What to dissolve Stannic acid with?
What to dissolve Stannic acid with?
|
|
zinc finger
Harmless
Posts: 25
Registered: 30-7-2019
Location: Germany
Member Is Offline
|
|
Either with lye as stannate, large amounts of hot water or with concentrated HCl or HNO3.
|
|
njl
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 609
Registered: 26-11-2019
Location: under the sycamore tree
Member Is Offline
Mood: ambivalent
|
|
For me HCl would be best, but it depends on what you want to keep.
Reflux condenser?? I barely know her!
|
|
j_sum1
Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 6269
Registered: 4-10-2014
Location: Unmoved
Member Is Offline
Mood: Organised
|
|
And I read "satanic acid". I would guess a little hot brimstone might work.
|
|
CharlieA
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 646
Registered: 11-8-2015
Location: Missouri, USA
Member Is Offline
Mood: No Mood
|
|
I see that I'm not the only dyslexic one! ![:D](./images/smilies/biggrin.gif) ![:D](./images/smilies/biggrin.gif)
|
|
DraconicAcid
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4301
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Offline
Mood: Semi-victorious.
|
|
Clearly holy water would be the best solvent......
Please remember: "Filtrate" is not a verb.
Write up your lab reports the way your instructor wants them, not the way your ex-instructor wants them.
|
|
Romix
Hazard to Others (Literally)
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 455
Registered: 19-6-2015
Member Is Offline
Mood: No Mood
|
|
No HNO3 doesn't dissolve it. And there's alot of HNO3 trapped in Stannic acid that's impossible to wash out. Adding HCl dissolves the gold with
Stannic acid.
|
|
zinc finger
Harmless
Posts: 25
Registered: 30-7-2019
Location: Germany
Member Is Offline
|
|
I see. So your goal is to leave gold behind and get rid of everything else?
Why don't you use NaOH or KOH and some heat?
|
|