I was considering copper plating a cast iron skillet to see if it allows for easier maintenance of the skillet with washing and maybe not having to season it. Obviously I'd remove the seasoning (hot lye works I've been told) and possibly use the sand blaster with something like walnut shelll or something that won't pit it.

I've read that copper doesn't plate well to cast iron and that another metal is often used as a first coat before copper, some suggested zinc another nickel (zinc not good for cooking and IDK about nickel).

I've dipped a handle in a solution of copper dissolved in HCl (it was still acidic) for about 20-30 second, and it left a copper sheen though it looked more dull/redish. I didn't want to hurt the handle, so I just tested this.

I have CuSO4 I thought I'd try and can use electrolysis which would probably be the only way to do this and get a thickness needed for cookware.

Does anyone have any suggestions (about the process or the general idea of it) or possibly have tried this?
View user's profile View All Posts By User
j_sum1
Administrator
********




Posts: 6252
Registered: 4-10-2014
Location: Unmoved
Member Is Offline

Mood: Organised

[*] posted on 21-5-2017 at 18:50


Well, my suggestion is to leave it as is. A good cast iron pan is great. And once properly seasoned requires very little care.

As for adhesion of copper to cast iron, I am no expert here but there are some things to consider.
Firstly, cast iron has a bcc crystal structure while copper is fcc. That generally does not make for good adhesion. Admittedly this is more of an issue for welding than plating but I suspect you are right -- an intermediate layer will likely be required.
Secondly, the presence of graphite in the cast iron cannot help adhesion.
Thirdly, I would avoid nickel in cookware that was going to be heated in an often acidic environment. I don't much like ingesting nickel salts.

there are plating recipes out there that have been discovered through trial and error. If you cannot find one then that suggests either that it does not work or that it is not a good idea. Probably both.


That said, if this is all about some scientific experimentation, by all means give it a shot. Post photos and results. :)
View user's profile View All Posts By User
Twospoons
International Hazard
*****




Posts: 1306
Registered: 26-7-2004
Location: Middle Earth
Member Is Offline

Mood: A trace of hope...

[*] posted on 21-5-2017 at 20:44


Quote: Originally posted by j_sum1  
Well, my suggestion is to leave it as is. ...

Thirdly, I would avoid nickel in cookware that was going to be heated in an often acidic environment. I don't much like ingesting nickel salts...


Seconded.
I wouldn't be too keen on ingesting copper salts either.
Iron, on the other hand, would actually be beneficial.

The other issue is copper is quite soft, so you'd likely end up scrubbing it off pretty quickly.




Helicopter: "helico" -> spiral, "pter" -> with wings
View user's profile View All Posts By User
Sulaiman
International Hazard
*****




Posts: 3625
Registered: 8-2-2015
Location: 3rd rock from the sun
Member Is Offline


[*] posted on 22-5-2017 at 02:42


Thirded,

copper and iron would be prone to electrolytic corrosion




CAUTION : Hobby Chemist, not Professional or even Amateur
View user's profile View All Posts By User
XeonTheMGPony
International Hazard
*****




Posts: 1638
Registered: 5-1-2016
Member Is Offline

Mood: No Mood

[*] posted on 25-5-2017 at 08:57


could do blast welding, but that is a tricky one to do once the pan all ready been formed
View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 25-5-2017 at 10:28


Fourthed
(Is that a word?)
View user's profile View All Posts By User
CharlieA
National Hazard
****




Posts: 646
Registered: 11-8-2015
Location: Missouri, USA
Member Is Offline

Mood: No Mood

[*] posted on 25-5-2017 at 11:47


Fifth'd, as in I second the motion; but it could also refer to a legal plea or maybe a beverage.
View user's profile View All Posts By User
clearly_not_atara
International Hazard
*****




Posts: 2722
Registered: 3-11-2013
Member Is Offline

Mood: Big

[*] posted on 25-5-2017 at 14:12


Quote: Originally posted by Sulaiman  
Thirded,

copper and iron would be prone to electrolytic corrosion

This is what really kills the idea. Anodic corrosion would probably destroy the pan as soon as even a microscopic hole formed in the copper.

I had a similar idea, finding a metal which could be used as a non-stick pan surface, but there isn't much. Ruthenium is non-corrodable, hard and cheap, because it is a byproduct of mining Pt and Pd, but it's rare, so it wouldn't stay cheap if you made pans out of it. It will also corrode iron AFAIK.

However, there is one pan coating material made from a nonmetal that would be nonstick and which does not corrode iron: CVD diamond. Let me know if you find a way to coat pans with that.
View user's profile View All Posts By User
brubei
Hazard to Others
***




Posts: 188
Registered: 8-3-2015
Location: France
Member Is Offline

Mood: No Mood

[*] posted on 25-5-2017 at 14:36


iron plating usely need to precoat your surface with Nickel (a mixture of NiH2SO4/NiCl/H3BO3 called Wood Nickel by plating industries) before adding any other metals to give a stable product against mecanical stress and frictions. I don't know if this has to be done on iron cast too, so don't skip your bibliogaphy.

[Edited on 25-5-2017 by brubei]