Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: Blue candles?
DistractionGrating
Hazard to Self
**




Posts: 68
Registered: 3-4-2014
Member Is Offline

Mood: Precipitated

[*] posted on 19-6-2016 at 21:27
Blue candles?


If I wanted to make some paraffin candles that burned a nice blue color, could I just mix copper sulfate with the paraffin? If so, what would be a reasonable concentration of copper sulfate to paraffin, w/w?
View user's profile View All Posts By User
Scalebar
Hazard to Self
**




Posts: 54
Registered: 6-5-2016
Location: Europe!
Member Is Offline

Mood: Looking for a way out

[*] posted on 19-6-2016 at 23:35


You'd probably want to concentrate on impregnating the wick with copper salts rather than the whole thing.
View user's profile Visit user's homepage View All Posts By User
TinSandwich
Harmless
*




Posts: 29
Registered: 24-2-2016
Member Is Offline

Mood: No Mood

[*] posted on 20-6-2016 at 00:01


That's a well timed question! Just last week me and some friends were desperately trying to make blue paraffin torches. Sadly all our attempts failed: we took rags, wet them in a molten paraffin/cuso4 mix and wrapped them around a stick, we even tried sprinkling copper sulfate in between the many layers of rags but the flame was still the regular yellow color after that.
It seems that the yellow/orange color of the paraffin flame "covers" the blue color of the copper sulfate flame.

You could try to get an alcohol burner (very similar to candles) and fuel it with a solution of methanol and cuso4 (sadly copper sulfate is insoluble in ethanol), you could also try using CuCl2: it's a bit harder to find but it's soluble in ethanol and acetone.
View user's profile View All Posts By User
deltaH
Dangerous source of unreferenced speculation
*****




Posts: 1663
Registered: 30-9-2013
Location: South Africa
Member Is Offline

Mood: Heavily protonated

[*] posted on 20-6-2016 at 00:32


You can use polyethylene glycol as the 'wax' to produce blue flames, which you can colour with organic salts of the metal whose colour you wish to impart.

See this patent for further details: http://www.google.com/patents/US3107511

The extra oxygen prevents the characteristic bright yellow colour of highly paraffinic flames, in the same way that alcohols burn with a blue-clear flame.




Mind your step or step your mind. Website: www.ideashack.org
View user's profile Visit user's homepage View All Posts By User
Marvin
National Hazard
****




Posts: 995
Registered: 13-10-2002
Member Is Offline

Mood: No Mood

[*] posted on 20-6-2016 at 01:12


Copper on it's own produces a green flame. CuCl is the usual emitting species in pyrotechnic blue and if the flame/mixture is too hot it breaks it apart and goes green. A solution of copper chloride in alcohol can produce a passable blue. Paraffin has particles of carbon producing the yellow light thermally (black body radiation) and this swamps atomic emitters.
View user's profile View All Posts By User
metalresearcher
National Hazard
****




Posts: 758
Registered: 7-9-2010
Member Is Offline

Mood: Reactive

[*] posted on 20-6-2016 at 03:16


When using CuSO4, you must use the white anhydrous version, not the blue CuSO4.5H2O crystals.
Just calcine the blue crystals by heating it to a few hundred degrees (but below red hot).

Water (vapor) + paraffin will induce the yellow flames.
View user's profile View All Posts By User
PHILOU Zrealone
International Hazard
*****




Posts: 2893
Registered: 20-5-2002
Location: Brussel
Member Is Offline

Mood: Bis-diazo-dinitro-hydroquinonic

[*] posted on 20-6-2016 at 04:10


I have also thought about it...the wick is also part of the problem it contains charcoal and often sodium both providing yellow color.

Glass fiber wick also contains sodium but it express less (I have used glass fiber fabric rolled at the end of a woden stock to make alcohol based troches (red, orange-pink, blue-green, green) for juggle. It is also less efficient to drive the liquid by capillarity than cotton wick does.

