Lactic Acid


I'm trying to make some PolyLactic Acid for a project I'm working on and am just looking to find the best way to acquire some Lactic Acid to begin with. It would be best if I were to obtain in chemically, but anywhere I can buy it is nice too. Thanks.
View user's profile View All Posts By User
Melgar
Anti-Spam Agent
*****




Posts: 2004
Registered: 23-2-2010
Location: Connecticut
Member Is Offline

Mood: Estrified

[*] posted on 1-11-2018 at 16:43


It's sold in homebrewing stores as an acidity regulator. Usually it's in an 88% solution. Apparently, it forms cyclic dimers quite readily, so good luck getting it to form chains. It might not be that difficult though, I've never actually tried it.



The first step in the process of learning something is admitting that you don't know it already.

I'm givin' the spam shields max power at full warp, but they just dinna have the power! We're gonna have to evacuate to new forum software!
View user's profile View All Posts By User
Texium
Administrator
Thread Moved
8-11-2018 at 09:30

  Go To Top