MgB2 compared to NbSn3


I am trying to determine what superconductor I should use for a project. I am making my own wires and materials so I have some questions about viability of each conductor. For the NbSn3 I would either coat a Niobium wire with tin and heat to form a coating of NbSn3 or I would mix tin and niobium metals together to make NbSn3, powder the mix, pack into a metal tube, heat, extrude using a wire rolling mil, and heat againl. For the MgB2 I would mix Magnesium with Boron and heat under an inert atmosphere at 800-1000 CĀ°. I would then powder it, pack into a copper or silver tube, heat, extrude using a roller mill, and heat again. Niobium and tin are relatively expensive, and I do not have any experience in electroplating to plate the tin onto the niobium. Boron and magnesium is cheaper and I already have magnesium. I can make the boron using the process of:
Na2B4O7 + HCl + H2O ā€”> H3BO3 ā€”> BO3 + Mg ā€”> B
MgB2 has a higher critical field than NbSn3 and can be cooled for cheaper than NbSn3.

Are there any details i am not accounting for?
View user's profile View All Posts By User
12thealchemist
Hazard to Others
***




Posts: 181
Registered: 1-1-2014
Location: The Isle of Albion
Member Is Offline

Mood: Rare and Earthy

[*] posted on 4-12-2018 at 08:39


I suspect it would be easier to form the intermetallic NbSn3 than MgB2 given boron's tendency to form many mixtures of B-B bonded species, for example the hexaboride. Synthesising pure MgB2 could be a challenge, despite the reduced cost.



Just my two pennyworth
My YouTube channel: www.youtube.com/channel/UC4t9tVlAk7ww1wgCVW4yUjg
Elements collected so far: 65; to collect: Ln, Rb, Sr, Ba, F, Kr, radioactives
View user's profile Visit user's homepage View All Posts By User
clearly_not_atara
International Hazard
*****




Posts: 2725
Registered: 3-11-2013
Member Is Offline

Mood: Big

[*] posted on 4-12-2018 at 21:23


I remember that once I asked a researcher who works with large superconducting magnets why NbSn3 is preferred over MgB2. He said that the former compound is much more ductile and easy to work with while MgB2 does not form wires easily.

trace impurities can strongly affect the properties of a superconductor. Synthesizing the pure material is important.




Quote: Originally posted by bnull  
you can always buy new equipment but can't buy new fingers.
View user's profile View All Posts By User
ninhydric1
Hazard to Others
***




Posts: 345
Registered: 21-4-2017
Location: Western US
Member Is Offline

Mood: Bleached

[*] posted on 4-12-2018 at 22:00


Niobium can be easily bought on Ebay as well, so making NbSn3 is probably a lot simpler than attempting to purify the various side products that might arise from the Mg + B reaction.



The philosophy of one century is the common sense of the next.
View user's profile View All Posts By User
Jackson
Hazard to Others
***




Posts: 189
Registered: 22-5-2018
Location: U S of A
Member Is Offline

Mood: :) Happy about new glassware :)

[*] posted on 5-12-2018 at 10:05


It sounds like I will probably go with NbSn3 due to it sounding like its easier to make successfully as compared to MgB2. Should I use a powder in tube method or should I make films of tin on Niobium wire and heat to cause diffusion of the tin into the niobium?
View user's profile View All Posts By User
Jackson
Hazard to Others
***




Posts: 189
Registered: 22-5-2018
Location: U S of A
Member Is Offline

Mood: :) Happy about new glassware :)

[*] posted on 5-12-2018 at 10:35


Another process is one where a bronze made of tin copper and niobium is draw into wires, wound into the desired shape, and heat treated to form the Nb3Sn. I dont know if this is more viable or not but it seems like it could work.