Pages:
1
2 |
AJKOER
Radically Dubious
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3026
Registered: 7-5-2011
Member Is Offline
Mood: No Mood
|
|
Path to Al Acetate and a Tinge of Cyanide(?) via Al Foil/ Carbon/ 5% Vinegar/ 3% H2O2/ Sea Salt and Delayed NH3 (aq) Addition
This thread’s original intent was to explorer the possible formation of aluminum acetate(s) by the direct action of aluminum metal (sourced from
Aluminum foil that has been heat treated to redness by a gas flame) acted upon by household vinegar (5% acetic acid) in the presence of 3% hydrogen
peroxide, a graphite rods (sold for use in pencils), and a small amount of sea salt. The mix was heated in a microwave for several 30 second sessions
which resulted in a limited formation of a fine white power. Acceleration of the attack of the aluminum metal apparently occurred upon the further
addition of pure ammonia water to the mix followed by microwave heating. This is not surprising given that the literature notes the corrosive action
of ammonium chloride on aluminum (and other metals, see https://www.researchgate.net/publication/271164226_Effect_of... ).
I believe the underlying reaction to have radical component and can be viewed as a takeoff of my thread ‘Acidic Radicals Based Synthesis’ at http://www.sciencemadness.org/talk/viewthread.php?tid=94166#... .
BACKGROUND
For background I start with Wikipedia comments on Aluminum tri-acetate preparation (link: https://en.wikipedia.org/wiki/Aluminium_triacetate ), to quote:
“According to the CRC Handbook of Inorganic Compounds, aluminium triacetate is a white, water-soluble solid and is usually prepared from aluminium
chloride or directly from aluminium by heating in an acetic acid solution with acetic anhydride.[1]
3 CH3COOH + AlCl3 → Al(CH3CO2)3 + 3 HCl
6 CH3COOH + 2 Al → 2 Al(CH3CO2)3 + 3 H2
Theoretically all of the aluminium / acetate / hydroxide salts can be prepared from aluminium hydroxide or sodium aluminate and acetic acid, but
formation of the triacetate only occurs in the absence of water.[4] In solutions, the diacetate is the major product formed...”
My presented path could be viewed, in part, as noted above via an in situ created Al(OH)3 (from the action of hydroxyl radicals as derived from H2O2).
Suggested path:
Al/Carbon/CH3HCO2-/H2O2/Sea Salt System:
------------------------------------------------------------
2 x [ Al --> Al(lll) + 3 e- ]
6 x [ e- + nH2O --> e-(aq) ]
3 x [ H2O2 = H+ + HO2- ]
3 x [ H+ + e-(aq) = •H ]
3 x [ •H + HO2- = •OH + OH- ]
3 x [ •OH + e-(aq)- = OH- ]
-----------------------------------------------
2 Al + 3 H2O2 ---> 2 Al(OH)3
Then, the action of dilute acetic acid acting on freshly created Al(OH)3.
A confirmation of the above path can be find in a source. To quote from ‘Kinetics of Corrosion Inhibition of Aluminum in Acidic Media by
Water-Soluble Natural Polymeric Pectates as Anionic Polyelectrolyte Inhibitors’ by Refat M. Hassan and Ishaq A. Zaafarany, in Materials (Basel).
2013 Jun; 6(6): 2436–2451, doi: 10.3390/ma6062436, link: https://www.ncbi.nlm.nih.gov/pmc/articles/PMC5458939/ :
“The corrosion rate was found to be a function of the concentration of the acid. This result indicates that at least one of the corrosion paths of
dissolution of Al metal in HCl solution should involve the presence of hydrogen ions in the rate-determining step…
3.1. Corrosion Mechanism
We propose a suitable mechanism of corrosion, in accordance with the above experimental observations. The corrosion of metal involves an
electrochemical process [47,48,49] resulting from dissolution of Al metal in the acid. This process can be expressed by the anodic and cathodic
processes, which are defined by Equations (4) and (5), respectively,
Al(s) <--Ox--> Al3+ + 3 e- (4)
2 H+ + 2 e- <--Red--> H2 (5)
The overall electrochemical process can be written as follows:
(6) 2 Al(s) + 6 H+ <-->2 Al3+ + 3 H2(g) (6)
The cathodic reaction produces Hchemisorbed by picking up an electron that released in the anodic reaction (H+ + e = Hchemisorbed ) in Al corrosion in
HCl. In such acidic solutions, the Hchemisorbed on the metal surface reacts by combining with other adsorbed Hchemisorbed to form H2 gas molecule,
which bubbles from the metal surface. A very small amount of the uncombined Hchemisorbed will remain; however, this amount does not affect the whole
process. “
Further possible path explaining the increased corrosion of Aluminum (creating Al ions) in the presence of ammonium ion:
Al = Al(lll) + 3 e-
3 x [ NH4+ = NH3 + H+ ]
3 x [ e- + H+ = •H ]
3 x [ NH3 + •H (or •OH) = •NH2 + H2 (or H2O) ]
Net: Al + 3 NH4+ = Al(lll) + 3 •NH2 + 3 H2 (g)
With the creation of the amidogen radical, a possible REDOX with a metal M:
•NH2 + M(ll) + H+ = NH3 + M(lll) (See, for example, (6) on p. 111O for a Nickel complex at https://www.nist.gov/sites/default/files/documents/srd/jpcrd... )
Interestingly, here is a long article noting "Amine radical cations are highly useful reactive intermediates in amine synthesis" in an organic
chemistry setting, see https://www.ncbi.nlm.nih.gov/pmc/articles/PMC3817571/ .
