sternman318
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 121
Registered: 21-4-2011
Member Is Offline
Mood: No Mood
|
|
Crystallization of KMnO4
Are there any viable routes to crystallizing potassium permanganate? It seems that it is so unstable that most routes would end up decomposing it. The
solution is pure, and of about 2% concentration( w/v, i believe)
|
|
Mixell
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 449
Registered: 27-12-2010
Member Is Offline
Mood: No Mood
|
|
It decomposes at 240 C, I think you can evaporate the water slowly, without any decomposition. Just put in on the hotplate and turn the heat just
before the point where bubbles appeared, let it sit for a few hours, slowly turning the heat down as more and more water evaporates.
|
|
Mixell
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 449
Registered: 27-12-2010
Member Is Offline
Mood: No Mood
|
|
Or if you don't want to evaporate all the way through, leave a concentrated solution and freeze it, crystals should form (KMnO4 is about 15 times more
soluble at 100C than at 0C).
|
|
redox
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 268
Registered: 22-2-2011
Location: The Land of Milk and Honey
Member Is Offline
Mood: Chalcogenetic
|
|
KMnO4 is not very stable in water, and your crystallized product will contain small amounts of MnO2 and KOH.
My quite small but growing Youtube Channel: http://www.youtube.com/user/RealChemLabs
Newest video: Synthesis of Chloroform
The difference between chemists and chemical engineers: Chemists use test tubes, chemical engineers use buckets.
|
|