What are "synthetic iron oxides"


It is found in most hardware stores. It has many colors
Black(Fe3O4), Red(Fe2O3), yellow(?), Green(?),blue(?)
I'm not sure if yellow or green iron oxides is possible. I might test if the green oxide is Cr2O3 since it looks very similar. Although after messing around with the red oxide, it seems to be calcined.
View user's profile View All Posts By User
NedsHead
Hazard to Others
***




Posts: 409
Registered: 9-12-2014
Location: South Australia
Member Is Offline

Mood: No Mood

[*] posted on 14-9-2017 at 03:06


If you look up the safety data sheet (SDS, MSDS) it'll tell you what the product consists of
View user's profile View All Posts By User
Elemental Phosphorus
Hazard to Others
***




Posts: 184
Registered: 11-11-2016
Location: Is everything
Member Is Offline

Mood: No Mood

[*] posted on 14-9-2017 at 04:06


I have a 1 pound bag of yellow iron oxide. It is most certainly possible, but the name 'iron oxide' is somewhat misleading, since it is actually iron oxide-hydroxide. (FeOOH)
I believe with enough heating it forms red iron oxide.
View user's profile View All Posts By User
Foeskes
Hazard to Others
***




Posts: 156
Registered: 25-2-2017
Member Is Offline

Mood: No Mood

[*] posted on 14-9-2017 at 04:57


Honestly most stuff in my country doesn't have msds. Even H2SO4 drain cleaner doesn't mention sulfuric acid on the bottle, just don't mix with basic drain cleaner. I did get a bag of white synthetic iron oxide, which is calcium carbonate. No idea on the green and blue one.
View user's profile View All Posts By User
MrHomeScientist
International Hazard
*****




Posts: 1806
Registered: 24-10-2010
Location: Flerovium
Member Is Offline

Mood: No Mood

[*] posted on 14-9-2017 at 06:44


What is these synthetic oxides used for? I wonder why they would claim it to be iron oxide when clearly it isn't. Does that particular chemical have lots of uses where you are?
View user's profile Visit user's homepage View All Posts By User
Foeskes
Hazard to Others
***




Posts: 156
Registered: 25-2-2017
Member Is Offline

Mood: No Mood

[*] posted on 14-9-2017 at 06:56


It seems to be used for dyeing. It is in the paint section of most hardware stores.
View user's profile View All Posts By User
Bert
Super Administrator
*********




Posts: 2821
Registered: 12-3-2004
Member Is Offline

Mood: " I think we are all going to die. I think that love is an illusion. We are flawed, my darling".

[*] posted on 14-9-2017 at 09:31


Pigments. I am amazed at the report of a "white Iron oxide" being offered.

In pyrotechnics, red and black Iron oxides are used as catalysts in such things as whistle mix. There are "natural" Iron oxides offered (crushed iron ore? RUST?!), as well as synthetic. They can have radically different performances, even among substances which are supposedly all "red Iron oxide" or "black Iron oxide".

Look at Iron oxides sold as cosmetics ingredients, offered on Amason, eBay & etc.




Rapopart’s Rules for critical commentary:

1. Attempt to re-express your target’s position so clearly, vividly and fairly that your target says: “Thanks, I wish I’d thought of putting it that way.”
2. List any points of agreement (especially if they are not matters of general or widespread agreement).
3. Mention anything you have learned from your target.
4. Only then are you permitted to say so much as a word of rebuttal or criticism.

Anatol Rapoport was a Russian-born American mathematical psychologist (1911-2007).

View user's profile View All Posts By User
Foeskes
Hazard to Others
***




Posts: 156
Registered: 25-2-2017
Member Is Offline

Mood: No Mood

[*] posted on 22-9-2017 at 01:14


I'm still not really sure what the dark blue "oxide" is.
View user's profile View All Posts By User
Fulmen
International Hazard
*****




Posts: 1701
Registered: 24-9-2005
Member Is Offline

Mood: Bored

[*] posted on 22-9-2017 at 01:27


I'm guessing they are called "iron oxides" as they are the most commonly used pigments, especially for concrete&masonry work.



We're not banging rocks together here. We know how to put a man back together.
View user's profile View All Posts By User
wg48
National Hazard
****




Posts: 821
Registered: 21-11-2015
Member Is Offline

Mood: No Mood

[*] posted on 22-9-2017 at 04:47


I googled for sellers of iron oxide. The were some misleading intro pics but I found no blue iron oxide for sale.
View user's profile View All Posts By User
Foeskes
Hazard to Others
***




Posts: 156
Registered: 25-2-2017
Member Is Offline

Mood: No Mood

[*] posted on 22-9-2017 at 17:44


I might buy some later and post a image. Maybe it's Prussian blue? Since it's name is pretty misleading.
View user's profile View All Posts By User
clearly_not_atara
International Hazard
*****




Posts: 2723
Registered: 3-11-2013
Member Is Offline

Mood: Big

[*] posted on 22-9-2017 at 18:57


Fougerite? Technically an oxide-hydroxide-carbonate:

https://duckduckgo.com/?q=fougerite&t=lm&iax=1&i...

[Edited on 23-9-2017 by clearly_not_atara]

fougerite.png - 95kB