Suggested media to clean brass part (water soluble)
Hello Mad Scientists,
I have several hundreds small pieces of brass that do have quite a bit of value but many of them are covered in a collection of oxides.
They are about the size of a 9mm shell with a bit of ceramic / steatite and a little brass screen inside (protected).
I have a rock tumbler that I would like to use to clean them so they can be sold.
Trouble is, I'm not sure of what polishing media would be best.
a) It has to be soluble
b) It has to be of aproximately the same hardness as the brass and steatite (not much!)
c) It shouldnt corrode the brass or make the existing corrosion worst.
There are several chemicals I thought of, salt being the most obvious but I'm afraid it'll tarnish the brass.
Magnesium Sulphate can be found in pharmacies in crystal form.
What do you think about MgSo4 hydrate ? Can you think of something else ?
The spirit of adventure was upon me. Having nitric acid and copper, I had only to learn what the words 'act upon' meant. - Ira Remsen
|
|
Deathunter88
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 514
Registered: 20-2-2015
Location: Beijing, China
Member Is Offline
Mood: No Mood
|
|
What about no media and just letting them grind against each other?
|
|
Herr Haber
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1236
Registered: 29-1-2016
Member Is Offline
Mood: No Mood
|
|
Not a bad idea !
I gave it a go for 30mn and the water came out green.
I'll let it run longer and see in a few hours.
I'd rather do it with a mild and abrasive because the parts are threaded and I'm not sure grinding against each other will get in there (thread is
outside).
There is also some writing but I doubt I'll get that.
I could get over a thousand Euros from that so any suggestion for abrasive or liquid / solvent to make a suspension or "mud" for lack of a better
word would be good.
I wouldnt even mind putting them through a Soxhlet to remove everything used in the process. Show me some Madness
The spirit of adventure was upon me. Having nitric acid and copper, I had only to learn what the words 'act upon' meant. - Ira Remsen
|
|
wg48temp9
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 771
Registered: 30-12-2018
Location: not so United Kingdom
Member Is Offline
|
|
See polishing material at https://www.vibratoryfinishing.co.uk/Consumables/
Some people have used granular cat litter, pieces of rubber/wood chips with polishing compound. Check out youtube.
Of cause none of those are soluble in water.
I am wg48 but not on my usual pc hence the temp handle.
Thank goodness for Fleming and the fungi.
Old codger' lives matters, wear a mask and help save them.
Be aware of demagoguery, keep your frontal lobes fully engaged.
I don't know who invented mRNA vaccines but they should get a fancy medal and I hope they made a shed load of money from it.
|
|
elementcollector1
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2684
Registered: 28-12-2011
Location: The Known Universe
Member Is Offline
Mood: Molten
|
|
My vote is for Epsom salt. Other options might be baking/washing soda (if they weren't so soft), and maybe sugar (again, unclear on the hardness,
which is the most important quality for abrasive polishing IIRC).
Elements Collected:52/87
Latest Acquired: Cl
Next in Line: Nd
|
|
bobm4360
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 59
Registered: 18-4-2011
Location: On a wretched little island.
Member Is Offline
Mood: No Mood
|
|
Try citric acid soak, 10g/100ml. With one piece, time until it looks good, then rinse with water. Dry with very low oven or hair dryer. Works great
on cartridges and similar sized brass pieces. When you have a good idea of the time it takes, then do bulk.
[Edited on 23-10-2019 by bobm4360]
|
|
Herr Haber
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1236
Registered: 29-1-2016
Member Is Offline
Mood: No Mood
|
|
Thank you all for all your inputs and suggestions.
Thanks for that link wg48temp9. I got a ball mill a couple months ago and now I go to sleep thinking about what I am going to put in next.
Pieces of rubber... I can think of a few use for that !
I got about 100 grams of big MgSO4.H20 crystals that I will try on another batch to see if it helps clean the thread.
I am not sure I can locate my citric acid but I have some sulphamic acid that might do the trick. I never had really good results from these methods
though. But sulphamic bath followed by drying + short time in the ball mill with Epsom salts might be a good combination.
So far, by just rubbing together in water I have cleaned most of the oxydes and debris that stuck to the brass but the threads remain green.
There is one positive aspect of this green oxyde: it makes the letters stand out.
I could stop the project "as is" but got to try some of your ideas ![:P](./images/smilies/tongue.gif)
The spirit of adventure was upon me. Having nitric acid and copper, I had only to learn what the words 'act upon' meant. - Ira Remsen
|
|
Herr Haber
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1236
Registered: 29-1-2016
Member Is Offline
Mood: No Mood
|
|
Well, sulphamic acid wasnt that great.
The brass turned "pink". Same thing happened years ago when cleaning .50 bullets so I should have known.
The spirit of adventure was upon me. Having nitric acid and copper, I had only to learn what the words 'act upon' meant. - Ira Remsen
|
|
Alkoholvergiftung
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 159
Registered: 12-7-2018
Member Is Online
|
|
I only know very deluted nitric Acid to "Burn" brass yellow. Than it gets it s Shining like new brass cartriges.
|
|
wg48temp9
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 771
Registered: 30-12-2018
Location: not so United Kingdom
Member Is Offline
|
|
Quote: Originally posted by Herr Haber ![](images/xpblue/lastpost.gif) | Well, sulphamic acid wasnt that great.
The brass turned "pink". Same thing happened years ago when cleaning .50 bullets so I should have known. |
Most acids tend to preferentially dissolve the zinc and leave amorphis copper, that's the pink color.
I am wg48 but not on my usual pc hence the temp handle.
Thank goodness for Fleming and the fungi.
Old codger' lives matters, wear a mask and help save them.
Be aware of demagoguery, keep your frontal lobes fully engaged.
I don't know who invented mRNA vaccines but they should get a fancy medal and I hope they made a shed load of money from it.
|
|
Herr Haber
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1236
Registered: 29-1-2016
Member Is Offline
Mood: No Mood
|
|
I used Epsom salts yesterday and... it worked beyond expectation on the parts that I tumbled with water the day before.
Of course it becomes a powder very fast and clogs every hole (important since the parts are antique gas burners) but it also dissolves well enough.
The threads were mostly clean and the burners being new but 70+ years old people will expect some tarnishing.
I'll be getting some more Espsom salt. I still have a few hundred burners to clean
The spirit of adventure was upon me. Having nitric acid and copper, I had only to learn what the words 'act upon' meant. - Ira Remsen
|
|