Now, in the case of elemental Aluminum, a corresponding suggested reaction per above would be:
.NH2 + ⅓ Al + H+ = NH3 + ⅓ Al(lll)
(As ⅓ Al --> ⅓ Al(lll) + e-
H+ + e- = •H
•H + •NH2 = NH3 )
In the presence of H2O2, a source of O2 on decomposition, could further interact with any formed amidogen radical as follows:
•NH2 + O2 = •H + HONO
Source: ‘Reaction between the amidogen radical, NH2, and molecular oxygen in low-temperature matrixes’, by John N. Crowley and John R. Sodeau, in
J. Phys. Chem., 1989, 93 (12), pp 4785–4790, DOI: 10.1021/j100349a021, link: https://pubs.acs.org/doi/10.1021/j100349a021 or http://www.diva-portal.se/smash/get/diva2:730237/FULLTEXT01.... Table 2.1 on page 25 suggesting products of NO + H2O and in the presence of H2O2
leads also to NO2 in water.
Any formed HONO (or HNO2) is unstable (see https://en.wikipedia.org/wiki/Nitrous_acid ) likely decomposing as follows:
2 HNO2 = NO + NO2 + H2O
As such any NO2 together or HNO2 (especially in the presence of NaCl acting in a similar fashion to HNO3), are reported to attack Aluminum metal.
This is likely due to a Fenton-type REDOX reaction in the presence of elemental Aluminum with any created HNO3 or HNO2) See, for example, "Fenton
chemistry in biology and medicine*" by Josef Prousek, to quote reaction (15) on page 2330:
"For Fe(II) and Cu(I), this situation can be generally depicted as follows [20,39],
Fe2+/Cu+ + HOX → Fe3+/Cu2+ + •OH + X- (15)
where X = Cl, ONO, and SCN. "
And my prior comments at http://www.sciencemadness.org/talk/viewthread.php?tid=30473#... .
Less likely but possible another reaction of interest includes creation of the acetate radical anion (see https://pubs.acs.org/doi/abs/10.1021/ja00105a032?journalCode... ):
CH3CO2H <-> H+ + CH3CO2-
CH3CO2- + •H --> •CH2CO2- + H2 or •CH2CO- + H2O
•CH2CO2- + •NH2 = CH2NH2- + CO2
Or: •CH2CO- + •NH2 = CH2CONH2
With respect to the last compound, note a recent comment I may on SM referencing cyanide paths (see http://www.sciencemadness.org/talk/viewthread.php?tid=103289 ):
Quote: Originally posted by AJKOER ![](images/xpblue/lastpost.gif) | .....
........
I did notice this article (see 'Excision of CN− and OCN− from acetamide and some amide derivatives triggered by low energy electrons' by Constanze
Koenig-Lehmann, et al, abstract at https://pubs.rsc.org/en/Content/ArticleLanding/2008/CP/b8121... ). To quote in part:
"Low energy electron attachment to acetamide and some of its derivatives shows unique features in that the unimolecular reactions of the transient
anions are remarkably complex, involving multiple bond cleavages and the formation of new molecules. Each of the three compounds acetamide
(CH3C(O)NH2), glycolamide (CH2OHC(O)NH2) and cyanoacetamide (CH2CNC(O)NH2) shows a pronounced resonance located near 2 eV and decomposing into CN−
along a concerted reaction forming a neutral H2O molecule and the corresponding radical (methyl and methoxy). "
Per the above, I would express the basis of a possible reaction as:
Al --> Al(lll) + 3 e-
3 x [ CH3C(O)NH2 + e- --> •CH3 + CN- + H2O ]
Net: Al + 3 CH3C(O)NH2 --> 3 •CH3 + Al(lll) + 3 CN- + 3 H2O
......
[Edited on 10-11-2018 by AJKOER][/rquote]
where the corresponding net reaction in the current case could be:
Net: Al + 3 CH2CONH2 --?--> 3 •CH2 + Al(lll) + 3 CN- + 3 H2O
indicating a possible, but small, cyanide presence.
In the current experiment, the action of the hydroxyl radical on elemental carbon is a path to CO:
•OH + C = •H + CO (EDIT see comments and references at http://www.sciencemadness.org/talk/viewthread.php?tid=97845#... )
Also, given the possible presence of CO, from the same referenced SM thread above:
[Edited on 4-10-2014 by AJKOER][/rquote]
--------------------------------------------------------------------
A bit harder, try this path (see https://chemiday.com/en/reaction/3-1-0-261):
CO + NH3 --500 C, Al2O3--> HCN + H2O
"Carbon monoxide react with ammonia to produce hydrogen cyanide and water. The technical method production hydrogen cyanide. This reaction takes place
at a temperature of 500-800°C, an overpressure. In this reaction, the catalyst is can be V2O5, CeO2 Al2O3, ThO2."
Text sounds like a translation.
At such high temperatures, I would expect:
NH3 + Heat ---> •H + •NH2
based on the action of hv on ammonia (see R1 at https://journals.ametsoc.org/doi/pdf/10.1175/1520-0469%28197... )
Then, subsequent reactions with CO forming HCN and H2O.
------------------------------------------------------------------
The above speculated radical mechanism is interesting, if correct, as the hydrogen atom radical can be formed at RT by the action of NaOH (or HCl) on
Aluminum metal where some .H radical could be imbued on the surface of the Aluminum. My prior related comment:
Quote: Originally posted by AJKOER ![](images/xpblue/lastpost.gif) |
.......
Next, imbue the surface of Mg or Al with the hydrogen atom radical (from the traditional nascent hydrogen generation methods based on say Al/NaOH).
