I have a solution of Cu(NO3)2 + Zn(NO3)2 + Co(NO3)2 + Sc(NO3)2 + Mn(NO3)2.
Any way to purify it to get the pure metals in any form?
[Edited on 21-12-2019 by Kamite]
|
|
unionised
International Hazard
   
Posts: 5135
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by Kamite  |
I have a solution of Cu(NO3)2 + Zn(NO3)2 + Co(NO3)2 + Sc(NO3)2 + Mn(NO3)2.
[Edited on 21-12-2019 by Kamite] |
No, you do not.
How did you come to the conclusion that you had?
Where did you get it?
|
|
Kamite
Harmless
Posts: 9
Registered: 3-7-2007
Member Is Offline
Mood: No Mood
|
|
Ok. Thank you, Unionised.
The question was to get the comments of an expert.
|
|
unionised
International Hazard
   
Posts: 5135
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
Well, I spent long enough at university studying chemistry, and even longer doing chemistry as my job that many people might think I am an expert.
In particular, I have the expertise required to recognise that Sc(NO3)2 doesn't exist.
So, once again...
No, you do not.
How did you come to the conclusion that you had?
Where did you get it?
|
|
DraconicAcid
International Hazard
   
Posts: 4413
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Offline
Mood: Semi-victorious.
|
|
If you actually had such a solution, separating the various metals from each other is the basis of standard first-year lab assignments. It's been a
standard lab assignment since they first added a lab component to first year chemistry courses.
http://file.akfarmahadhika.ac.id/E-BOOK/12-1213-akfarmahad-1...
Vogel wrote a full textbook on it. Chapter 5 goes through the steps for separating all the possible cations into groups, and then separating them out
from each other, taking advantage of the different complex ions they form, and the different solubilities of their various salts.
Please remember: "Filtrate" is not a verb.
Write up your lab reports the way your instructor wants them, not the way your ex-instructor wants them.
|
|
fusso
International Hazard
   
Posts: 1922
Registered: 23-6-2017
Location: 4 ∥ universes ahead of you
Member Is Offline
|
|
Can open the pdf, but cant see anything except the covers. Why is it blank?
[Edited on 191222 by fusso]
|
|
DraconicAcid
International Hazard
   
Posts: 4413
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Offline
Mood: Semi-victorious.
|
|
Quote: Originally posted by fusso  | Can open the pdf, but cant see anything except the covers. Why is it blank?
[Edited on 191222 by fusso] |
That's weird. I can read the whole thing.
Please remember: "Filtrate" is not a verb.
Write up your lab reports the way your instructor wants them, not the way your ex-instructor wants them.
|
|
Sulaiman
International Hazard
   
Posts: 3781
Registered: 8-2-2015
Member Is Online
|
|
I also had no problem, Adobe/Chrome/Win10
CAUTION : Hobby Chemist, not Professional or even Amateur
|
|
fusso
International Hazard
   
Posts: 1922
Registered: 23-6-2017
Location: 4 ∥ universes ahead of you
Member Is Offline
|
|
Im using firefox default pdf reader.
|
|
wg48temp9
National Hazard
  
Posts: 787
Registered: 30-12-2018
Location: not so United Kingdom
Member Is Offline
|
|
It does not open for me and I get a message the site can not be reached with a suggestion of opening a stored version on google which does open with
very small font that is not readable.
I am using chrome on win7. Yes my PC is old almost as old as my previous PC but I can run my old software on it.
At least when my tumble dryer got old I was offered a new one to stop the old one burning the house down. Why is it software manufactures get to
effectively decommission something I bought from them ??? (a rhetorical question)
PS: I wish everyone a great and happy Christmas or what/who ever you celebrate at this time of the year.
I will be away shortly to have some uric acid (probably) nodules zapped by a pulsed laser. Apparently I have accumulated several of them in two places
were its not a good idea to have nodules. Unfortunately access for the leaser (remind me to thank the guy that invented fibre optics) and basket, they
use to remove the broken up nodules, is small and not usually used as an entrance for anything. If the general randomness of life the universe and
everything and the NHS are nice to me I will be back here to finish my spree of posting more colourful graphs in a few days. I know your all looking
forward to them LOL
Apparently after the procedure, urinating will be eye wateringly painful for a day or two but no more so than passing a nodule. Just the thought has
brought tears to my eyes.
[Edited on 12/22/2019 by wg48temp9]
I am wg48 but not on my usual pc hence the temp handle.
Thank goodness for Fleming and the fungi.
Old codger' lives matters, wear a mask and help save them.
Be aware of demagoguery, keep your frontal lobes fully engaged.
I don't know who invented mRNA vaccines but they should get a fancy medal and I hope they made a shed load of money from it.
|
|
B(a)P
International Hazard
   
