Hello guys
here in my country i can get an npk 15 15 15 fertilizer for about 1USD for 2.5lbs witch containes 42%ammonium nitrate ,phosphoric acid and a potassium
salt
i took 11pounds and disolved everything in water and filtered then added some calcium hydroxide and left it for a few days to fully react ( a strong
ammonia odor is coming off of it )
and i plan on filtering again and adding about a gallong of 30% sulfuric acid and filter the calcium sulfate percipitate and distill it over to get
nitric acid
is it possible ?and is there any better ways to do it ?
thanks
|
|
aga
Forum Drunkard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 7030
Registered: 25-3-2014
Member Is Offline
|
|
Get the nirate out first, dry, then distill that with sulphuric acid.
Edit:
Welcome to ScienceManess !
[Edited on 14-11-2016 by aga]
|
|
Texium
|
Thread Moved 14-11-2016 at 13:28 |
Jstuyfzand
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 166
Registered: 16-1-2016
Location: Netherlands
Member Is Offline
Mood: Learning, Sorta.
|
|
What is this amazing country you speak of?
|
|
CHEMxpl
Harmless
Posts: 21
Registered: 14-11-2016
Member Is Offline
Mood: No Mood
|
|
I live in Algeria ;
okay so i've tried samples (100grams) and dissolved everything and recrystallized it but since the solubility of AN is very high even in cold water i
got some potassium nitrate cristals and some maybe phosphate impurities crash out as well
now i don't know if there's potassium chloride that reacts with the AN (hope not cuz that would prodce hcl and make aqua regia)
if i try to get the nitrates out alone i'll lose a lot, 50+%.
|
|
Tsjerk
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3026
Registered: 20-4-2005
Location: Netherlands
Member Is Offline
Mood: Mood
|
|
Why don't you add sulfuric acid to the solution you got after the first filtration (before adding calcium hydroxide) and distill this? You will have a
bit more salts in your pot, but nothing that is interfering with your distillation.
What concentration are you aiming for?
|
|
CHEMxpl
Harmless
Posts: 21
Registered: 14-11-2016
Member Is Offline
Mood: No Mood
|
|
I'm trying to get the azeotropic concentration of 68% even if i had to run multiple distilations
but that sounds a great idea
i guess i'll get anothger 11lbs and do that but what concernes me is the possiblity of the presence of chlorides
how do i know if there's any? and how am i gonna get rid of them?
and also does phosphoric acid reacts with calcium hydroxide?
|
|
Maroboduus
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 257
Registered: 14-9-2016
Location: 26 Ancho Street
Member Is Offline
Mood: vacant
|
|
Chlorides in nitric acid cause a precipitate with silver.
|
|
Tsjerk
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3026
Registered: 20-4-2005
Location: Netherlands
Member Is Offline
Mood: Mood
|
|
Phosphoric acid obviously reacts with hydroxides, but both phosphoric acid and its salts don't come over in this distillation.
Fertilizers are usually poor in chlorides as plants don't accumulate chloride too well, after repeated use the fertilizer would then make the soil
salty because chloride gets enriched.
@ Maroboduus, as does silver with phosphate and sulfate, especially in concentrated solutions. So not practical here.
[Edited on 16-11-2016 by Tsjerk]
|
|
CHEMxpl
Harmless
Posts: 21
Registered: 14-11-2016
Member Is Offline
Mood: No Mood
|
|
@Tsjerk
okay that's amazingly helpful thanks
also it says that it containes 7.5% nitric nitrogene and 7.5%ammoniacal nitrogene
according to my calculation there's 33% of no3- (42%ammonium nitrate),is it correct?
and i have 5kgs of it so 330x5=1650grams of no3-
let's just say i would loose 150grams of it so we're left with 1500g
can some one tell me how much 68%nitric acid can i get ?
|
|
Maroboduus
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 257
Registered: 14-9-2016
Location: 26 Ancho Street
Member Is Offline
Mood: vacant
|
|
Quote: Originally posted by Tsjerk ![](images/xpblue/lastpost.gif) | Phosphoric acid obviously reacts with hydroxides, but both phosphoric acid and its salts don't come over in this distillation.
Fertilizers are usually poor in chlorides as plants don't accumulate chloride too well, after repeated use the fertilizer would then make the soil
salty because chloride gets enriched.
@ Maroboduus, as does silver with phosphate and sulfate, especially in concentrated solutions. So not practical here.
[Edited on 16-11-2016 by Tsjerk] |
Maybe you could explain how sulphate and phosphate get into the distillate?
I said in nitric acid, not in a broth of mixed fertilizers.
This is an old method for testing nitric acid for chlorides.
|
|
Tsjerk
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3026
Registered: 20-4-2005
Location: Netherlands
Member Is Offline
Mood: Mood
|
|
CHEMxpl was talking about not wanting to form aqua regia, which would happen when sulfuric acid is added to the fertilizer solution (so before
distillation).
Ofcourse you could probably show this process after distillation as HCl together with a couple of other N/O/Cl species comes over, but that would be
to late in this case as you already distilled. Once aqua regia has formed there is no way to get rid of it anymore, Woelen has a nice post about it
somewhere.
68% nitric acid is 68% weight /weight, with a density of about 1,4 kg/liter. So 0.68 x 1.4 kg nitric acid will give you one liter 68% nitric acid.
[Edited on 16-11-2016 by Tsjerk]
|
|
CHEMxpl
Harmless
Posts: 21
Registered: 14-11-2016
Member Is Offline
Mood: No Mood
|
|
thank you guys you helped me a lot !
|
|
CHEMxpl
Harmless
Posts: 21
Registered: 14-11-2016
Member Is Offline
Mood: No Mood
|
|
update: adding the calcium hydroxdie actually helps a lot as i noticed i'm getting much purer and cleaner nitrate cristals
and it removed a alot of the phosphates
no all ihave to do is to add sulfuric acid and distil it
|
|
Tsjerk
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 3026
Registered: 20-4-2005
Location: Netherlands
Member Is Offline
Mood: Mood
|
|
I understand it helps with crystallisation of pure nitrate, but what I meant with adding sulfuric acid before calcium hydroxide was that you skipp the
whole crystallisation part and distill directly. Don't let aga foul you in thinking you need pure nitrate salt for this.
So the whole procedure would be: dissolve fertilizer, filter, add sulfuric acid, distil off nitric acid.
|
|
CHEMxpl
Harmless
Posts: 21
Registered: 14-11-2016
Member Is Offline
Mood: No Mood
|
|
yes of course that's what i'm doing
i just wanted to try it and see what it does
but next time i'll skip the calcium
anyway i'm very happy with this whole thnig
i can get nitric acid much much cheaper like this
[Edited on 19-11-2016 by CHEMxpl]
|
|