TmNhRhMgBrSe
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 112
Registered: 4-7-2019
Member Is Offline
|
|
How to identify methanol, ethanol, isopropanol at home?
Some black heart pharmacies sell methanol to lie consumers. How to identify methanol, ethanol, isopropanol at home?
https://www.passiontimes.hk/article/02-21-2020/60243
[Edited on 20年07月04日 by CELamCheng]
sorry for bad english
|
|
Sulaiman
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3625
Registered: 8-2-2015
Location: 3rd rock from the sun
Member Is Offline
|
|
By smell,
BUT if not familiar or unable to distinguish then b.p. is usable.
unless the ethanol is dilute (<40%) when it could have similar BP to isopropanol.
P. S. Also flame test : methanol burns with a very faint blue flame, ethanol blue with a little yellow, isopropanol more yellow.
EDIT : see next post. None of the above would work. Sorry.
[Edited on 4-7-2020 by Sulaiman]
CAUTION : Hobby Chemist, not Professional or even Amateur
|
|
mackolol
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 459
Registered: 26-10-2017
Member Is Offline
Mood: Funky
|
|
Quote: Originally posted by Sulaiman ![](images/xpblue/lastpost.gif) | By smell,
BUT if not familiar or unable to distinguish then b.p. is usable.
unless the ethanol is dilute (<40%) when it could have similar BP to isopropanol.
P. S. Also flame test : methanol burns with a very faint blue flame, ethanol blue with a little yellow, isopropanol more yellow.
[Edited on 4-7-2020 by Sulaiman] |
I strongly doubt that the methanol would be pure. And if not, it isn't possible to recognise it by smell neither by flame colour...
|
|
outer_limits
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 139
Registered: 3-3-2020
Member Is Offline
Mood: hybridized
|
|
You could use Lucas' reagent to differentiate between secondary and primary alcohols.
To differentiate ethanol from methanol you could perform simple iodoform test
This combination is sufficient in qualitative context if you know that your solution consist of one or combination of 3 mentioned: MeOH, EtOH, IPrOH
Boiling point could be checked only if you are sure that you have one of them in its pure form, but I would rather rely on chemical tests.
[Edited on 4-7-2020 by outer_limits]
|
|
Texium
|
Thread Moved 8-2-2023 at 13:10 |