You need an alcohol gel containing traces of a halocarboxylate of copper (chloroacetate of Cu) and Cu(II) perchlorate.
You may also work with CuCl2(NH3)4 and Cu(NH3)4(OH)2 complexes...those goes more onto the electric blue side.

But beware of the toxicity for indoor...there is for sure a catalytic reaction happening leading to accrid, suffocating smel/fumes after a while.




PH Z (PHILOU Zrealone)

"Physic is all what never works; Chemistry is all what stinks and explodes!"-"Life that deadly disease, sexually transmitted."(W.Allen)
View user's profile View All Posts By User
unionised
International Hazard
*****




Posts: 5128
Registered: 1-11-2003
Location: UK
Member Is Offline

Mood: No Mood

[*] posted on 20-6-2016 at 10:39


Quote: Originally posted by metalresearcher  
When using CuSO4, you must use the white anhydrous version, not the blue CuSO4.5H2O crystals.
Just calcine the blue crystals by heating it to a few hundred degrees (but below red hot).

Water (vapor) + paraffin will induce the yellow flames.

There are two reasons why that's known to be wrong.
The obscure reason is that people who run flare stacks add steam to suppress smoke and soot- that would make the flame bluer and less smoky.
The more obvious reason is that the quantity of stem released from the tiny amount of water from hydrated copper sulphate on the wick is insignificant compared to that produced by the burning paraffin.
View user's profile View All Posts By User
Daffodile
Hazard to Others
***




Posts: 167
Registered: 7-3-2016
Location: Highways of Valhalla
Member Is Offline

Mood: Riding eternal

[*] posted on 20-6-2016 at 11:55


Somehow having Methanol burn, released from an inert and stable media would probably be your best bet. Not very bright though. Most Copper salts are annoying as they emit no colour at low temperatures, and green at high temperatures. Good luck.
View user's profile View All Posts By User
DraconicAcid
International Hazard
*****




Posts: 4355
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Offline

Mood: Semi-victorious.

[*] posted on 20-6-2016 at 12:06


Quote: Originally posted by Marvin  
Copper on it's own produces a green flame. CuCl is the usual emitting species in pyrotechnic blue and if the flame/mixture is too hot it breaks it apart and goes green. A solution of copper chloride in alcohol can produce a passable blue.


I thought it was green in the presence of halides, and blue otherwise.....




Please remember: "Filtrate" is not a verb.
Write up your lab reports the way your instructor wants them, not the way your ex-instructor wants them.
View user's profile View All Posts By User
UC235
National Hazard
****




Posts: 565
Registered: 28-12-2014
Member Is Offline

Mood: No Mood

[*] posted on 20-6-2016 at 12:20


Paraffin wax candles will not produce a blue flame. They burn yellow naturally because of black-body emission from soot particles produced in the fuel-rich flame. Since you cannot blow oxygen into the flame to make it burn more completely, you need to use substances that have a lower oxygen requirement for complete combustion. The small multicolor birthday candles sold commercially use trimethyl citrate as the fuel and burn clear blue without addition of metal salt colorants.

I've tried (many many years ago) loading copper soaps into paraffin wax up until the whole mass was tacky and unusable. It gave a slight green tint to the yellow flame and caked the burning wick with what was probably Cu2O.
View user's profile View All Posts By User
Daffodile
Hazard to Others
***




Posts: 167
Registered: 7-3-2016
Location: Highways of Valhalla
Member Is Offline

Mood: Riding eternal

[*] posted on 20-6-2016 at 12:27


Quote: Originally posted by UC235  
The small multicolor birthday candles sold commercially use trimethyl citrate as the fuel and burn clear blue without addition of metal salt colorants.



So someone could potentially melt a bunch of those candles, mix with some solvent to make a glob, and coat onto torches? I'm just throwing ideas out there so this probably wont work.

View user's profile View All Posts By User

  Go To Top