Carbonates/ hydroxides from carbonates?
I want to understand why hydroxides are formed when Sodium carbonate is added to a Fe / Cr chlorides mixture (stainless steel + HCl)?
The question arises from SM wiki chromates (potassium/sodium).
"The chromium(III) hydroxide can be easily made by dissolving stainless steel in hydrochloric acid, followed by precipitation with sodium
carbonate.[4]"
"Sodium carbonate (not sodium hydroxide) is added to the solution to neutralize all remaining acids and precipitate a mixture of iron and chromium
hydroxides"
Also I started to check precipitation of carbonates by adding sodium cabonate to metal sulfates/chlorides to check how it precipitates.
When adding Na2CO3 sol. to an old FeCl2 (probably with FeCl3) sol., obtained blue / green, also some white - turning light green - precipitates.
On air standing, all became brown (in one night).
so here are the questions:
1) Why NaOH cannot be used to neutralize Fe/Cr chlorides to get Fe/Cr hydroxides? (in chromate syntesis) Common sense is : use Hydroxide to get
hydroxide and use carbonate to get carbonate.
2) cCan some one explain or share the FeCl2/FeCl3 + Na2CO3 to get Hydroxide? (my asumption is : FeCl2(aq) + Na2CO3(aq) -> FeCO3(s) + 2NaCl(aq) - no
hydroxide. I read that iron (III) carbonate does not exist.
Thanks
Go SAFE, because stupidity and bad Luck exist.
|
|
DraconicAcid
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4298
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Offline
Mood: Semi-victorious.
|
|
These transition metal ions are hydrated in aqueous solution. Because of the high charge, the water molecules are easily deprotonated by random
bases.
[Fe(H2O)6](3+) + 3 B --> 3 HB+ + Fe(OH)3(s) + 3 H2O
For iron(III), carbonate, ammonia, and hydroxide will all precipitate iron(III) hydroxide. For chromium, excess hydroxide will result in the
formation of soluble [Cr(OH)4]-
Please remember: "Filtrate" is not a verb.
Write up your lab reports the way your instructor wants them, not the way your ex-instructor wants them.
|
|
Maurice VD 37
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 66
Registered: 31-12-2018
Member Is Offline
|
|
RU KLO's first question was about the reaction of Cr^3+ and carbonate. He wanted to know why it produces an hydroxide.
The equation of the reaction should be :
2 Cr3+ + 3 CO3^2- --> Cr2(CO3)3
But this rection does not happen. Or if it happens, Cr2(CO3)3 is immediately hydrolyzed according to :
Cr2(CO3)3 + 3 H2O --> 2 Cr(OH)3 + 3 CO2
This hydrolysis reaction is produced when any triply-charged ion, like Cr3+ or Al3+ or Fe3+, is in contact with a solution containing the carbonate
ion. These metallic ions do not produce carbonates.
|
|
chornedsnorkack
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 546
Registered: 16-2-2012
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by Maurice VD 37 ![](images/xpblue/lastpost.gif) |
This hydrolysis reaction is produced when any triply-charged ion, like Cr3+ or Al3+ or Fe3+, is in contact with a solution containing the carbonate
ion. These metallic ions do not produce carbonates. |
Not true.
Cr3+, Al3+ and Fe3+ indeed do not produce carbonates. But it is not applicable to "any triply-charged ion" because
triply charged ions include lanthanides - and these do form carbonates.
Lanthanides seem to form carbonate precipitates. Th and U form soluble carbonate complexes (besides solid carbonates).
Picking a good base to produce hydroxide depends strongly on the metals. Some dissolve in excess of hydroxide, so you could like a weaker base... but
carbonate may or may not go to the precipitates. Some metals are easily precipitated by ammonia, others are dissolved by it... or blown up.
|
|