One may assume that the •H radical functional behaves (per its seemingly reversible formation reaction: e- + H+ = •H ) as apparently a (e-,H+)
pair acting on ions. For an example from 'Hydrometallurgy 2008: Proceedings of the Sixth International Symposium', p. 818, a commercial reductive
leaching equation, to quote:
" PbS + 2 •H = Pb + H2S (5) " (see https://books.google.com/books?id=1etfSdk55SYC&pg=PA818&... )
which I view functionally as follows:
Pb(+2)S(2-) + 2 (e-, H+) = Pb + H2S (g)
......
[Edited on 4-10-2018 by AJKOER] |
So the surface .H could be further enlisted in other (unspecified) reactions with CO per above via the radical reaction:
•H + NH3 = H2 + •NH2
which are the same radicals (.H, .NH2) postulated above to be formed at high temperatures that eventually result in a HCN product.
[Edited on 9-11-2018 by AJKOER] |
Some possible paths to a cyanide presence. Assuming the presence of CO, I would suggest also the simple path:
CO + •NH2 = •CONH2 (or •CN + H2O)
•H2N + CO = •H2NCO (or •NC + H2O)
•H2NCO + •CONH2 = H2NC(O)C(O)NH2 (oxamide)
(Or: •NC + •CN = NCCN )
Per Wiki on Cyanogen (https://en.wikipedia.org/wiki/Cyanogen ) to quote:
“Cyanogen is the anhydride of oxamide:
H2NC(O)C(O)NH2 → NCCN + 2 H2O
…….
Like other cyanides, cyanogen is very toxic, as it readily undergoes reduction to cyanide, …”
Given the theory presented above, the observed pale blue coloration developed in the synthesis following the introduction of pure aqueous NH3 in
distilled water, may be due to HCN or a harmless bluish tinge created from the addition of aqueous ammonia to an aluminum salt (see https://mysite.du.edu/~jcalvert/phys/alumin.htm and search on 'bluish').
In any event, perform the experiment in a well vented area.
I believe the reduction in color upon boiling with added vinegar, suggests a successful preparation with a minor threat of HCN.
EXPERIMENT DETAILS
----------------------------------
Started with 200 mL of 5% white distilled household vinegar, 100 mL H2O2, ¼ and increased to ¾ teaspoon of over the counter sea salt, and flame
heated Al foil with a preheated surface area of 10.7 sq inches. Also note, I was short on my supply of carbon and employed just 2 small low surface
area graphite rods. Ideally, one would like to have a ratio of Aluminum surface area to C that is small to encourage corrosion chemistry with the Al,
and not otherwise to foster reactions leading to, say CO, at the more noble carbon electrode. Also, activated carbon (AC) may be superior to graphite
as per this source (https://www.researchgate.net/publication/239705822_Generatio...) hydroxyl radicals are created in aqueous solutions with microwave radiation
treatment.
[Edited on 24-11-2018 by AJKOER]
[Edited on 25-11-2018 by AJKOER]
|
|
AJKOER
Radically Dubious
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3026
Registered: 7-5-2011
Member Is Offline
Mood: No Mood
|
|
Start and near finish pictures.
Note, Aluminum consumed except for small piece that was not heat treated.
![Photo Editor-20181124_104959.jpg - 352kB](http://www.sciencemadness.org/talk/files.php?pid=555726&aid=71934)
[Edited on 24-11-2018 by AJKOER]
|
|
AJKOER
Radically Dubious
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3026
Registered: 7-5-2011
Member Is Offline
Mood: No Mood
|
|
Final picture taken in a larger vessel (due to the added vinegar) taken some 12 hours after decanting, adding more vinegar and heating. Note, blue
marks in the picture are actually on the exterior of the vessel.
![Photo Editor-20181124_120119.jpg - 246kB](http://www.sciencemadness.org/talk/files.php?pid=555728&aid=71936)
[Edited on 25-11-2018 by AJKOER]
|
|
AJKOER
Radically Dubious
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3026
Registered: 7-5-2011
Member Is Offline
Mood: No Mood
|
|
More earlier pictures
|
|
UC235
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 565
Registered: 28-12-2014
Member Is Offline
Mood: No Mood
|
|
What is this incoherent garbage. You corroded some aluminum foil in salty vinegar and made aluminum hydroxide suspension and a mess.
|
|
unionised
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
"aluminum metal (sourced from Aluminum foil that has been heat treated to redness by a gas flame)"
Why bother?
Mind you, that question can be asked of the whole thread.
|
|
AJKOER
Radically Dubious
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3026
Registered: 7-5-2011
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by unionised ![](images/xpblue/lastpost.gif) | "aluminum metal (sourced from Aluminum foil that has been heat treated to redness by a gas flame)"
Why bother?
Mind you, that question can be asked of the whole thread. |
As to why aluminum foil should be heated in a flame (in places till it is red), apparently, the heat treatment weakens the protective coating and
disrupts the annealing process (which makes the Al foil seemingly inert). Here is an extract of my prior comment on this topic:
Quote: Originally posted by AJKOER ![](images/xpblue/lastpost.gif) | .....
I can across an excellent white paper (link https://www.google.com/url?sa=t&source=web&rct=j&... ) detailing reaction of Aluminum and water with promoters to address the
protective Al2O3 layer. To quote from page 7:
"It has been shown that mixtures of aluminum and aluminum oxide (Al2O3) powders are reactive with water in the pH range of 4-9 (11-13) and at
temperatures of 10-90 oC. These Al-Al2O3 powder mixtures must be heavily ball-milled together in order to produce hydrogen reactions. Hydrogen can
be evolved at room temperature using essentially neutral water, although the hydrogen evolution rate increases with increasing temperature. "
Also, to quote page 8: "The aluminum oxide may be in the form of bayerite (Al(OH)3), boehmite (AlO(OH)), gamma alumina (γ-Al2O3), or alpha alumina
(α-Al2O3). Alpha alumina powder was reported to give the maximum hydrogen evolution. It has been speculated that the milling of aluminum and aluminum
oxide powders together helps to mechanically disrupt the adherent and coherent oxide layers present on the aluminum powder, and that this is the
reason for the enhanced hydrogen generation in pH neutral water (11-13).
