fra77x
Harmless
Posts: 6
Registered: 3-11-2021
Member Is Offline
|
|
Hello and help for lightsensitive paint
Hello, this is my first post here.
I am interested to make some photosensitive paint (UV). I have read some wikipedia articles about silver and dichromates and I wonder if someone can
tell me if it is at all possible at my level and (non existent) equipment and perhaps if it is, to point me to some directions.
Regards,
John
[Edited on 11-11-2021 by fra77x]
|
|
walruslover69
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 225
Registered: 21-12-2017
Member Is Offline
Mood: No Mood
|
|
Hi John, It's definitely possible but it depends on what your actual end goal is. Silver chloride/bromide/iodide are commonly used are is how film and
polaroids work. These reactions are also not reversible, and require a little bit of developing. Usually a suspension of silver chloride or silver
bromide suspended in gelatin is used. But photosensitivity is dependent on the wavelength of light. It really depends on what your end goal is.
|
|
fra77x
Harmless
Posts: 6
Registered: 3-11-2021
Member Is Offline
|
|
Thanks. I have read about gelatin and I have some here. My goal is to prepare some photosensitive paint so I can use it to cover copper boards and
expose them with a mask to UV light (like sun or UV LEDS) perhaps I will also use some lens to make the mask appear smaller So I can get greater
detail by printing bigger masks and using lens to focus).
Now I read that I can make silver chloride by mixing silver nitrate with salt. And to make silver nitrate I have to dissolve some silver metal with
nitric acid. And to make nitric acid I can use HCl, nitrate salt and copper.
So now my question is how to make a nitrate salt. I read that any source of nitrate can work like sodium nitrate,potassium nitrate, ammonium nitrate
but I have no idea how/where to get such chemicals.
Is it possible to make ammonium nitrate by using ammonia and sodium bicarbonate? How should I proceed?
[Edited on 11-11-2021 by fra77x]
|
|
Twospoons
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1306
Registered: 26-7-2004
Location: Middle Earth
Member Is Offline
Mood: A trace of hope...
|
|
What you are looking for is a photocured polymer - quite different from a silver photographic emulsion. Totally different chemistry.
If all you want is to make PCBs on the cheap (its quite hard to beat the prices out of China these days), I'd suggest you look at toner transfer.
Laser printer + some transfer paper (I prefer "Press'n'Peel Blue" - gives excellent results) + a hot plate. It takes a bit of work to get the process
right (true of every method of PCB production), but once you do you can turn out a board in 30 minutes. And you can get high levels of detail with a
little care - I've achieved 5mil/5mil track/space on 1/2oz double-sided Kapton flex. Apologies for the imperial units - electronic cad seems stuck in
the past sometimes.
Helicopter: "helico" -> spiral, "pter" -> with wings
|
|
fra77x
Harmless
Posts: 6
Registered: 3-11-2021
Member Is Offline
|
|
I never had success with laser printer transfer method. I have also tried to use a photosensitive coating but I could never apply it correctly. I am
also interested to make a photosensitive paint as a way to spend some time with chemistry.
So it is a different process. I believe I have read I need to make some type of polymer, I have read about dichromate.
Is this achievable with my means?
|
|
Twospoons
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1306
Registered: 26-7-2004
Location: Middle Earth
Member Is Offline
Mood: A trace of hope...
|
|
Start here: https://en.wikipedia.org/wiki/Photopolymer
That will give you a broad overview of the chemistry, and offer a starting point for your research.
I looked at that ( for making 3d printing resin), and threw it in the "too hard" basket.
Helicopter: "helico" -> spiral, "pter" -> with wings
|
|
fra77x
Harmless
Posts: 6
Registered: 3-11-2021
Member Is Offline
|
|
I have read this article and hopped there was still a chance to be able to do something, that's the reason I asked here. So creating photopolymers is
too hard, that's what I wanted to hear.
Thanks
|
|
beta4
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 56
Registered: 3-2-2019
Member Is Offline
|
|
Making a photoresist is unfortunately hard, and if you are just beginning with chemistry I would suggest to stay away from carcinogenic substances
such as dichromates.
If you want to make printed circuit boards you can buy presensitized boards that already have a photoresist coar atop the copper.
I have a video on my channel explaining the process https://youtu.be/5d9JvZiYhEg but there are many similar ones online.
If for some reason you need to apply a photoresist to an existing surface, I had most luck with gelled photoresist rolls you can buy from ebay. They
are like double sided tape, you peel one of the two protective films and apply it to the surface, expose it to UV light through a mask, let the resin
cure, peel the other protective film and develop it.
I show how to use this kind of photoresist in my video where I explain how to make double sided printed circuits at home (including plated-through
holes) https://youtu.be/Kn92cLf69iw using a process I developed that can be done in an amateur lab.
Additionally, a few companies sell liquid photoresist in spray cans, such as positiv 20
https://www.tme.eu/Document/b7a6a16ed14d2aa6149ed9a14fb1b03d...
but it is hard to find and hard to apply without a spin coater.
|
|
fra77x
Harmless
Posts: 6
Registered: 3-11-2021
Member Is Offline
|
|
Quote: |
Making a photoresist is unfortunately hard |
I hopped it was different.
