Li ion batteries same size but different capacities?


I have some LIs from 2 battery packs, they have the same cylindrical shape, diameter and length, but with wildly different capacities (0.8 & 2.6Ah). Is this possible? Are those claimed to have higher capacity actually have capacity similar to the lower ones?
(Claimed to be damaged/broken from someone else so don't ask me if they work or not)




View user's profile View All Posts By User
Sulaiman
International Hazard
*****




Posts: 3781
Registered: 8-2-2015
Member Is Online


[*] posted on 30-7-2019 at 09:35
approximately :


If the electrodes are thin then the cell can store a lot of energy,
if the electrodes are thick then the cell can deliver higher current.




CAUTION : Hobby Chemist, not Professional or even Amateur
View user's profile View All Posts By User
vmelkon
National Hazard
****




Posts: 669
Registered: 25-11-2011
Location: Canada
Member Is Offline

Mood: autoerotic asphyxiation

[*] posted on 30-7-2019 at 16:14


Quote: Originally posted by fusso  
I have some LIs from 2 battery packs, they have the same cylindrical shape, diameter and length, but with wildly different capacities (0.8 & 2.6Ah). Is this possible? Are those claimed to have higher capacity actually have capacity similar to the lower ones?
(Claimed to be damaged/broken from someone else so don't ask me if they work or not)


Sure. Why not.
The external package (cylindrical) might be large but it might contain a small battery.

This isn't anything new. I once bought a Ni-Cd "D" cell battery in 1992 and when I cut it open, I saw that it actually contains a slightly larger than an AA battery inside.




Signature ==== Is this my youtube page? https://www.youtube.com/watch?v=tA5PYtul5aU
We must attach the electrodes of knowledge to the nipples of ignorance and give a few good jolts.
Yes my evolutionary friends. We are all homos here.
View user's profile View All Posts By User
fusso
International Hazard
*****




Posts: 1922
Registered: 23-6-2017
Location: 4 ∥ universes ahead of you
Member Is Offline


[*] posted on 30-7-2019 at 22:40


Quote: Originally posted by vmelkon  
Sure. Why not.
The external package (cylindrical) might be large but it might contain a small battery.

This isn't anything new. I once bought a Ni-Cd "D" cell battery in 1992 and when I cut it open, I saw that it actually contains a slightly larger than an AA battery inside.
No, I mean the cylindrical LIs are the 18650 type.

[Edited on 190731 by fusso]




View user's profile View All Posts By User
wg48temp9
National Hazard
****




Posts: 787
Registered: 30-12-2018
Location: not so United Kingdom
Member Is Offline


[*] posted on 30-7-2019 at 22:57


As an other poster already stated, as confirmed by batterybro.com

"The two most important specs for 18650 cells are capacity measured in mAh (milliamp hours) and maximum continuous discharge measured in A (amperes). When selecting a battery type you must favor one over the other. High-capacity batteries have a low max. continuous discharge and high-amp batteries have a low capacity. Typical highest-capacity batteries in 2015 are ~3500mAh, and highest-amp batteries are 30A."




I am wg48 but not on my usual pc hence the temp handle.
Thank goodness for Fleming and the fungi.
Old codger' lives matters, wear a mask and help save them.
Be aware of demagoguery, keep your frontal lobes fully engaged.
I don't know who invented mRNA vaccines but they should get a fancy medal and I hope they made a shed load of money from it.
View user's profile View All Posts By User
Twospoons
International Hazard
*****




Posts: 1353
Registered: 26-7-2004
Location: Middle Earth
Member Is Offline

Mood: A trace of hope...

[*] posted on 31-7-2019 at 22:15


The cathode chemistry makes a big difference - it can be optimised for capacity or current delivery.
https://batteryuniversity.com/learn/article/types_of_lithium...