Author: Subject: Melting metals
Chemgineer
Hazard to Others
***




Posts: 216
Registered: 25-5-2021
Member Is Offline


[*] posted on 4-9-2024 at 15:26
Melting metals


I've used a small electric melting furnace and noticed an electrical tingle in my hand when handling the graphite mold. I thought this was an effect of a bad Chinese furnace.

However I have now used a separate high temperature hot plate (coiled element in a brick type setup) and I get the same tingle when trying to touch melted aluminium with steel tongs.

Is this an electromagnetic effect from the 240v AC heating element inducing a current in the molten metals?
View user's profile View All Posts By User
Rainwater
National Hazard
****




Posts: 946
Registered: 22-12-2021
Member Is Offline

Mood: Break'n glass & kick'n a's

[*] posted on 4-9-2024 at 17:50


Not at 50/60 hz with a coiled element.
That sounds like a fault.
I would check the grounding of the furnace. Given that it is not blowing a fuse, it will be in the return path.
A gfci outlet should keep use safe if your not electrically proficient.

[Edited on 5-9-2024 by Rainwater]




"You can't do that" - challenge accepted
View user's profile View All Posts By User
Twospoons
International Hazard
*****




Posts: 1330
Registered: 26-7-2004
Location: Middle Earth
Member Is Offline

Mood: A trace of hope...

[*] posted on 4-9-2024 at 18:42


It could also be a fault with your house wiring. I had a similar thing happen when the neutral connection to our house corroded through - anything earthed and metal was tingly.



Helicopter: "helico" -> spiral, "pter" -> with wings
View user's profile View All Posts By User
Chemgineer
Hazard to Others
***




Posts: 216
Registered: 25-5-2021
Member Is Offline


[*] posted on 5-9-2024 at 01:09


The strange thing is I am only touching the molten metal with a steel tool, the crucible it is in is isolated from the heating element.
View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5128
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 5-9-2024 at 03:03


Many "insulators" become slightly conductive when hot.
So it's possible that you are feeling a leakage current.
Graphite is quite a good conductor.
View user's profile View All Posts By User
averageaussie
Hazard to Self
**




Posts: 92
Registered: 30-4-2023
Location: Right behind you
Member Is Offline

Mood: school :(

[*] posted on 5-9-2024 at 15:18


forgive me but how are you feeling the electricity? outside of a small arc like in a static shock I'm not sure how you would feel an electric tingle.
View user's profile View All Posts By User
Chemgineer
Hazard to Others
***




Posts: 216
Registered: 25-5-2021
Member Is Offline


[*] posted on 6-9-2024 at 04:55


I'm feeling a frequency buzzing up my arm. I am wondering if the refractory brick that has the heating coil in it is actually slightly conductive.

Either that or the molten alluminium is have a current induced in it my magnetic induction.
View user's profile View All Posts By User
Morgan
International Hazard
*****




Posts: 1705
Registered: 28-12-2010
Member Is Offline

Mood: No Mood

[*] posted on 6-9-2024 at 07:56


So when you turn off the voltage does it still produce the "buzzing" or resonance?
View user's profile View All Posts By User
Chemgineer
Hazard to Others
***




Posts: 216
Registered: 25-5-2021
Member Is Offline


[*] posted on 6-9-2024 at 08:32


Quote: Originally posted by Morgan  
So when you turn off the voltage does it still produce the "buzzing" or resonance?


If i turn the furnace on with solid alluminium in it and try, I don't get the effect, only happens when its up to temp and melted.
View user's profile View All Posts By User
Rainwater
National Hazard
****




Posts: 946
Registered: 22-12-2021
Member Is Offline

Mood: Break'n glass & kick'n a's

[*] posted on 6-9-2024 at 14:36


Quote: Originally posted by averageaussie  
forgive me but how are you feeling the electricity? outside of a small arc like in a static shock I'm not sure how you would feel an electric tingle.

Getting electrocuted is one of those things that can be neither be properly described nor ever forgotten. It's almost the same as being tasered but mostly not as overwhelming due to mains frequency being 50/60 and a taser being a lot more

A simple test. Get a dmm or something that can read continuity or resistance and voltage.
Your country will determine which is what, but with the unit unpluged from the wall, test all 3 prongs to the frame of the furnace, only the ground pin should have continuity to the frame.
If none of them have it, problem found.

Next, same thing but there is a relay in the way of testing. So plug it up, turn it on, and get to smelting. Once your melt looks nice, use your meter again and check for voltage on the case




"You can't do that" - challenge accepted
View user's profile View All Posts By User