCl and 0.35 M HCl."

I understand the "g/L" to be grams per litre, of course, but what kind of measurement is "0.35 M"?
View user's profile View All Posts By User
gutter_ca
Hazard to Others
***




Posts: 173
Registered: 7-6-2010
Location: California
Member Is Offline

Mood: Bored at work!

[*] posted on 14-2-2013 at 09:46


"M" in this case indicates molarity, commonly used for acids and bases. In this case, there are 0.35 moles of HCl per liter of solution.



View user's profile Visit user's homepage View All Posts By User
bfesser
Resident Wikipedian
*****




Posts: 2114
Registered: 29-1-2008
Member Is Offline

Mood: No Mood

[*] posted on 14-2-2013 at 09:52


This is a ridiculous thread. Please do some research on your own next time before posting. <em>Any</em> introductory chemistry material will cover <a href="http://en.wikipedia.org/wiki/Concentration" target="_blank">concentration</a> <img src="../scipics/_wiki.png" /> and <a href="http://en.wikipedia.org/wiki/Molar_concentration" target="_blank">molarity</a> <img src="../scipics/_wiki.png" />. Also, please post in the appropriate forum&ndash;this belongs in <strong><a href="forumdisplay.php?fid=12">Beginnings</a></strong>.

<a href="http://lmgtfy.com/?q=What+does+%27M%27+stand+for+in+chemistry%3F&l=1" target="_blank">What does 'M' stand for in chemistry?</a> <img src="../scipics/_ext.png" />

[Edited on 7/9/13 by bfesser]




View user's profile View All Posts By User
Traveller
Hazard to Self
**




Posts: 98
Registered: 29-9-2012
Location: western Canada
Member Is Offline

Mood: inquisitive

[*] posted on 14-2-2013 at 09:53


I see. So, if a person had 34% Muriatic acid, is there a way to convert 0.35 moles to g/L?
View user's profile View All Posts By User
bfesser
Resident Wikipedian
*****




Posts: 2114
Registered: 29-1-2008
Member Is Offline

Mood: No Mood

[*] posted on 14-2-2013 at 10:44


<a href="http://en.wikipedia.org/wiki/Mole_(unit)" target="_blank">Moles</a> <img src="../scipics/_wiki.png" /> is not the same as molarity. Again, the information you seek can easily be found by conducting a web search.

[Edited on 7/9/13 by bfesser]




View user's profile View All Posts By User
Traveller
Hazard to Self
**




Posts: 98
Registered: 29-9-2012
Location: western Canada
Member Is Offline

Mood: inquisitive

[*] posted on 14-2-2013 at 11:04


Excuse me but, everything I've found on the Web is so complicated, I am having trouble understanding what they are trying to say. This is why I asked for an explanation here.
View user's profile View All Posts By User
Traveller
Hazard to Self
**




Posts: 98
Registered: 29-9-2012
Location: western Canada
Member Is Offline

Mood: inquisitive

[*] posted on 14-2-2013 at 11:15
moles?


The following is an excerpt from "Advances in Gold Ore Processing" by M.D. Adams:

"Laboratory-scale tests were conducted at room temperature on 20% solids slurry containing 25 g/L NaOCl and 0.35 M HCl."

I understand the g/L to be grams per litre but the "M" has me a bit confused. I'm told the "M" stands for moles. I looked up the whole mole/molar thing on the Net and, although I understand it to be a mass per volume thing, the actual way of determining just how much HCl to add to a litre to achieve 0.35 moles escapes me.
View user's profile View All Posts By User
bfesser
Resident Wikipedian
*****




Posts: 2114
Registered: 29-1-2008
Member Is Offline

Mood: No Mood

[*] posted on 14-2-2013 at 11:21


Please don't <a href="viewthread.php?tid=23366">double/cross post</a>. But thanks for using the appropriate forum.

Perhaps you're one of those people who don't learn well by reading.
Try this video I found with a 2 second Google search but haven't watched:
<iframe sandbox width="420" height="315" src="http://www.youtube.com/embed/ryfLrSWxaGA" frameborder="0" allowfullscreen></iframe>

[Edited on 2/14/13 by bfesser]




View user's profile View All Posts By User
Vargouille
Hazard to Others
***




Posts: 380
Registered: 16-4-2012
Member Is Offline

Mood: No Mood

[*] posted on 14-2-2013 at 11:24


There is, of course, a way to convert from molarity (moles per liter) to grams per liter. If you know the molar mass (given in grams per mole), you can calculate it. Multiplying a molarity by a molar mass will cancel the units for moles and give you just g/L.
View user's profile View All Posts By User
Traveller
Hazard to Self
**




Posts: 98
Registered: 29-9-2012
Location: western Canada
Member Is Offline

Mood: inquisitive

[*] posted on 14-2-2013 at 11:33


If I could figure out how to delete the other thread, it would be gone by now.