However, recent research has suggested that the enhancing effect of aluminum oxide on the reactivity of aluminum with water may also be
mechanochemical in nature (14). Aluminum powders that were reacted with fine boehmite powders at elevated temperatures produced a layer of
fine-grained, mechanically weak gamma alumina on the surfaces of the aluminum powders. "
Apparently weakened gamma alumina reacts as follows:
Induction Stage: Al2O3 + H2O ---) 2 AlOOH
Followed by:
6 AlOOH + 2 Al ----) 4 Al2O3 + 3 H2
leading to the rupturing of Aluminum oxide layer.
So, the burning of processed Al foil could produce some weaken gamma alumina as could occur also in the salt cake example. Given the moderate pH range
upon which the composition of Al and weakened gamma Al2O3 is subject to rupture per the above reactions, we have a tenative explanation of the
initialization reaction in the electrochemical setting.
[Edited on 23-6-2014 by AJKOER] |
The above coupled with several experimental verifications on my part confirm the theory.
But of course, you can easily verify it yourself as either the Al foil rapidly dissolves in some situations or it does not!
[Edited on 24-11-2018 by AJKOER]
|
|
AJKOER
Radically Dubious
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3026
Registered: 7-5-2011
Member Is Offline
Mood: No Mood
|
|
Note, the path I outlined appears (as all the Al is gone!) effective and does not generate a large amount of the insoluble aluminum diacetate as
mentioned in this thread https://www.reddit.com/r/chemistry/comments/4m6to8/make_alum... .To quote:
"If Al(CH*3CO2)3* (aluminium tri-acetate) is what you need, then trying to make this from aluminium metal and acetic acid is not the easiest or most
efficient method. It is better to react the aluminium metal with a solution of sodium hydroxide first to make a solution of NaAl(OH)4 (sodium
aluminate). This way, the aluminium oxide is not a problem, since it reacts with NaOH solution to make the same product:
Al*2O3* + 2 NaOH + 3 H*2O -----> 2 NaAl(OH)4*
This is quite slow and doesn't produce any gas, so it can look like the reaction is doing nothing while the aluminium oxide dissolves. But once the
oxide is all gone, the aluminium metal underneath reacts to form more sodium aluminate. This reaction is much faster:
2 Al + 6 H*2O + 2 NaOH -----> 2 NaAl(OH)4* + 3 H*2*
Once you have a solution of sodium aluminate, the next step is to add 3 molar equivalents of acetic acid:
NaAl(OH)4 + 3 CH*3CO2H -----> CH3CO2Na + Al(CH3CO2)2*OH
So why not add 4 equivalents of acetic acid to make Al(CH*3CO2)3? Because aluminium tri-acetate is water soluble, while aluminium di-acetate is not.
So in the reaction above, the Al(CH3CO2)2OH precipitates as a solid, while the CH3CO2*Na (sodium acetate) byproduct stays in solution.
So you can then isolate pure Al(CH*3CO2)2*OH and then add this to one more equivalent of acetic acid to make aluminium tri-acetate solution:
Al(CH*3CO2)2OH + CH3CO2H -----> Al(CH3CO2)3* + H*2*O
Then to make solid Al(CH*3CO2)3*, just leave the solution to evaporate (if you want nice crystals) or boil the water off to make a powder."
[Edited on 24-11-2018 by AJKOER]
|
|
AJKOER
Radically Dubious
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3026
Registered: 7-5-2011
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by UC235 ![](images/xpblue/lastpost.gif) | What is this incoherent garbage. You corroded some aluminum foil in salty vinegar and made aluminum hydroxide suspension and a mess.
|
Thanks for the comment sharing concerns some may have.
With respect to 'incoherent', I refer you to my prior referenced thread employing acidic radicals (link: http://www.sciencemadness.org/talk/viewthread.php?tid=94166#... where interestingly, with the source article of that thread having a web
publication date of September 15, 2017, perhaps many textbooks are so outdated, they could be 'garbage').
Thanks also in mentioning the presence of salt, in particular sea salt, which apparently has many roles. First, as my prep is based on an
electrochemical cell (or battery cell), it is in the province of electrochemistry and can be referred to as an electrosynthesis (see https://en.wikipedia.org/wiki/Electrosynthesis). In that regard, NaCl serves in the role of an electrolyte. Second, in the corrosion chemistry of
Aluminum, NaCl can apparently engage in surface attacks of the protective Al2O3 layer (see this review for more details http://jes.ecsdl.org/content/161/9/C421.full ). Lastly, not pure NaCl, but sea salt, which some researchers have noted interestingly that it may
be chemically more active (perhaps from multiple trace elements which can be catalytic and I would support this conjecture by the apparent biochemical
sensitivity of fish to replacing sea salt with pure NaCl, read https://books.google.com/books?id=H1BGAAAAYAAJ&pg=PA72&a... ).
Now, the comment may be partially correct on the aluminum hydroxide suspension perhaps created upon the addition of aqueous NH3, due to the bluish
tint (and perhaps not the more problematic HCN), per this source (https://mysite.du.edu/~jcalvert/phys/alumin.htm ) to quote:
"Aluminium dissolves slowly in dilute hydrochloric acid to make a clear solution. When ammonium hydroxide is added, a characteristic translucent gel
precipitates, with a bluish tinge."
