Thermite with Aluminium Oxide?
I recently have purchased aluminium oxide and iron oxide (aluminium oxide by mistake) to make thermite.
I'm wondering will this work and if not I'm thinking maybe I could reduce the aluminium.
|
|
ScienceSquirrel
|
Thread Moved 21-12-2012 at 04:31 |
Eddygp
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 858
Registered: 31-3-2012
Location: University of York, UK
Member Is Offline
Mood: Organometallic
|
|
What would you reduce it with? Iron oxide is already oxidized so it can't reduce aluminium oxide. It would be hilarious if it did.
there may be bugs in gfind
[ˌɛdidʒiˈpiː] IPA pronunciation for my Username
|
|
Adas
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 711
Registered: 21-9-2011
Location: Slovakia
Member Is Offline
Mood: Sensitive to shock and friction
|
|
Wikipedia says that Al2O3 is useful for dehydration of alcohols to alkenes.
Rest In Pieces!
|
|
Manifest
Script Kiddie Asshole
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 229
Registered: 7-12-2012
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by Eddygp ![](images/xpblue/lastpost.gif) | What would you reduce it with? Iron oxide is already oxidized so it can't reduce aluminium oxide. It would be hilarious if it did.
|
If you're talking about the Thermite, no it can't be reduced with Aluminium oxide.
You could reduce it though with Charcoal and then do the thermite.
I should've read it
|
|
ScienceSquirrel
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1863
Registered: 18-6-2008
Location: Brittany
Member Is Offline
Mood: Dogs are pets but cats are little furry humans with four feet and self determination!
|
|
You are not going to reduce aluminium oxide with charcoal.
http://en.wikipedia.org/wiki/Aluminium#Production_and_refine...
|
|
Eddygp
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 858
Registered: 31-3-2012
Location: University of York, UK
Member Is Offline
Mood: Organometallic
|
|
Maybe sodium will do the trick... but you should then get sodium. Why can't you forget about thermite and use it for other purposes?
there may be bugs in gfind
[ˌɛdidʒiˈpiː] IPA pronunciation for my Username
|
|
Pyro
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1305
Registered: 6-4-2012
Location: Gent, Belgium
Member Is Offline
Mood: No Mood
|
|
magnesium should work too no?
all above information is intellectual property of Pyro. ![:D](./images/smilies/biggrin.gif)
|
|
Manifest
Script Kiddie Asshole
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 229
Registered: 7-12-2012
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by Eddygp ![](images/xpblue/lastpost.gif) | Maybe sodium will do the trick... but you should then get sodium. Why can't you forget about thermite and use it for other purposes?
|
I've got no other purposes to use it for. Might sell it ![:(](./images/smilies/sad.gif)
Next time I'll read it properly.
|
|