Author: Subject: Chemical Resistance of Stoppers
Yttrium2
Perpetual Question Machine
*****




Posts: 1104
Registered: 7-2-2015
Member Is Offline


[*] posted on 18-3-2018 at 09:16
Chemical Resistance of Stoppers


Which bungs / Stoppers are best?

Which have the most chemical Resistance?

Or, which material stopper is used for what?
View user's profile Visit user's homepage View All Posts By User
DavidJR
National Hazard
****




Posts: 908
Registered: 1-1-2018
Location: Scotland
Member Is Offline

Mood: Tired

[*] posted on 18-3-2018 at 09:25


Ground glass stoppers are best.
View user's profile View All Posts By User
Morgan
International Hazard
*****




Posts: 1708
Registered: 28-12-2010
Member Is Offline

Mood: No Mood

[*] posted on 18-3-2018 at 10:00


Well I bought a bunch of rubber stoppers with no holes, one, and two holes and over time they started to sweat an oily substance and aside from that they are now hard. Maybe putting them in bags and keeping them in the garage in summer did it.
So for some things these silicone stoppers are better like higher temperatures but they aren't good for some chemicals. I don't like the way the black rubber stoppers smell, thus I kept them outside. And it's a hassle if you don't have the right size so I forced myself to buy a bunch of sizes once again. Here's some larger sizes of the silicone stoppers atop my freezer in the garage. These stoppers smell too though, but maybe over time the odor will fade.
https://www.ebay.com/itm/80pc-1-16-3-4-High-Temp-Silicone-Ru...

DSC_0002 (1).JPG - 220kB DSC_0003.JPG - 231kB

[Edited on 18-3-2018 by Morgan]
View user's profile View All Posts By User
Magpie
lab constructor
*****




Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline

Mood: Chemistry: the subtle science.

[*] posted on 18-3-2018 at 10:21


I usually buy EPDM. For best chemical and heat resistance I use Viton.



The single most important condition for a successful synthesis is good mixing - Nicodem
View user's profile View All Posts By User
Akhil jain
Hazard to Self
**




Posts: 83
Registered: 19-2-2018
Member Is Offline

Mood: No Mood

[*] posted on 18-3-2018 at 11:38


It is best to use rubber stoppers since holes can be dig in it ,they are air tight and cheap.
But if you are making nitric acid you can't use rubber stoppers since nitric acid attacks rubber. In this preparation whole apparatus is made of glass




Subscribe to my youtube channel named akhil the chemist. search it and you will get it this channel is unique .
https://www.youtube.com/channel/UC9GD00yhAoKajgjRWvqyH-w
View user's profile View All Posts By User
BromicAcid
International Hazard
*****




Posts: 3254
Registered: 13-7-2003
Location: Wisconsin
Member Is Offline

Mood: Rock n' Roll

[*] posted on 18-3-2018 at 11:46


Once upon a time, cork stoppers were about all that was available. Older literature however is able to use them for many applications by treating them with the appropriate compound (waterglass, shellac, bitumen, etc). On the plus side they are cheap.



Shamelessly plugging my attempts at writing fiction: http://www.robvincent.org
View user's profile Visit user's homepage View All Posts By User
metalresearcher
National Hazard
****




Posts: 759
Registered: 7-9-2010
Member Is Offline

Mood: Reactive

[*] posted on 18-3-2018 at 11:54


Quote: Originally posted by Akhil jain  
It is best to use rubber stoppers since holes can be dig in it ,they are air tight and cheap.
But if you are making nitric acid you can't use rubber stoppers since nitric acid attacks rubber. In this preparation whole apparatus is made of glass


However, this is a tedious job. Same with silicone stoppers. Simply using a cordless drill is not an option as the hole drilled jumps back as it is too elastic. Even when the drill bit is 2mm larger than the diameter of the tube to be used.




View user's profile View All Posts By User
Akhil jain
Hazard to Self
**




Posts: 83
Registered: 19-2-2018
Member Is Offline

Mood: No Mood

[*] posted on 18-3-2018 at 11:58


It is not a tedious job to make holes in rubber stoppers
If you have a cork borer it is very easy if you have a drill it's still easy. You can even drill two holes and pass two delivery tubes in it . Use rubber stoppers if you don't want your gases to leak out . It is easy to work with rubber stoppers than glass ones




Subscribe to my youtube channel named akhil the chemist. search it and you will get it this channel is unique .
https://www.youtube.com/channel/UC9GD00yhAoKajgjRWvqyH-w
View user's profile View All Posts By User
Magpie
lab constructor
*****




Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline

Mood: Chemistry: the subtle science.

[*] posted on 18-3-2018 at 12:00


I use one of those “cork borers” to bore holes in the rubber.



The single most important condition for a successful synthesis is good mixing - Nicodem
View user's profile View All Posts By User
Akhil jain
Hazard to Self
**




Posts: 83
Registered: 19-2-2018
Member Is Offline

Mood: No Mood

[*] posted on 18-3-2018 at 12:01


Quote: Originally posted by Morgan  
Well I bought a bunch of rubber stoppers with no holes, one, and two holes and over time they started to sweat an oily substance and aside from that they are now hard. Maybe putting them in bags and keeping them in the garage in summer did it.
So for some things these silicone stoppers are better like higher temperatures but they aren't good for some chemicals. I don't like the way the black rubber stoppers smell, thus I kept them outside. And it's a hassle if you don't have the right size so I forced myself to buy a bunch of sizes once again. Here's some larger sizes of the silicone stoppers atop my freezer in the gara



[Edited on 18-3-2018 by Morgan]

Can I use silicon stoppers for making nitric acid . Won't they be attacked by fuming HNO3




Subscribe to my youtube channel named akhil the chemist. search it and you will get it this channel is unique .
https://www.youtube.com/channel/UC9GD00yhAoKajgjRWvqyH-w
View user's profile View All Posts By User
Sulaiman
International Hazard
*****




Posts: 3738
Registered: 8-2-2015
Location: 3rd rock from the sun
Member Is Offline


[*] posted on 18-3-2018 at 12:19


For boring holes through corks and red rubber bungs, I have similar to these
https://www.ebay.co.uk/itm/Ajax-Scientific-6-Piece-Brass-Cor...
but I rarely use them.
There are matching sharpeners https://www.ebay.co.uk/itm/RVFM-Cork-Borer-Sharpener/1223699...