However, upon decanting to remove most of the mess, and then the reduction of color upon addition of more acetic acid with microwave heating, implies
to me likely removal of the Al(OH)3 translucent gel or other created compound.
-------------------------------------------------
Anyone, however, is free to follow the CRC Handbook of Inorganic Compounds, to prepare aluminium triacetate from aluminium chloride or directly from
aluminium by heating in an acetic acid solution with acetic anhydride.
[Edited on 25-11-2018 by AJKOER]
|
|
AJKOER
Radically Dubious
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3026
Registered: 7-5-2011
Member Is Offline
Mood: No Mood
|
|
Both pictures taken 1 day after decanting. Note, a small amount of fine white precipitate (possibly Aluminum diacetate) and the bottom picture (taken
in sunlight minutes latter) displays a green tint (ferrous (?) from small iron content of the Al foil or found in vinegar). Solution shows not sign of
viscosity.
![Photo Editor-20181125_075326.jpg - 288kB](http://www.sciencemadness.org/talk/files.php?pid=555911&aid=71957)
![Photo Editor-20181125_075251.jpg - 197kB](http://www.sciencemadness.org/talk/files.php?pid=555911&aid=71959)
[Edited on 25-11-2018 by AJKOER]
|
|
unionised
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by AJKOER ![](images/xpblue/lastpost.gif) |
As to why aluminum foil should be heated in a flame (in places till it is red), apparently, the heat treatment weakens the protective coating and
disrupts the annealing process (which makes the Al foil seemingly inert).
[Edited on 24-11-2018 by AJKOER] |
The process for annealing aluminum is to heat it near to the melting point.
So, your idea of "disrupting" the annealing, by annealing it makes no sense.
|
|
AJKOER
Radically Dubious
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3026
Registered: 7-5-2011
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by unionised ![](images/xpblue/lastpost.gif) | .....
The process for annealing aluminum is to heat it near to the melting point.
So, your idea of "disrupting" the annealing, by annealing it makes no sense. |
Yes, but a better path to growing a strong protective Al2O3 layer is via anodizing (see https://www.thebalance.com/what-is-anodizing-2340009 ) and not heating.
Also, the qualification is heating till the Al foil glows red (high temperature induced disruption I would suspect).
---------------------------------------------------------
A corrosion related point, I claim my ammonia water was likely pure NH3 (aq) as I prepared it by placing distilled water (DW) in a large mouth vessel
together in a container (which was twice the volume of the DW) loaded with yellow colored household ammonia rich in surfactants, etc. I carefully
placed a plug (prepared by wrapping layers of Al foil around my finger) full of NaCl into the household ammonia and sealed the entire chamber. As NH3
has much reduced solubility in seawater, I expected with time the DW would amass a good amount of the liberated ammonia from the now salt rich
household ammonia.
A day latter, I opened the vessel, I was surprised to see the amount of bubbling/attack performed on the Al plug! This level of corrosion by NH3/NaCl
is why I added the pure NH3 water to this threads reaction mix as I was not impressed by the level of attack I was seeing. The result is apparent!
As to the mechanics of the attack by NH4+, one source notes 'a pH and corrosion potential changes with time', see http://citeseerx.ist.psu.edu/viewdoc/download?doi=10.1.1.849... . My suggested radical attack either directly by the •NH2 radical, or from
products generated from associated REDOX reactions, is my assessment, which is in line with this observation.
Further support for my radical based path is a case from 1983 (see https://www.researchgate.net/publication/271683294_Stabiliza... ) of stabilizing corrosion in the presence of both Al and Cu. The answer is
washing with an aerated mix of NH3/NH4+. My take on the mechanics is that the Cu/NH3/O2 battery produces solvated electrons, which in the presence of
O2, makes superoxide (•O2-). This latter radical anion is great in scavenging many radicals (including in the human body) as illustrated as follows:
•NH2 + •O2- + H+ (from water) = NH3 + O2
•OH + •O2- = OH- + O2
•CO3- + •O2- = CO3(2-) + O2
Also, a reaction with Al3+, on the Al surface, which could be impeding (by creating the aluminum semi reduced superoxide product below, which is
capable of converting metal ions to low valence states, and associated levels of solubility like with cuprous salts, see cited reference below):
Al3+ + •O2- = [Al(•O2-)](2+) (see comments and sources at http://www.sciencemadness.org/talk/viewthread.php?tid=96347#... )
all of which may reduce the progress of a corrosive attack.
[Edited on 25-11-2018 by AJKOER]
|
|
DraconicAcid
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4298
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Offline
Mood: Semi-victorious.
|
|
Why would it be different from any of his other "ideas"?
Please remember: "Filtrate" is not a verb.
Write up your lab reports the way your instructor wants them, not the way your ex-instructor wants them.
|
|
Tsjerk
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3026
Registered: 20-4-2005
Location: Netherlands
Member Is Offline
Mood: Mood
|
|
That, and there is no protective coating on aluminium foil, except for the couple of nano meters of aluminium oxide. Heating it over a flame will make
it brittle and effectively convert it to aluminium oxide. Try to measure volume of hydrogen gas evolved with NaOH with and without heating it to red
dullness if you don't believe me.
|
|
AJKOER
Radically Dubious
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3026
Registered: 7-5-2011
Member Is Offline
Mood: No Mood
|
|
Thanks Draconic acid but here is an extract of the original discussion as to the process:
Quote: Originally posted by AJKOER ![](images/xpblue/lastpost.gif) | .....
