Growing pyrite (iron sulfide) crystals
Recently I obtained iron sulfide by react iron with sulfur.
I was wondering if it is possible to grow iron sulfide crystals via dissolving this sulfide in some acid or substance and then leaving it volatilise,
in a similar way to grow crystals in water.
|
|
DraconicAcid
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4299
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Offline
Mood: Semi-victorious.
|
|
Not very likely. If you dissolve it in some acid, the most likely thing to volatilize is H2S.
Additionally, pyrite is FeS2, not a simple sulphide. Which is too bad- it forms lovely crystals.
Please remember: "Filtrate" is not a verb.
Write up your lab reports the way your instructor wants them, not the way your ex-instructor wants them.
|
|
Harristotle
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 138
Registered: 30-10-2011
Location: Tinkerville
Member Is Offline
Mood: I tink therefore I am
|
|
I have no idea if this will work, so please accept this as wild speculation.
Suppose you took your iron sulfide, placed it in one of chironex's autoclaves, that he used for making quantum dots. ie, one of these http://www.ebay.com/itm/Hydrothermal-Autoclave-Reactor-Teflo...
Place some of your iron sulfide, and then some water and heat to a couple of hundred degrees in an oven. Slowly cool and see if you get any
crystalisation.
Open carefully, in a well ventilated area.
Keep your dog handy so you can blame him, if any of your friends walk by and sniff ! ![:)](./images/smilies/smile.gif)
I am thinking this is probably a bit like the geochemical processes, and you might be able to get some solubility at high temp.
your mileage may vary, and I have no real clue on this - only an experiment will tell!
Cheers,
H.
|
|
DraconicAcid
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4299
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Offline
Mood: Semi-victorious.
|
|
If we're going into wild speculation, a hydrothermal process with some ionic solvent (such as a hydrated metal salt such as calcium nitrate
tetrahydrate) might work better.
Please remember: "Filtrate" is not a verb.
Write up your lab reports the way your instructor wants them, not the way your ex-instructor wants them.
|
|
Sir M
Harmless
Posts: 5
Registered: 24-9-2017
Location: Central Europe
Member Is Offline
Mood: fuming
|
|
Couldn't the iron sulfide be dissolved in warm solution made by dissolving sulfur in NaOH to form soluble polysulfides?
Got the idea from dissolving of HgS, which works that way.
|
|
wg48
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 821
Registered: 21-11-2015
Member Is Offline
Mood: No Mood
|
|
Zinc sulphide crystals are grown from molten sodium chloride using a two zone quartz reactor with a temperature difference between the zones. In the
hotter zone is placed the source zinc sulphide, which dissolves and diffuses to the cooler zone where it crystallises.
Perhaps it would work with iron pyrites perhaps with a different salt. If I remember correctly it was in a patent. It would be a challenge building a
800C + reactor with two temperature controlled zones.
I found the patent https://www.google.com/patents/US3374067
It was KCl not NaCl.
[Edited on 9-10-2017 by wg48]
|
|
DraconicAcid
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 4299
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Offline
Mood: Semi-victorious.
|
|
Quote: Originally posted by wg48 ![](images/xpblue/lastpost.gif) | Zinc sulphide crystals are grown from molten sodium chloride using a two zone quartz reactor with a temperature difference between the zones. In the
hotter zone is placed the source zinc sulphide, which dissolves and diffuses to the cooler zone where it crystallises.
Perhaps it would work with iron pyrites perhaps with a different salt. If I remember correctly it was in a patent. It would be a challenge building a
800C + reactor with two temperature controlled zones.
I found the patent https://www.google.com/patents/US3374067
It was KCl not NaCl.
[Edited on 9-10-2017 by wg48] |
That's interesting to know. There are a number of different chloride salts and mixtures that one could try that would melt at a lower temperature,
which may or may not dissolve the sulphide at a given temperature. It might be possible to dissolve the pyrite at a high temperature, and slowly
decrease the temperature to one at which the pyrite isn't soluble, but the salt is still liquid.
ETA: http://www.sciencedirect.com/science/article/pii/S1876610215...
There's a eutectic mixture of the chlorides of potassium, sodium, calcium, and magnesium that melts at 385oC, and is very stable up to 500oC. If the
pyrite will dissolve appreciably at 500 oC, then crystallize as the temperature is reduced to, say 400 oC, then crystals may form. Then you let it
cool to room temperature and separate the crystals from the matrix with water.
[Edited on 9-10-2017 by DraconicAcid]
Please remember: "Filtrate" is not a verb.
Write up your lab reports the way your instructor wants them, not the way your ex-instructor wants them.
|
|
Texium
|
Thread Moved 9-10-2017 at 13:39 |
wg48
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 821
Registered: 21-11-2015
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by DraconicAcid ![](images/xpblue/lastpost.gif) |
ETA: http://www.sciencedirect.com/science/article/pii/S1876610215...
There's a eutectic mixture of the chlorides of potassium, sodium, calcium, and magnesium that melts at 385oC, and is very stable up to 500oC. If the
pyrite will dissolve appreciably at 500 oC, then crystallize as the temperature is reduced to, say 400 oC, then crystals may form. Then you let it
cool to room temperature and separate the crystals from the matrix with water.
[Edited on 9-10-2017 by DraconicAcid] |
I thought about a eutectic too but I would expect they would have thought about that too.
Heat up to dissolve and then cool down to form the crystals is achievable with just a crucible so that is much simpler. I suspect that if the amount
dissolved is small you will only get small crystals where as the two zone diffusion method would just need more time. But the heat up and cool method
would be a good starting point to get the right mixture of salts and temperature. Apparently various crystals can be grown this way if a suitable
molten salt or combination is available.
There is also the possibility of using a deep eutectic ionic liquid apparently some dissolve metal oxides perhaps one dissolves sulphides
|
|
crystal grower
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 474
Registered: 3-1-2016
Location: Os Petrosum
Member Is Offline
Mood: Puzzled
|
|
If you go to the nearest iron mine and pick up any rock with little pyrite vein, it will be probably much prettier than what you would ever manage
artificially.
Not saying it's not worth it if you're interrested in the "science part". Just wanted to let you know it isn't the easiest thing really.