I followed the search you posted a link to and, although I can grasp the concept of a mole being a measurement of a concentration of a substance in a solution, I am still no closer to understanding how many ml. of HCl have to be added to a litre of solution to achieve 0.35 M.
View user's profile View All Posts By User
Traveller
Hazard to Self
**




Posts: 98
Registered: 29-9-2012
Location: western Canada
Member Is Offline

Mood: inquisitive

[*] posted on 14-2-2013 at 11:38


Oops, didn't see right away that you posted a video as well.
View user's profile View All Posts By User
DraconicAcid
International Hazard
*****




Posts: 4502
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Offline

Mood: Semi-victorious.

[*] posted on 14-2-2013 at 11:39


To convert the 34% "muriatic acid" to a molarity would require the density of the acid. Luckily for you, this can be looked up in the CRC handbook of Chemistry and Physics, which tells me that 34% hydrochloric acid is 10.9 M. So you'd have to dilute it by a factor of 31. Measure out 32 mL of your 34% acid (careful!! That stuff is nasty!) and dilute it to 1.0 L.
View user's profile View All Posts By User
bfesser
Resident Wikipedian
*****




Posts: 2114
Registered: 29-1-2008
Member Is Offline

Mood: No Mood

[*] posted on 14-2-2013 at 11:42


Sorry. I tend to edit my replies many times after posting... you probably read it before I had finished with it.



View user's profile View All Posts By User
cAMP
Harmless
*




Posts: 24
Registered: 6-7-2011
Location: East Coast, USA
Member Is Offline

Mood: No Mood

[*] posted on 14-2-2013 at 12:08
By way of explanation


Can a mod please move this topic to Beginnings...

Anyway, molarity or M means "moles per liter" or m/L and is a convenient way of expressing concentration. Moles are a unit of measure, like a dozen or a gross, meaning 12 and 144 respectively. A mole is 6.02x10^23 of something. This is an enormous number, but considering the smallness of atoms, a mole of a substance is usually a measurable, easily defined amount. For example, one mole of sodium chloride measures 58.44 grams / mole.

Since molarity is a measure of concentration, a solution containing one mole of sodium chloride per liter of water would contain 1 liter of water (the solvent) and one mole (6.02x10^23 molecules of sodium chloride, which have a mass of 58.44 grams). This would be 1M or 1 molar solution of sodium chloride.

For your hydrochloric acid, it's a bit more complicated, because HCl(aq) is usually measured for non-scientific purposes as a weight percentage of HCl gas disoolved in water, using a unit of measurement called Baumé units. But there are charts to look this up online. 34% HCl by weight converts to 10.90 molarity, which is calculated based on density and the weight percentage.

If you know that you have a 10.90 molar solution of HCl in water, you know that you have 10.90 moles per liter of HCl. Figure out the molar mass of HCl and multiply by 10.90 and you will have your answer in g / L.

In the future, please try to do your homework first, and then ask these types of questions in the Beginnings section of the site.




"You just spent the entire night arguing grand unification theories with Albert Einstein!" - Geordi LaForge
View user's profile View All Posts By User
IrC
International Hazard
*****




Posts: 2710
Registered: 7-3-2005
Location: Eureka
Member Is Offline

Mood: Discovering

[*] posted on 14-2-2013 at 12:47


Quote: Originally posted by DraconicAcid  
To convert the 34% "muriatic acid" to a molarity would require the density of the acid. Luckily for you, this can be looked up in the CRC handbook of Chemistry and Physics, which tells me that 34% hydrochloric acid is 10.9 M. So you'd have to dilute it by a factor of 31. Measure out 32 mL of your 34% acid (careful!! That stuff is nasty!) and dilute it to 1.0 L.


As new to chemistry as this member sounds I think I would include also the warning "add the acid to water" "DO NOT ADD THE WATER TO ACID!".




"Science is the belief in the ignorance of the experts" Richard Feynman
View user's profile View All Posts By User
Traveller
Hazard to Self
**




Posts: 98
Registered: 29-9-2012
Location: western Canada
Member Is Offline

Mood: inquisitive

[*] posted on 14-2-2013 at 14:07


Okay, now it makes sense. Most of the things I was reading didn't go into the same detail as the guy in the video did.

I even managed to find a calculator online that will convert moles to grams (and vice versa), if you know the molar mass of the compound.
View user's profile View All Posts By User
Traveller
Hazard to Self
**




Posts: 98
Registered: 29-9-2012
Location: western Canada
Member Is Offline

Mood: inquisitive

[*] posted on 14-2-2013 at 17:36


Sorry about posting this in this forum. I re-posted it in Beginnings, as one member suggested, but couldn't figure out how to delete this thread from this forum.

I know this is elementary stuff to you guys, but to me it was quite confusing. You fellows have done a much better job of explaining this than anything on the Internet, except, of course, for the video bfesser found and posted for me on my Beginnings thread.

And thanks for looking out for me, IrC, with the warning to add acid to water and not the other way around. I already knew this, but it's good to see someone looking out for the inexperienced.
View user's profile View All Posts By User
Polverone
Now celebrating 23 years of madness
Threads Merged
17-2-2013 at 23:20
bfesser
Resident Wikipedian
Thread Moved
9-7-2013 at 12:21

  Go To Top