palladiumdreams
Harmless
Posts: 5
Registered: 25-11-2016
Member Is Offline
Mood: No Mood
|
|
stannous chloride
I am trying make a 2M solution of stannous chloride and am getting left with a purple solution once all the tin is dissolved. I am positive that I am
using 99% pure tin and 31% hardware grade HCL. I have not polluted the mixture with any precious metals. Any clue to what I may or may not be doing
wrong?
|
|
Meltonium
Hazard to Self
![*](images/xpblue/star.gif)
Posts: 97
Registered: 23-9-2016
Location: Home in pajamas
Member Is Offline
Mood: Fluorinated
|
|
The only thing I can think of would be a contaminant on your glassware. A stray permanganate crystal maybe? Or also, Tin chloride solutions oxidize in
air to form another tin complex, so that might be happening.
|
|
palladiumdreams
Harmless
Posts: 5
Registered: 25-11-2016
Member Is Offline
Mood: No Mood
|
|
Glassware was clean with no traces of precious metals or permanganates present. I checked the tin and it is rated as 99.9% pure. I'm at a loss as to
why and it takes quite a bit of time to wait for the tin to dissolve.
|
|
byko3y
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 721
Registered: 16-3-2015
Member Is Offline
Mood: dooM
|
|
It's hard to understand what "purple" means. Just like dillute permanganate solution? Or maybe more like this? https://upload.wikimedia.org/wikipedia/en/b/be/Tin%28II%29_h...
|
|
Xenoid
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 775
Registered: 14-6-2007
Location: Springs Junction, New Zealand
Member Is Offline
Mood: Comfortably Numb
|
|
Just a long shot...![:)](./images/smilies/smile.gif)
Are you sure you don't have 99.9% pure Titanium (Ti) and not pure Tin (Sn). It wouldn't be the first time someone mixed up the element symbols!
Titanium is grey and tough, Tin is bright and fairly soft.
Titanium dissolves slowly in HCl to give a distinct violet solution!
|
|
palladiumdreams
Harmless
Posts: 5
Registered: 25-11-2016
Member Is Offline
Mood: No Mood
|
|
The color is brilliant purple like permanganate.
Very sure it is not titanium, the Tin melted on low heat. Where I bought it from offered an assay cert for the Tin
When I had my solution on low heat I had the lid 98% covered with a watch glass.
I would like to know what I have made and whether or not the solution is salvageable for another project. I know I can recover the tin metal at some
point.
|
|
Sulaiman
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3630
Registered: 8-2-2015
Location: 3rd rock from the sun
Member Is Offline
|
|
I have 99.9% Sn and reagent grade HCl a few times with no pigmentation so no experience
but I'd start by boiling a sample of the HCl to dryness to get an idea of contaminants present.
CAUTION : Hobby Chemist, not Professional or even Amateur
|
|
AJKOER
Radically Dubious
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3026
Registered: 7-5-2011
Member Is Offline
Mood: No Mood
|
|
An idea is that you may have formed a small amount of "purple of Cassius", which is created by the action of SnCl2 on a gold salt.
In other words, something you employed was previously used in dissolving gold and left a trace amount. In practice, SnCl2 is used to test for the
presence of gold, and may have just found some.
For more background on SnCl2 see http://tin.atomistry.com/stannous_chloride.html , which is a compilation of historical extracts from chemistry journals over time.
[Edited on 29-11-2016 by AJKOER]
|
|
palladiumdreams
Harmless
Posts: 5
Registered: 25-11-2016
Member Is Offline
Mood: No Mood
|
|
I figured I had "purple of Cassius" but I did not think silver (nitrate) would cause that effect.. To my knowledge there just is not gold or PGM
present so I am still stumped.
Thanks for the link AJKOER
Is the tin chloride??? still useful for silvering mirrors as a reducing agent or should I just try and recycle the tin?
|
|
Boffis
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1848
Registered: 1-5-2011
Member Is Offline
Mood: No Mood
|
|
What colour is your hydrochloric acid? Colourless or yellow?
I used to think that the yellow colour in hardware store 30% HCl was due to iron but to my surprise tests revealed that the iron content of the acid
form our local hardware store is very low and the colour appears to be a dye. Who knows what colour it would turn if you try to reduce it.
Its easy now to buy high purity HCl so I no longer bother with hardware store grade material.
|
|
woelen
Super Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 7988
Registered: 20-8-2005
Location: Netherlands
Member Is Offline
Mood: interested
|
|
Add a little H2O2 to the purple solution. If it turns deep orange, then you have titanium in your solution, which in that case explains the purple
color.
|
|
palladiumdreams
Harmless
Posts: 5
Registered: 25-11-2016
Member Is Offline
Mood: No Mood
|
|
Thanks for suggestions people. Woelen's suggestion did the trick. I added a 3% solution of Hydrogen Peroxide and solution turned orange.
|
|
gipo
Harmless
Posts: 1
Registered: 19-7-2017
Member Is Offline
Mood: No Mood
|
|
In Australia, Bondall Hydrochloric Acid contains a small amount of titanium dioxide <1% (for some strange reason) which turns any stannous chloride
made with Bondall purple.
|
|
MrHomeScientist
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1806
Registered: 24-10-2010
Location: Flerovium
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by Boffis ![](images/xpblue/lastpost.gif) | I used to think that the yellow colour in hardware store 30% HCl was due to iron but to my surprise tests revealed that the iron content of the acid
form our local hardware store is very low and the colour appears to be a dye. Who knows what colour it would turn if you try to reduce it.
|
I'm not sure that's correct. Iron(III) chloride is very strongly colored in solution, especially in solutions with high concentrations of chloride
ions. See Periodic Videos' latest video on the World's Saltiest Water - a sample from that has a miniscule trace of iron, but it's still extremely strongly colored because of all the chloride.
|
|
Booze
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 121
Registered: 26-2-2017
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by MrHomeScientist ![](images/xpblue/lastpost.gif) | Quote: Originally posted by Boffis ![](images/xpblue/lastpost.gif) | I used to think that the yellow colour in hardware store 30% HCl was due to iron but to my surprise tests revealed that the iron content of the acid
form our local hardware store is very low and the colour appears to be a dye. Who knows what colour it would turn if you try to reduce it.
|
I'm not sure that's correct. Iron(III) chloride is very strongly colored in solution, especially in solutions with high concentrations of chloride
ions. See Periodic Videos' latest video on the World's Saltiest Water - a sample from that has a miniscule trace of iron, but it's still extremely strongly colored because of all the chloride.
|
If you can, use sunny side HCl. It is colorless and probably very little impurities.
|
|