Weird White film on measuring cylinder


Hi,
I was extracting limonene from oranges using a distillation and collecting the product in a clear plastic measuring cylinder after it had finished no layers were formed but when the water was poured off the measuring cylinder had a white coating on it. i can't get this off and have tried washing with water. the cylinder smells strongly of oranges so i think it is limonene. Any idea how to recover this???

[Edited on 3-10-2018 by Housane]
View user's profile View All Posts By User
Heptylene
Hazard to Others
***




Posts: 319
Registered: 22-10-2016
Member Is Offline

Mood: No Mood

[*] posted on 3-10-2018 at 12:05


Have you tried washing with a solvent like ethanol? If you want to keep what you remove from the cylinder you can the evaporate/boil off the solvent. If you just want to wash the cylinder, soap could work too.
View user's profile View All Posts By User
MrHomeScientist
International Hazard
*****




Posts: 1806
Registered: 24-10-2010
Location: Flerovium
Member Is Offline

Mood: No Mood

[*] posted on 3-10-2018 at 12:11


Perhaps something slightly dissolved the plastic in the cylinder? So the white film might actually be etched and "frosted" plastic (analogy to frosted glass).
View user's profile Visit user's homepage View All Posts By User
wg48
National Hazard
****




Posts: 821
Registered: 21-11-2015
Member Is Offline

Mood: No Mood

[*] posted on 3-10-2018 at 12:36


Lemonene dissolves polystyrene so if your plastic cylinder was polystyrene you may have irreversible damaged it and contaminated the limonene.




Borosilicate glass:
Good temperature resistance and good thermal shock resistance but finite.
For normal, standard service typically 200-230°C, for short-term (minutes) service max 400°C
Maximum thermal shock resistance is 160°C
View user's profile View All Posts By User
fusso
International Hazard
*****




Posts: 1922
Registered: 23-6-2017
Location: 4 ∥ universes ahead of you
Member Is Offline


[*] posted on 3-10-2018 at 12:40


Quote: Originally posted by wg48  
Lemonene dissolves polystyrene so if your plastic cylinder was polystyrene you may have irreversible damaged it and contaminated the limonene.
Can transferring the limonene to a glass RBF then re-steam-distill purify it?

[Edited on 03/10/18 by fusso]




View user's profile View All Posts By User
Housane
Hazard to Others
***




Posts: 127
Registered: 3-9-2018
Location: Worcester, England
Member Is Offline

Mood: Let’s make

[*] posted on 3-10-2018 at 21:46


Hi i will try washing it with soap. the cylinder is made of PP
View user's profile View All Posts By User
Herr Haber
International Hazard
*****




Posts: 1236
Registered: 29-1-2016
Member Is Offline

Mood: No Mood

[*] posted on 4-10-2018 at 03:19


Quote: Originally posted by Housane  
Hi i will try washing it with soap. the cylinder is made of PP


So is the blue gl45 cap I have on my limonene.
It is slightly being attacked even though liquid limonene never touches it.
View user's profile View All Posts By User
XeonTheMGPony
International Hazard
*****




Posts: 1641
Registered: 5-1-2016
Member Is Offline

Mood: No Mood

[*] posted on 4-10-2018 at 04:01


Welcome to the wonderful world of material compatibility charts, the first thing you look at befor even thinking about plastic!
View user's profile View All Posts By User
RogueRose
International Hazard
*****




Posts: 1597
Registered: 16-6-2014
Member Is Offline


[*] posted on 4-10-2018 at 05:15


I'm guessing the limonene oxidized or partially dissolved the plastic. IIRC when I looked at the substance it had warnings about some plastics.
View user's profile View All Posts By User
DavidJR
National Hazard
****




Posts: 908
Registered: 1-1-2018
Location: Scotland
Member Is Offline

Mood: Tired

[*] posted on 4-10-2018 at 07:36


Yeah limonene isn't great with plastics in general