Author: Subject: Making Iron from Sand
Yttrium2
Perpetual Question Machine
*****




Posts: 1104
Registered: 7-2-2015
Member Is Offline


[*] posted on 2-9-2022 at 19:48
Making Iron from Sand


https://www.youtube.com/watch?v=OPIUMpiV0IY

Pretty cool, not too often do we see trending videos in the YouTube section on chemistry

Saw one a while ago about the production of bronze, iirc.
View user's profile Visit user's homepage View All Posts By User
Yttrium2
Perpetual Question Machine
*****




Posts: 1104
Registered: 7-2-2015
Member Is Offline


[*] posted on 2-9-2022 at 20:02


How hot does a “primitive” furnace like this get?
View user's profile Visit user's homepage View All Posts By User
j_sum1
Administrator
********




Posts: 6338
Registered: 4-10-2014
Location: At home
Member Is Offline

Mood: Most of the ducks are in a row

[*] posted on 2-9-2022 at 20:36


Yeah. This guy is good.
A lot of skill in mandling clay and other bushcraft techniques.
Fundamental to a lot of what he does is having good procedures for making charcoal.

I watched another one of his recently where the source material was bacterial sludge that had concentrated iron (I think as the sulfide). It was a pretty good effort with a nice result. He made an iron knife.

To answer your question, just look up the melting point of iron.
View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5129
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 3-9-2022 at 02:18


Quote: Originally posted by j_sum1  
Y
To answer your question, just look up the melting point of iron.

And then look up the melting point of the iron/ carbon eutectic.
View user's profile View All Posts By User
Yttrium2
Perpetual Question Machine
*****




Posts: 1104
Registered: 7-2-2015
Member Is Offline


[*] posted on 3-9-2022 at 17:59


Quote: Originally posted by unionised  
Quote: Originally posted by j_sum1  
Y
To answer your question, just look up the melting point of iron.

And then look up the melting point of the iron/ carbon eutectic.


Is this for making steel?
View user's profile Visit user's homepage View All Posts By User
j_sum1
Administrator
********




Posts: 6338
Registered: 4-10-2014
Location: At home
Member Is Offline

Mood: Most of the ducks are in a row

[*] posted on 3-9-2022 at 20:10


Cast Iron has a carbon content of typically 4.3% by mass. That is the eutectic point of the carbon iron system. Eutectic temperature is 1147C
Properties of cast iron differ significantly from steel.

Steels of various kinds have properties determined in part by the microstructure which is related to the heating/cooling history around the eutectoid point (0.76%C and 723°C)
At this concentration of carbon the steel melts at around 1500°C. Cooling passes through the austenite phase and then the ferrite phase.

A higher melt temperature is required in practice. Typical slag temperature is around 1630°C, and it needs to be molten to effectively carry away impurities.

I have not watched the video you posted, but the previous one I did watch is presumably similar. I would estimate that he achieved a temperature just shy of 1600°C which is just enough to have an effective slag. And my guess is that he ended up with a high carbon steel rather than a cast iron: maybe 1% carbon.
Of course this is all guessing, but it does give a ball-park answer to your question.

The iron-carbon phase diagram is a complex beast. (Simple version below) But it has features that mean that steel properties are very manipulable. This is one of the reasons why steel is so ubiquitous.




[edit - post better diagram]

[Edited on 4-9-2022 by j_sum1]
View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5129
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 4-9-2022 at 09:31


Quote: Originally posted by Yttrium2  


Is this for making steel?

It's complicated but what you get out of a primitive furnace is "pig iron" or "cast iron" which has a lot of carbon in it.
To turn it into steel you need to remove the carbon some how. It's "unhelpful" that the stuff we call "cast iron" actually has less iron in than steel has.
View user's profile View All Posts By User
Yttrium2
Perpetual Question Machine
*****




Posts: 1104
Registered: 7-2-2015
Member Is Offline


[*] posted on 13-10-2022 at 22:15


Quote: Originally posted by j_sum1  
Cast Iron has a carbon content of typically 4.3% by mass. That is the eutectic point of the carbon iron system. Eutectic temperature is 1147C
Properties of cast iron differ significantly from steel.

Steels of various kinds have properties determined in part by the microstructure which is related to the heating/cooling history around the eutectoid point (0.76%C and 723°C)
At this concentration of carbon the steel melts at around 1500°C. Cooling passes through the austenite phase and then the ferrite phase.

A higher melt temperature is required in practice. Typical slag temperature is around 1630°C, and it needs to be molten to effectively carry away impurities.

I have not watched the video you posted, but the previous one I did watch is presumably similar. I would estimate that he achieved a temperature just shy of 1600°C which is just enough to have an effective slag. And my guess is that he ended up with a high carbon steel rather than a cast iron: maybe 1% carbon.
Of course this is all guessing, but it does give a ball-park answer to your question.

The iron-carbon phase diagram is a complex beast. (Simple version below) But it has features that mean that steel properties are very manipulable. This is one of the reasons why steel is so ubiquitous.




[edit - post better diagram]

[Edited on 4-9-2022 by j_sum1]



What’s in the 2.4’— area?
View user's profile Visit user's homepage View All Posts By User