rockyit98
Hazard to Others
***




Posts: 283
Registered: 12-4-2019
Location: The Known Universe
Member Is Offline

Mood: no mood is a good mood

[*] posted on 18-10-2019 at 22:11
silicon carbide from old abrasive paper ("sand" paper)





i been keeping/collecting used abrasive paper for a while. lately i needed SiC fine powder to mix with fire clay (70%Al2O3 30%SiO2) to increase its thermal conductivity,since SiC have high value about upward of 200W m−1K−1.since SiC is very hard i can't ball mill it.so i turned to my old collection of abrasive paper.
some are black and others are not. only black ones are made of SiC. rest are Al2O3.so i cut a sample of black ones and measured it weigh using a milligram scale .then burned it heating it to red hot to burn off carbon then measured the residue .after some calculation it was 60% SiC.i was so happy:).
i desired 200g of SiC so burned all of my old black abrasive paper.
i washed the SiC and let them dry.used a strainer to get the fine SiC.

the image below is a new abrasive paper and the rest after the straining since i used the good stuff.sorry:(
hope this helped. thank you.
FYI:you can use SiC and fire clay to make Microwave crucible because SiC absorbs Microwave well.can get up to 1500C if you used proper clay and insulation.

SiC - Copy.jpg - 383kB




"A mind is a terrible thing to lose"-Meisner
View user's profile View All Posts By User
Boffis
International Hazard
*****




Posts: 1886
Registered: 1-5-2011
Member Is Offline

Mood: No Mood

[*] posted on 19-10-2019 at 01:23


Can't you just buy the silicon carbide? I use it for polishing rock slabs and its dirt cheap. You can even buy it ready ground from 32 to 1200 mesh, its available in 100 to 500g amounts on ebay what more could you want?
View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5129
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 19-10-2019 at 04:35


Quote: Originally posted by Boffis  
what more could you want?

The satisfaction of doing it yourself.
The joy of knowing it is recycled.
View user's profile View All Posts By User
Ubya
International Hazard
*****




Posts: 1247
Registered: 23-11-2017
Location: Rome-Italy
Member Is Offline

Mood: I'm a maddo scientisto!!!

[*] posted on 19-10-2019 at 11:25


how do they mill it industrially?
i have a big clump of SiC crystals, i'd like to grind some to make abrasive powder





---------------------------------------------------------------------
feel free to correct my grammar, or any mistakes i make
---------------------------------------------------------------------
View user's profile View All Posts By User
fusso
International Hazard
*****




Posts: 1922
Registered: 23-6-2017
Location: 4 ∥ universes ahead of you
Member Is Offline


[*] posted on 19-10-2019 at 11:30


Sometimes extracting the treasury parts from some trashy bois is satisfying and therapeutic, and they're free too!