13enigma
Harmless
*




Posts: 48
Registered: 4-6-2017
Member Is Offline

Mood: No Mood

[*] posted on 23-11-2017 at 11:20
Is there an easy process to cut diamonds, perhaps a dremel tool or lasers


I was think of buying a dremel tool with Diamond blades but was told that it would not cut the rough diamonds I have. What techniques are there employed by chemists and gemologists
View user's profile View All Posts By User
aga
Forum Drunkard
*****




Posts: 7030
Registered: 25-3-2014
Member Is Offline


[*] posted on 23-11-2017 at 12:25


Diamonds are generally cut with Diamonds.

Cleaving is a highly skilled art, where the cutter whacks one diamond against the other along a known cleave-line, where they know the diamond being cut will probably split in this process.

Spinning the diamond against a fixed diamond can be used to shape them (both) into some round shape by abrasion.

Laser cutting also works.

All from Wiki : https://en.wikipedia.org/wiki/Diamond_cutting




View user's profile View All Posts By User
karlosĀ³
International Hazard
*****




Posts: 1520
Registered: 10-1-2011
Location: yes!
Member Is Offline

Mood: oxazolidinic 8)

[*] posted on 23-11-2017 at 14:16


Quote: Originally posted by aga  

Cleaving is a highly skilled art, where the cutter whacks one diamond against the other along a known cleave-line, where they know the diamond being cut will probably split in this process.

Somewhat reminiscable of the flint processing our ancestors did, no? :)
I bet one of those H. habilis would be very experienced in seeing and using the cleave lines of a diamond too.
View user's profile View All Posts By User
macckone
Dispenser of practical lab wisdom
*****




Posts: 2168
Registered: 1-3-2013
Location: Over a mile high
Member Is Offline

Mood: Electrical

[*] posted on 23-11-2017 at 16:03


cutting diamonds is done by cleavage with a hammer and specialized chisel
View user's profile View All Posts By User
Texium
Administrator
Thread Moved
23-11-2017 at 19:09
phlogiston
International Hazard
*****




Posts: 1379
Registered: 26-4-2008
Location: Neon Thorium Erbium Lanthanum Neodymium Sulphur
Member Is Offline

Mood: pyrophoric

[*] posted on 24-11-2017 at 03:17


Mercury can also be refined electrolytically.
Because it does not require heating it might perhaps be a less risky way of purifying Hg than distillation. It would involve soluble mercury salts, however.




-----
"If a rocket goes up, who cares where it comes down, that's not my concern said Wernher von Braun" - Tom Lehrer
View user's profile View All Posts By User
zed
International Hazard
*****




Posts: 2284
Registered: 6-9-2008
Location: Great State of Jefferson, City of Portland
Member Is Offline

Mood: Semi-repentant Sith Lord

[*] posted on 25-11-2017 at 17:21


Diamonds may be cut or faceted by other diamonds, along certain planes.

Other materials are actually harder than diamonds (or so I have been told). And, could thus do the job. Maybe.

Boron Nitride? I'll check. I checked. Greater compressive strength.

But, how does that translate into abrasive power?

https://phys.org/news/2009-02-scientists-material-harder-dia...

Also.....

When is a Diamond, harder than a Diamond?

https://www.sciencealert.com/scientists-have-made-a-rare-dia...

[Edited on 26-11-2017 by zed]

[Edited on 26-11-2017 by zed]
View user's profile View All Posts By User