Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: fixing cracked glass / glassblowing
Yttrium2
Perpetual Question Machine
*****




Posts: 1104
Registered: 7-2-2015
Member Is Offline


[*] posted on 22-6-2020 at 20:54
fixing cracked glass / glassblowing


My retort has somehow developed a crack around where the stopper connects. I am wondering if I can heat the area till red with a torch to seal in the crack or will this stress the glass? I mean does the entire retort need to be heated to prevent stressing the glass? They do have those giant torches for killing weeds, how well do those work for blowing glass? - I may need to heat the entire vessel to get rid of the crack..


Also, how do you tell if a glass is stressed? Somewhere earlier I was reading of a way to determine if a glass is stressed and will shatter later on from improper annealing



any advice on this topic greatly appreciated.

[Edited on 6/23/2020 by Yttrium2]
View user's profile Visit user's homepage View All Posts By User
Chemetix
Hazard to Others
***




Posts: 376
Registered: 23-9-2016
Location: Oztrayleeyah
Member Is Offline

Mood: Wavering between lucidity and madness

[*] posted on 22-6-2020 at 23:05


The quick answer is is yes with a maybe. There's a bit more to go over than a few posts can cover. PM me and I'll guide you through what you need to know and what equipment you might need. There are technique variations that you can use depending on the available equipment, so if you tell me what sort of equipment you might be able to get your hands on then I can suggest which technique is likely to succeed.
View user's profile View All Posts By User
Belowzero
Hazard to Others
***




Posts: 173
Registered: 6-5-2020
Location:                 Member Is Offline
Member Is Offline


[*] posted on 22-6-2020 at 23:26


Quote: Originally posted by Chemetix  
The quick answer is is yes with a maybe. There's a bit more to go over than a few posts can cover. PM me and I'll guide you through what you need to know and what equipment you might need. There are technique variations that you can use depending on the available equipment, so if you tell me what sort of equipment you might be able to get your hands on then I can suggest which technique is likely to succeed.


I'd be interested too , please consider doing this in the public square :)
View user's profile View All Posts By User
wg48temp9
National Hazard
****




Posts: 786
Registered: 30-12-2018
Location: not so United Kingdom
Member Is Offline


[*] posted on 23-6-2020 at 01:38


You may want watch a glass repair video by Codyslab:

https://www.youtube.com/watch?v=86X5f9xprQ4

Its probably more about the problems of repairing a cracked flask so its a how not to do it video for repairing cracked flasks. I have seen a more successful video from an experienced glass blower but could not find it. I have tried it myself with mostly similar problems to Cody ie the crack propagating. Ideally for boro glass you will need at least an oxy propane torch.




I am wg48 but not on my usual pc hence the temp handle.
Thank goodness for Fleming and the fungi.
Old codger' lives matters, wear a mask and help save them.
Be aware of demagoguery, keep your frontal lobes fully engaged.
I don't know who invented mRNA vaccines but they should get a fancy medal and I hope they made a shed load of money from it.
View user's profile View All Posts By User
Ubya
International Hazard
*****




Posts: 1247
Registered: 23-11-2017
Location: Rome-Italy
Member Is Offline

Mood: I'm a maddo scientisto!!!

[*] posted on 23-6-2020 at 03:20


propane alone won't work probably, to fix a star crack on one of my little flasks i had to use oxy-propane from a small torch, otherwise the glass is not hot enough to flow.

this process stresses the glass, you can see the stress spots with a polarizing filter and an LCD screen





---------------------------------------------------------------------
feel free to correct my grammar, or any mistakes i make
---------------------------------------------------------------------
View user's profile View All Posts By User
Chemetix
Hazard to Others
***




Posts: 376
Registered: 23-9-2016
Location: Oztrayleeyah
Member Is Offline

Mood: Wavering between lucidity and madness

[*] posted on 23-6-2020 at 15:46


I'll get a video up on how to repair cracks.

In case you missed the first video, glassblowing for complete beginners, have a look. https://www.youtube.com/watch?v=BjX5JwOvKGM

You can use the bunsen and blow tube technique to heal cracks on small pieces. For bigger pieces with thicker walls you'll need a small oxy- fuel brazing torch. Jewellery torches or plumbers torches will work.

Codys lab failed using a welding torch because of a few techniques he missed. I'll show you why in the video.
View user's profile View All Posts By User
XeonTheMGPony
International Hazard
*****




Posts: 1641
Registered: 5-1-2016
Member Is Offline

Mood: No Mood

[*] posted on 23-6-2020 at 16:20


I use a map torch for most my glass stuff, propane turbo torch for smaller tube work.

I greatly miss my smith little torch HVAC edition it was perfect for that shit!
View user's profile View All Posts By User
Chemetix
Hazard to Others
***




Posts: 376
Registered: 23-9-2016
Location: Oztrayleeyah
Member Is Offline

Mood: Wavering between lucidity and madness

[*] posted on 24-6-2020 at 21:23


You can check out the video on how to heal small cracks I've posted on youtube.
https://youtu.be/MiW7vDJofeA

It's quick and dirty, but gets the point across. Hope it helps.
View user's profile View All Posts By User
Belowzero
Hazard to Others
***




Posts: 173
Registered: 6-5-2020
Location:                 Member Is Offline
Member Is Offline


[*] posted on 25-6-2020 at 06:35


Quote: Originally posted by Chemetix  
You can check out the video on how to heal small cracks I've posted on youtube.
https://youtu.be/MiW7vDJofeA

It's quick and dirty, but gets the point across. Hope it helps.


Very nice video, thanks for the effort!
Gives me a lot more confidence in repairing my cracked condensor. The illustration of the polarization is really useful and quite obvious once shown like this, not so much just reading it from paper.

I am pretty sure people on youtube will like your content , you have a very clear way of explaining and a calm over you that makes it comfortable to watch.
Okay enough with the feathers :)
View user's profile View All Posts By User
wg48temp9
National Hazard
****




Posts: 786
Registered: 30-12-2018
Location: not so United Kingdom
Member Is Offline


[*] posted on 25-6-2020 at 16:58


Quote: Originally posted by Chemetix  
You can check out the video on how to heal small cracks I've posted on youtube.
https://youtu.be/MiW7vDJofeA

It's quick and dirty, but gets the point across. Hope it helps.


Having watched your first video how you get the scratch to propagated a crack round a glass tube by touching the scratch with molten glass. I figured the same thing happens when you heat the centre of a crack to repair it.

Thanks for the two videos.




I am wg48 but not on my usual pc hence the temp handle.
Thank goodness for Fleming and the fungi.
Old codger' lives matters, wear a mask and help save them.
Be aware of demagoguery, keep your frontal lobes fully engaged.
I don't know who invented mRNA vaccines but they should get a fancy medal and I hope they made a shed load of money from it.
View user's profile View All Posts By User
Yttrium2
Perpetual Question Machine
*****




Posts: 1104
Registered: 7-2-2015
Member Is Offline


[*] posted on 25-6-2020 at 19:09


can anyone explain how strain develops in glass?


Is this the best cheap polariscope that money can buy?


Would a bunsen burner be a good torch as opposed to the ones that screw onto the propane tanks that do not adjust? - My guess is yes, (would it be a good purchase?)
and in addition to the bunsen burner, I need a bunsen burner control valve regulator?

[Edited on 6/26/2020 by Yttrium2]

delete2.jpg - 16kB

[Edited on 6/26/2020 by Yttrium2]
View user's profile Visit user's homepage View All Posts By User