I can across an excellent white paper (link https://www.google.com/url?sa=t&source=web&rct=j&... ) detailing reaction of Aluminum and water with promoters to address the
protective Al2O3 layer. To quote from page 7:
"to quote page 8: "The aluminum oxide may be in the form of bayerite (Al(OH)3), boehmite (AlO(OH)), gamma alumina (γ-Al2O3), or alpha alumina
(α-Al2O3). Alpha alumina powder was reported to give the maximum hydrogen evolution. It has been speculated that the milling of aluminum and aluminum
oxide powders together helps to mechanically disrupt the adherent and coherent oxide layers present on the aluminum powder, and that this is the
reason for the enhanced hydrogen generation in pH neutral water (11-13).
However, recent research has suggested that the enhancing effect of aluminum oxide on the reactivity of aluminum with water may also be
mechanochemical in nature (14). Aluminum powders that were reacted with fine boehmite powders at elevated temperatures produced a layer of
fine-grained, mechanically weak gamma alumina on the surfaces of the aluminum powders. "
Apparently weakened gamma alumina reacts as follows:
Induction Stage: Al2O3 + H2O ---) 2 AlOOH
Followed by:
6 AlOOH + 2 Al ----) 4 Al2O3 + 3 H2
leading to the rupturing of Aluminum oxide layer.
[Edited on 24-11-2018 by AJKOER] |
So, there is a white paper quoted again above referring to a mechanochemical process that starts on page 8.
Then, on page 9, there is then a diagram in the white paper from which I reprinted the author's cited reaction path leading to H2 and bursting of the
Al2O3 layer.
Sorry, but I don't see my 'idea', and I doubt anyone wants to assess my artistic talent in attempting to reproduce that figure.
The 2008 work I am quoting from is titled 'Reaction of Aluminum with Water to Produce Hydrogen' by John Petrovic (Ph.D, Materials Science, see https://www.linkedin.com/in/john-petrovic-49aa8241 ) and George J Thomas, who are consultants to the U.S. Department of Energy on the Hydrogen
Program. Both authors are retired scientists from Los Alamos National Laboratory and Sandia National Laboratories, respectively.
[Edited on 25-11-2018 by AJKOER]
|
|
Texium
Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4546
Registered: 11-1-2014
Location: Salt Lake City
Member Is Offline
Mood: PhD candidate!
|
|
Alright. Let's take some time to pick this one apart. Quote: Originally posted by AJKOER ![](images/xpblue/lastpost.gif) | "Aluminum powders that were reacted with fine boehmite powders at elevated temperatures produced a layer of fine-grained, mechanically weak gamma
alumina on the surfaces of the aluminum powders." | The only thing the authors describe here in detail that
relates to heating is heating a mixture of aluminum powder and a particular type of fine aluminum oxide powder. This is an
entirely different situation than sticking a piece of aluminum foil in a flame. Without any actual analysis of your supposed "flame activated
aluminum" and more conclusive results, the paper that you cite has absolutely NO relevancy to what you're talking about.
Quote: Originally posted by AJKOER ![](images/xpblue/lastpost.gif) | So, there is a white paper quoted again above referring to a mechanochemical process that starts on page 8.
Then, on page 9, there is then a diagram in the white paper from which I reprinted the author's cited reaction path leading to H2 and bursting of the
Al2O3 layer.
Sorry, but I don't see my 'idea'. | The problem is that you extrapolated from an experiment that is entirely
different than what you conducted, and tried to use that as evidence for your dubious and unquantitative claims, and then you took the assumptions
that you made from that and made more assumptions that you attempt to back up with more papers that would only be even tangentially related if some of
your assumptions were correct (which they aren't).
You are wrong on so many levels that this barely scratches the surface. Maybe you have some false impression that the crackpot experiments and
conjecture that you often post here go unchallenged because everyone believes you, or people don't know how to refute you. The truth is though, it's
just exhausting, and nobody wants to waste their time doing it when you're just going to go on believing your fantasy version of chemistry and never
actually learn a damn thing.
|
|
Texium
|
Thread Moved 25-11-2018 at 12:55 |
Tsjerk
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3026
Registered: 20-4-2005
Location: Netherlands
Member Is Offline
Mood: Mood
|
|
Quote: Originally posted by Texium (zts16) ![](images/xpblue/lastpost.gif) | The problem is that you extrapolated from an experiment that is entirely different than what you conducted, and tried to use that as evidence for your
dubious and unquantitative claims, and then you took the assumptions that you made from that and made more assumptions that you attempt to back up
with more papers that would only be even tangentially related if some of your assumptions were correct (which they aren't). |
What you describe is his hallmark indeed.
I tried to refute him, but he keeps, and keeps, and keeps coming with crap about why he isn't wrong. I can't imaging how much time AJOEKER needed to
write his 2400+ posts... Normally you would think someone with a name like AJOEKER is "a joker", but that would be one hell of an elaborate "joke".
I didn't know there was a term like fractal wrongness, I love it and it spot on in this case.
Quote: |
Fractally wrong people are often immune to the stopped clock rule because they are not exactly stopped clocks. More like clocks losing a random number
of seconds a day, in the wrong time zone of the wrong planet.
|
LMAO
[Edited on 25-11-2018 by Tsjerk]
|
|
AJKOER
Radically Dubious
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3026
Registered: 7-5-2011
Member Is Offline
Mood: No Mood
|
|
Your comments are technically accurate, however, I have used and learned to use flame heated aluminum by experimenting. Note, Al foil can also have a
plastic (acrylic) coating at times (discussed in an old thread on SM here http://www.sciencemadness.org/talk/viewthread.php?tid=72608#... ), so flame treating also removes any other protective coating.
