Author: Subject: Tin and Copper acetates
Romix
Hazard to Others (Literally)
***




Posts: 492
Registered: 19-6-2015
Member Is Offline

Mood: No Mood

[*] posted on 19-5-2021 at 19:59
Tin and Copper acetates


I've left beaker full of BGA ICs in vinegar for a year to remove the solder.
Solder dissolved, some copper too. There's a white precipitate in a tin acetate solution what it can be? Also I having a problem dropping metals out of the solution, tried baking soda, nothing drops, displacing with pure aluminum and zinc, nothing too.
View user's profile View All Posts By User
Romix
Hazard to Others (Literally)
***




Posts: 492
Registered: 19-6-2015
Member Is Offline

Mood: No Mood

[*] posted on 19-5-2021 at 20:12


The solution still is very acidic. Will neutralize it with Tin slag left from melting very oxidized lead free reels.
Probably will take another year or so.
View user's profile View All Posts By User