CAUTION : Hobby Chemist, not Professional or even Amateur
View user's profile View All Posts By User
Magpie
lab constructor
*****




Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline

Mood: Chemistry: the subtle science.

[*] posted on 18-3-2018 at 13:14


I use my borers all the time. Thanks Sulaiman for the link to the sharpeners, I just bought one off Amazon.



The single most important condition for a successful synthesis is good mixing - Nicodem
View user's profile View All Posts By User
symboom
International Hazard
*****




Posts: 1143
Registered: 11-11-2010
Location: Wrongplanet
Member Is Offline

Mood: Doing science while it is still legal since 2010

[*] posted on 18-3-2018 at 14:02


Could rubber stoppers be coated in teflon spray to proteck them from corrosive compounds suchbas rubber desolving solvents and strong acids



View user's profile View All Posts By User
phlogiston
International Hazard
*****




Posts: 1379
Registered: 26-4-2008
Location: Neon Thorium Erbium Lanthanum Neodymium Sulphur
Member Is Offline

Mood: pyrophoric

[*] posted on 18-3-2018 at 14:28


Quote: Originally posted by metalresearcher  

However, this is a tedious job. Same with silicone stoppers. Simply using a cordless drill is not an option as the hole drilled jumps back as it is too elastic. Even when the drill bit is 2mm larger than the diameter of the tube to be used.


Freeze the rubber prior to drilling.
Ben Krasnow (Applied Science) has a video on machining frozen rubber with a cnc router.




-----
"If a rocket goes up, who cares where it comes down, that's not my concern said Wernher von Braun" - Tom Lehrer
View user's profile View All Posts By User
Yttrium2
Perpetual Question Machine
*****




Posts: 1104
Registered: 7-2-2015
Member Is Offline


[*] posted on 18-3-2018 at 14:35


Quote: Originally posted by metalresearcher  
Quote: Originally posted by Akhil jain  
It is best to use rubber stoppers since holes can be dig in it ,they are air tight and cheap.
But if you are making nitric acid you can't use rubber stoppers since nitric acid attacks rubber. In this preparation whole apparatus is made of glass


However, this is a tedious job. Same with silicone stoppers. Simply using a cordless drill is not an option as the hole drilled jumps back as it is too elastic. Even when the drill bit is 2mm larger than the diameter of the tube to be used.



They have drill bits for rubber stopper
View user's profile Visit user's homepage View All Posts By User
Sulaiman
International Hazard
*****




Posts: 3738
Registered: 8-2-2015
Location: 3rd rock from the sun
Member Is Offline


[*] posted on 18-3-2018 at 15:46


Quote: Originally posted by Magpie  
I use my borers all the time.


So do you bear "the mark of the chemist" ?




CAUTION : Hobby Chemist, not Professional or even Amateur
View user's profile View All Posts By User
Magpie
lab constructor
*****




Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline

Mood: Chemistry: the subtle science.

[*] posted on 18-3-2018 at 15:53


No marks except on my wood bench. I now place a piece of sacrificial wood under the stopper when boring. I also wear leather gloves.



The single most important condition for a successful synthesis is good mixing - Nicodem
View user's profile View All Posts By User
Morgan
International Hazard
*****




Posts: 1708
Registered: 28-12-2010
Member Is Offline

Mood: No Mood

[*] posted on 18-3-2018 at 17:43


I saw this but just wonder how a brad point drill bit would work?

How to drill a hole into a rubber stopper
https://www.youtube.com/watch?v=S9Webmd9Jvw

https://www.toolstoday.com/g-22-the-brad-point-boring-bit
View user's profile View All Posts By User
LearnedAmateur
National Hazard
****




Posts: 513
Registered: 30-3-2017
Location: Somewhere in the UK
Member Is Offline

Mood: Free Radical

[*] posted on 19-3-2018 at 00:12


I use orange rubber stoppers mostly, got a couple of glass ones too which are obviously fine for the majority of applications, but rubber is attacked by a lot of solvents over time. I’ve noticed that when stoppering a flask containing ethanol, isopropanol, toluene etc. They tend to swell and ‘wet’ bits will flake off. I’ve ended up having these bits floating around in the mixture/solvent when they’re removed before.



In chemistry, sometimes the solution is the problem.

It’s been a while, but I’m not dead! Updated 7/1/2020. Shout out to Aga, we got along well.
View user's profile View All Posts By User
XeonTheMGPony
International Hazard
*****




Posts: 1641
Registered: 5-1-2016
Member Is Offline

Mood: No Mood

[*] posted on 19-3-2018 at 03:36


I've applied a gentle layer of silicon grease then wrapped in teflon tape the stoppers when I had to use them for harsh reactions and it seems to have don the job on most of them for most of the time, rubber is a crap material IMO hardens over time, can fuse to the glass in certain conditions, cheap rubbers smell bad.

They had their time, I prefer to use glass gas inlets and such failing that chemically treated cork wold be preferable to rubber!

I never used silicon befor but knowing the material I'd say it'd be better.

Then there is machined teflon stoppers one can get.