The purpose for heat treating the Al foil becomes especially obvious with the so called Bleach Battery. Mix aqueous NaOCl with a weak acid (like
vinegar) forming HOCl. Pour it into two vessels, each with copper pennies and one with Al foil that is heat treated and the other that is not
treated.
It becomes quickly apparent that there is the significant different in chlorine formation, so perform this experiment in a well ventilated setting.
Note, one half cell reaction involves Al, the other HOCl (which breaks down into Cl2). Believe me there is an obvious difference in the speed of the
reaction in the vessel with heat treated Al foil in releasing chlorine fumes.
Some comments from a prior thread:
Quote: Originally posted by AJKOER ![](images/xpblue/lastpost.gif) |
.......
Note, as I previously performed on SM, chlorine gas can be sourced from a 'bleach battery' without the use of a strong acid. Here is a detailed
rehash of the steps involved in the so called Bleach battery:
1. Whip up some Hypochlorous acid by mixing bleach (NaOCl) and vinegar (which contains Acetic acid HAc) in the volume ratio 1.4 parts of 5% vinegar to
one part of 8.25% extra strength chlorine bleach.
2. To the HOCl add a piece of copper metal which will function as the cathode and an Aluminum source (like foil, but heat to red on a stove to
increase reactivity) to act as the anode.
3. Lastly, add much NaCl to act as the electrolyte and to salt out the chlorine. I usually jump start the reaction in a microwave (1 minute should
work).
The underlying chemical reaction leading to hypochlorous acid is given by:
NaOCl + HAc --> HOCl + NaAC
-------------
An alternate preparation of HOCl creating more conc HOCl (which is also avoids organic acids subject to attack by the hypochlorous acid in the
presence of copper) is:
2 NaOCl + CaCl2 = 2 NaCl + Ca(OCl)2
Ca(OCl)2 + 2 NaHCO3 --> Na2CO3 + CaCO3 (s) + 2 HOCl (cool and let stand to remove the CaCO3)
Net: 2 NaOCl + CaCl2 + 2 NaHCO3 --> 2 NaCl + Na2CO3 + CaCO3 (s) + 2 HOCl
------------------------
My take on the major electrochemical half-reactions:
In anodic zone (aluminum pieces):
6 H2O <--> 3 H3O+ + 3 OH-
Al + 3OH- ⇒ Al(OH)3 + 3 e-
At the cathode (copper metal):
3 HOCl + 3 H3O+ + 3 e- ⇒ 3/2 Cl2(g) + 6 H2O
for an implied net reaction of:
3 HOCl (aq) + Al (s) --NaCl--> Al(OH)3 (s) + 3/2 Cl2 (g) Eo net = 3.93 V
Note, the moles of consumed HOCl (from NaOCl) to form one mole is not as efficient as employing, for example, NaHSO4 acting on NaOCl+NaCl, but no
strong acid or acid salt was used!
Incidentally, the battery cell is theoretically capable of generating 3.93 volts. References: see http://www.exo.net/~pauld/saltwater/ and http://sci-toys.com/scitoys/scitoys/echem/batteries/batterie... and also http://www.dtic.mil/dtic/tr/fulltext/u2/d019917.pdf
[Edited on 9-7-2018 by AJKOER] |
|
|
Tsjerk
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3026
Registered: 20-4-2005
Location: Netherlands
Member Is Offline
Mood: Mood
|
|
You are a caricature of yourself.
|
|
AJKOER
Radically Dubious
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3026
Registered: 7-5-2011
Member Is Offline
Mood: No Mood
|
|
I have since added the credentials of one of the authors, whose work was assumed to be mine (since I did not place quotes around my transcription of
his reactions depicted in a diagram) and now responsible for my ill fame, relating to mechanochemical treatment of aluminum metal at elevated
temperatures. He is John Petrovic, Ph.D, Materials Science, see https://www.linkedin.com/in/john-petrovic-49aa8241 .
------------------------------------------------------------------
Tsjerk, I wonder if you have the ability to do even the simple experiment I detailed (don't forget the 1 minute microwave jump start), which should
take no more than 10 minutes to get it all together. If so you would be still smelling the chlorine (from the chamber with the treated Al foil)!
-----------------------------------------
A bigger challenge, repeat my thread synthesis replacing the graphite with a lot of activated carbon (AC), so that its surface area is in excess of
the Aluminum, employing a microwave and don't forget the sea salt!
I would definitely expect even better results, based on this 2007 work (has anyone noticed how recent the science is I am citing?, link: https://www.researchgate.net/publication/239705822_Generatio...
My take:
AC = AC+ + e- (aq)
Then, as in the opening part of this thread:
Al/Carbon/CH3HCO2-/H2O2/Sea Salt System:
------------------------------------------------------------
2 x [ Al --> Al(lll) + 3 e- ]
6 x [ e- + nH2O --> e-(aq) ]
3 x [ H2O2 = H+ + HO2- ]
3 x [ H+ + e-(aq) = •H ]
3 x [ •H + HO2- = •OH + OH- ]
Memo: Net last 4 reactions:
e-(aq) + H2O2 = •OH + OH- (a one electron reduction of H2O2 likely accelerated by microwaving in the presence of AC)
3 x [ •OH + e-(aq)- = OH- ]
----------------------------------------------------
2 Al + 3 H2O2 + nH2O ---> 2 [Al(H2O)6](OH)3
Then, the action of dilute acetic acid acting on freshly created Aluminum hydroxide aqua complex, plus likely a needed ammonia/NH4+ boost via:
Al = Al(lll) + 3 e-
3 x [ NH4+ = NH3 + H+ ]
3 x [ e- + H+ = •H ]
3 x [ NH3 + •H (or •OH) = •NH2 + H2 (or H2O) ]
-------------------------------------------------------
Net: Al + 3 NH4+ = Al(lll) + 3 •NH2 + 3 H2 (g)
Not really that complex (at least, so far).