Posts: 1139
Registered: 29-9-2019
Member Is Offline
Mood: Festive
|
|
Works fine on my phone. Pixel with Android 10.
|
|
unionised
International Hazard
   
Posts: 5135
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
Still waiting for the OP to explain
Sc(NO3)2
I'm not holding my breath.
|
|
XeonTheMGPony
International Hazard
   
Posts: 1641
Registered: 5-1-2016
Member Is Offline
Mood: No Mood
|
|
It sucks lab scum, get adobe pdf reader.
Downloaded perfectly and readable with out issue.
[Edited on 22-12-2019 by XeonTheMGPony]
|
|
fusso
International Hazard
   
Posts: 1922
Registered: 23-6-2017
Location: 4 ∥ universes ahead of you
Member Is Offline
|
|
Nevermind, I just installed Foxit reader.
|
|
DraconicAcid
International Hazard
   
Posts: 4413
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Offline
Mood: Semi-victorious.
|
|
Well, coming up with a separation scheme may be fun. And it's probably been too long for the OP to use it as an answer to his homework question.
First, add excess sodium hydroxide. Zinc and scandium (presumably +3) form complex ions and stay in solution; the others precipitate as hydroxides.
Adding enough ammonium nitrate to the solution to buffer it around 8.5 will keep the zinc in solution as the ammonia complex, scandium will
precipitate out as the hydroxide (I think).
To the first precipitate, add concentrated ammonia. The copper and cobalt will dissolve as ammine complexes; the manganese will stay precipitated as
the hydroxide (possibly having oxidized to Mn(III) hydroxide or MnO2, depending on how much air is in contact with the solution.
To separate copper from cobalt, boil off most of the ammonia, and then acidify with acetic acid. Treat with sodium anthranilate- the copper compound
will precipitate at relatively low pH, whereas the cobalt compound is still soluble until the pH is raised significantly.
Please remember: "Filtrate" is not a verb.
Write up your lab reports the way your instructor wants them, not the way your ex-instructor wants them.
|
|
Kamite
Harmless
Posts: 9
Registered: 3-7-2007
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by DraconicAcid  | If you actually had such a solution, separating the various metals from each other is the basis of standard first-year lab assignments. It's been a
standard lab assignment since they first added a lab component to first year chemistry courses.
http://file.akfarmahadhika.ac.id/E-BOOK/12-1213-akfarmahad-1...
Vogel wrote a full textbook on it. Chapter 5 goes through the steps for separating all the possible cations into groups, and then separating them out
from each other, taking advantage of the different complex ions they form, and the different solubilities of their various salts.
|
Thank you very much. This is what I was looking for.
|
|
Kamite
Harmless
Posts: 9
Registered: 3-7-2007
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by DraconicAcid  | Well, coming up with a separation scheme may be fun. And it's probably been too long for the OP to use it as an answer to his homework question.
First, add excess sodium hydroxide. Zinc and scandium (presumably +3) form complex ions and stay in solution; the others precipitate as hydroxides.
Adding enough ammonium nitrate to the solution to buffer it around 8.5 will keep the zinc in solution as the ammonia complex, scandium will
precipitate out as the hydroxide (I think).
To the first precipitate, add concentrated ammonia. The copper and cobalt will dissolve as ammine complexes; the manganese will stay precipitated as
the hydroxide (possibly having oxidized to Mn(III) hydroxide or MnO2, depending on how much air is in contact with the solution.
To separate copper from cobalt, boil off most of the ammonia, and then acidify with acetic acid. Treat with sodium anthranilate- the copper compound
will precipitate at relatively low pH, whereas the cobalt compound is still soluble until the pH is raised significantly. |
Thank you again for replying. It seems easy. I am reading Vogel´s procedure.
In fact, in the solution are lanthanides aswell, as cerium, neodymium and gadollinium. The determination was done by XRF spectrometry.
Do you have a quick aswer at hand for the lanthanides?
It is a research just for fun, not a home work.
[Edited on 23-12-2019 by Kamite]
[Edited on 23-12-2019 by Kamite]
|
|
Kamite
Harmless
Posts: 9
Registered: 3-7-2007
Member Is Offline
Mood: No Mood
|
|
You are right, it is Sc(NO3)3.
As the determination was done by XRF spectrometry, I did not pay enough attention to this molecule that is a litle different to the others around.
|
|