I have used several methods for PCB, most of what one can find in tutorials. I know about graphic designing and I wanted to develop my own way to
design PCB (I like to use illustrator) I also like to experiment with focused lensing. Also I thought if sink printing uses a photosensitive paint (is
it right?) then perhaps it wasn't so hard to get/ or even to make. It seems I guessed wrong. In general I just wanted to have the freedom of making my
own photosensitive paint so to use it in "experiments" with printing, etching and things like that. I will investigate further and thanks for the tip
that dichromates are carcinogenic and I should avoid them.
Is there any other way to make a photoresistive paint? I mean without dichromates?
|
|
wg48temp9
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 770
Registered: 30-12-2018
Location: not so United Kingdom
Member Is Offline
|
|
Prior to bichromate bitumen was once as a photoresist. There are probably lots of other compounds compounds that could be used. Try searching for
historic photoengraving methods.
The gelatin bichromate process is simple and effective I have made prints using it but yes dichromate is carcinogenic. It was once common in chemistry
sets. Depending on where you live you may not be able to buy it these days.
Presumably you have to buy the copper clad board so I suggest you buy a can of spray on photoresist or even better dry film photoresist, £4.34 for
a sheet 0.3m x 2m
see: https://www.ebay.co.uk/itm/224482571845_trkparms=ispr%3D1&am...
I am wg48 but not on my usual pc hence the temp handle.
Thank goodness for Fleming and the fungi.
Old codger' lives matters, wear a mask and help save them.
Be aware of demagoguery, keep your frontal lobes fully engaged.
I don't know who invented mRNA vaccines but they should get a fancy medal and I hope they made a shed load of money from it.
|
|
fra77x
Harmless
Posts: 6
Registered: 3-11-2021
Member Is Offline
|
|
Bitumen of Judea or Syrian asphalt... the first photograph... photolithography.. cool stuff. Thanks wg48. I found some ammonium bichromate for 50 euro
per 500 gr. Too expensive I think. I will investigate a bit the bitumen process.
I will also try gelatin with carbon.
I have tried with dry film photoresist and I couldn't get reliable results mainly due to the ripples that were unavoidable during the coating.
Photoresist spray seems interesting.
|
|
TLutman
Harmless
Posts: 26
Registered: 13-10-2019
Member Is Offline
|
|
Have you tried pre sensitized boards? That’s what I’ve always used with decent results, even with smd, down to 0402 passives and chips.
I’m trying a different exposure method right now, using a SLA printer (resin 3d printer), trying to eliminate the whole laser jet/transparency
thing.
I’ve watched a few videos on the dry film method, and to prevent wrinkles they spray the bare copper with a fine spray of distilled water and
squeegee it out before laminating.
|
|
violet sin
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1476
Registered: 2-9-2012
Location: Daydreaming of uraninite...
Member Is Offline
Mood: Good
|
|
Photographic silver emulsion leaves suspended silver oxide particles in the gelatin, and washes the unbruised silver salts into solution, and away
where they can't change the image later. Think all the trouble of making your own film for a big camera. Not exposing it accidentally, getting it
even coatings, etc. Not sure the clear parts wash all gelatin away so you'd have a clean etch?
Silk screen resist isn't that expensive, and in my experience ( screen printing) it's easy. Use a rudimentary stick or 1" putty knife to get some on
the screen, start with a small blob. Skreet it side to side with a rubber blade print wiper, untill it's even. Let dry in a dark cabinet with forced
air. Set your negative on it and expose to sunlight by watch count.
A proper framed print screen, shirt contacting side up with your velum on it image down and a board with foam under the print screen to supply back
pressure against the image. Place a glass sheet over the velum for intimate contact between image and dried emulsion. This ensures no bubbles that
take away sharpness, and also that your tightest marks are going to be face down on the PCB ... Not up where you load your paint for the masking yet
to come. You can expose it. Wash it out while the black covered parts are soft and the exposed parts are hard. Too early and you have pinholes
everywhere, soft edges and too much washing ruins the screen. Too late and your supposedly soft parts under the image still won't wash out easy.
Once it's cleaned up, you can use a dab or two of the emulsion to fix pinholes.
Start printing in acrylic paint on the PCB with a rubber printing squeegee, or something easy to wash out. Don't let it set on your screen! Washing
early is easier than scrubbing later. You can get a lot of use out of a wood frame, couple yards of screen, small jar of resist and some acrylic
paint. If the design is good, it's kinda hard to wear out the screen. It gets harder the more things you sub in or change, results vary, with
practice/skill
I've used hand drawn fingernail polish, numerous runs of a black sharpie, pitch and l tried super glue. If you want detail, do it right or buy them.
It is infuriating to try and do surface mount parts by hand I tell you. Also don't drill the holes too big if it's through hole parts. Closing the
gap is a pain. I've deff down it wrong more times and ways than right. But I have also printed t-shirt for a few years when in college, by the
thousands. So if reproducibility and precision is key, buy at least purpose made items. Now the frames and screens can be made by any idiot, I should
know. The sun is free and works on a cloudy day too. The squeegee, resist material and fabric for the screen are not trivial accessories.
|
|