[Edited on 26-11-2018 by AJKOER]
|
|
woelen
Super Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 7987
Registered: 20-8-2005
Location: Netherlands
Member Is Offline
Mood: interested
|
|
I tried to understand the point of thios experiment, but I lost track of it almost immediately at the start of the first post ![:(](./images/smilies/sad.gif)
@AJKOER: In nearly all of your posts you complicate things so much that it becomes gibberish for most (all?) readers of this forum. Who can assess the
correctness of what you write? Who wants to wade through tons and tons of seemingly irrelevant equations and references, often presented in such a way
that there hardly is any visible structure in the "dumps".
If you want people to show any interest in your experiments or discussions, then you really have to change things! Most people simply ignore your
posts and unfortunately they have a good reason to do so. You are the one who can change that, only you!
|
|
AJKOER
Radically Dubious
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3026
Registered: 7-5-2011
Member Is Offline
Mood: No Mood
|
|
Thanks Woelen, I will separate out the highly technical references for those interested.
--------------------------------------------------------------------------------------------------
Back to my challenged claim that heated Al foil can produce a gamma alumina coating that has been described by an authority (John Petrovic, Ph.D,
Materials Science) as having a weakened surface structure, and further per the web:
"The diffraction patterns in the temperature range (550–850 °C) correspond to the γ-Al2O3 phase."
Also, per the web:
"Aluminum melts at around 600 C and steel around 1400 C. Molten steel is white hot and molten aluminum red hot. "
So, red hot Al is in the range of possible gamma alumina creation, which may induce a weakened gamma layer.
In my opinion, several prior experiments performed by me confirm this reactivity as well, and if anyone wants to continue to challenge the reactivity
claim, perhaps try to perform my suggested experiment relating to a Bleach Battery cell. However, one need only look at the pictures in this very
thread and my prior comment, to quote from caption on one of the thread pictures:
"Note, Aluminum consumed except for small piece that was not heat treated."
Apparently, I was not able to uniformly heat all the Al foil to redness leaving a small untreated piece that is still resistant.
However, if one still wishes to contest this point, it does not matter to the central fact that in this thread, using microwave (MV) assisted heating
(perhaps key per a reference claiming radical formation with MV application on activated carbon and other sources citing interaction between hydroxyl
radicals and graphite), I fairly rapidly dissolved heat treated Al foil (using a methane flame) with weak 5% vinegar, weak 3% H2O2, two small graphite
rods and sea salt followed by a late addition of dilute pure ammonia water, likely producing not Al(OH)3, but an aluminum acetate salt (to be
determined).
I added some alcohol to a sample of my final mix and eventually it should produce crystals. Unfortunately, as I increased NaCl dosing early on (to try
to dissolve the Al foil before I conceived of adding NH3), I expect lots of NaCl, but in future runs, this should not be an issue.
[Edited on 26-11-2018 by AJKOER]
|
|
Tsjerk
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3026
Registered: 20-4-2005
Location: Netherlands
Member Is Offline
Mood: Mood
|
|
Quote: Originally posted by AJKOER ![](images/xpblue/lastpost.gif) |
Tsjerk, I wonder if you have the ability to do even the simple experiment I detailed (don't forget the 1 minute microwave jump start), which should
take no more than 10 minutes to get it all together. If so you would be still smelling the chlorine (from the chamber with the treated Al foil)!
[Edited on 26-11-2018 by AJKOER] |
You are suggesting I should microwave a mixture of vinegar, concentrated bleach, salt, copper and burned aluminium foil and then smell it... Thank you
very much but I will pass on that one.
I do have some 99% NaOH draincleaner and aluminum foil in my kitchen, I will mix some burned and unburned alu-foil with some dissolved NaOH and report
what happens... As my whole point was that aluminium foil in a flame oxidizes to the oxide. It won't produce bubbles anymore as there is no aluminium
anymore. You have oxide in your experiments, not aluminium.
|
|
AJKOER
Radically Dubious
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3026
Registered: 7-5-2011
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by Tsjerk ![](images/xpblue/lastpost.gif) | ...
....
You are suggesting I should microwave a mixture of vinegar, concentrated bleach, salt, copper and burned aluminium foil and then smell it... Thank you
very much but I will pass on that one.
.....As my whole point was that aluminium foil in a flame oxidizes to the oxide. It won't produce bubbles anymore as there is no aluminium anymore.
You have oxide in your experiments, not aluminium.
|
On the Bleach Battery, you can use the microwave for say 40 seconds on both vessels at once. This reduces the inception period, and then see the
difference in Cl2 creation. The electrochemical cell does not generate chlorine from Al2O3, so by your argument (lots of Al2O3 created), there should
be no contest, and your untreated Al foil should prove to be superior!
My view is it that it not the quantity of Al presence after flame treatment, but the amount of exposed Al feeding the half cell reaction.
Now, per the first picture in this thread, it still looks pretty good. But even if it all Al2O3, should not the oxide be more easily subject to an
acid attack creating acetate? I don't agree, but what is the problem if it does dissolve faster, you should endorse the flame treatment process.
[Edited on 26-11-2018 by AJKOER]
|
|
Tsjerk
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3026
Registered: 20-4-2005
Location: Netherlands
Member Is Offline
Mood: Mood
|
|
Did you do this chlorine battery experiment you talk about with a proper negative?
I just put some "treated" aluminum in NaOH, with a proper negative, and found the burned aluminium to be about 95% reduced in hydrogen production.
|
|