Sn + HNO3 => Sn(NO3)2 - tin(II) nitrate


Hello,
What happens when you put some tin in nitric acid?
Maybe with a conc of between 1 to 10 M.
Does [[Sn3(OH)4]2](+) [NO3](-) form in water? Does it decompose forming SnO?

Wikipedia does not document tin(II) nitrate.
There is only tin(IV) nitrate.
Another site, a forum, mentions that dry tin(II) nitrate can’t be prepared but you can have Sn(NO3)2.20 H2O

There is this page
https://www.sciencedirect.com/science/article/abs/pii/002016...
but that is a single page preview.




Signature ==== Is this my youtube page? https://www.youtube.com/watch?v=tA5PYtul5aU
We must attach the electrodes of knowledge to the nipples of ignorance and give a few good jolts.
Yes my evolutionary friends. We are all homos here.
View user's profile View All Posts By User
Bedlasky
International Hazard
*****




Posts: 1250
Registered: 15-4-2019
Location: Period 5, group 6
Member Is Offline

Mood: Volatile

[*] posted on 26-11-2021 at 11:42


Tin reacts with nitric acid to produce hydrous SnO2. You cannot produce any tin nitrate in aqueous solution.

I once analysed some Sn-Pb-Cu alloy. I dissolved it in nitric acid, filter off SnO2.xH2O and by strong heating converted it to anhydrous SnO2. Pb was determined as PbSO4 and Cu by iodometry.




View user's profile View All Posts By User
vmelkon
National Hazard
****




Posts: 669
Registered: 25-11-2011
Location: Canada
Member Is Offline

Mood: autoerotic asphyxiation

[*] posted on 26-11-2021 at 16:58


Actually, I am trying to separate some Sn-Cu-Ag alloy.
HCl dissolves the Sn. What is left is a red powder that slowly produces bubbles, so I assume it still contains some tin.
My plan was to use HNO3 to dissolve this powder but looks like some insoluble yellow white substance formed, so I think this is the SnO2.




Signature ==== Is this my youtube page? https://www.youtube.com/watch?v=tA5PYtul5aU
We must attach the electrodes of knowledge to the nipples of ignorance and give a few good jolts.
Yes my evolutionary friends. We are all homos here.
View user's profile View All Posts By User
S.C. Wack
bibliomaster
*****




Posts: 2419
Registered: 7-5-2004
Location: Cornworld, Central USA
Member Is Offline

Mood: Enhanced

[*] posted on 26-11-2021 at 18:10


With cooling and an excess of acid diluted with at least 3/4 volume of water, tin is said to give a colorless solution of stannous nitrate...and ammonium nitrate, which are not particularly separable or isolated as such. Hydrolysis products would depend on all of the variables...it is said that the yellow-white substance is a mixture of white stannic nitrate and a yellow basic stannic nitrate.