Sciencemadness Discussion Board
Not logged in [Login ]
Go To Bottom

Printable Version  
Author: Subject: Question on pottery-grade Cr2O3.
Velzee
Hazard to Others
***




Posts: 381
Registered: 19-8-2015
Location: New York
Member Is Offline

Mood: Taking it easy

[*] posted on 7-4-2016 at 14:06
Question on pottery-grade Cr2O3.


I recently purchased a pound of Cr2O3 from a pigment store, and after reading the SM wiki and deciding to make some chromium(III) sulfate, I came across this information from the chromium(III) sulfate page:


Quote:

Chromium(III) sulfate can be more directly produced by the action of cold, dilute sulfuric acid on chromium(III) hydroxide or chromium(III) oxide. It should be noted, however, that many grades of chromium(III) oxide are not reactive enough, often as a result of being calcined, to respond to treatment with acid.


And this from the Cr2O3 page:


Quote:

Chrome green is available at pottery shops as a green pigment, sometimes with traces of calcium carbonate. This material, however, may be too unreactive to produce other chromium compounds.


And, indeed, my Cr2O3 produced no noticeable reaction upon treatment with cold H2SO4.

So, my question is, how can I increase the reactivity(if possible) of the Cr2O3, or at least enough to react with H2SO4?




Check out the ScienceMadness Wiki: http://www.sciencemadness.org/smwiki/index.php/Main_Page

"All truth passes through three stages. First, it is ridiculed. Second, it is violently opposed. Third, it is accepted as being self-evident."
—Arthur Schopenhauer

"¡Vivá Cristo Rey!"
—Saint José Sánchez del Río
View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 7-4-2016 at 14:20


If your pottery Cr2O3 is anything like mine it won't even be affected by fusing with KOH!

I ended up fusing it with KNO3 which converts it (with very high yield) to K2Cr2O7.

[Edited on 7-4-2016 by blogfast25]




View user's profile View All Posts By User
DraconicAcid
International Hazard
*****




Posts: 4364
Registered: 1-2-2013
Location: The tiniest college campus ever....
Member Is Online

Mood: Semi-victorious.

[*] posted on 7-4-2016 at 14:29


I've seen a prep that called for reacting it with aluminum in a thermite reaction to get the more managable chromium metal.



Please remember: "Filtrate" is not a verb.
Write up your lab reports the way your instructor wants them, not the way your ex-instructor wants them.
View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 7-4-2016 at 16:07


Quote: Originally posted by DraconicAcid  
I've seen a prep that called for reacting it with aluminum in a thermite reaction to get the more managable chromium metal.


If you know how to run a decent aluminothermic reduction, then yes. If not, your metal yield may be quite small.




View user's profile View All Posts By User
j_sum1
Administrator
********




Posts: 6338
Registered: 4-10-2014
Location: At home
Member Is Offline

Mood: Most of the ducks are in a row

[*] posted on 7-4-2016 at 16:13


I have found product separation with CrO3 / Al thermite to be problematic. One great fused mass.
I think the best route to something useful is KNO3 to dichromate.




View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 7-4-2016 at 16:17


Quote: Originally posted by j_sum1  
I have found product separation with CrO3 / Al thermite to be problematic. One great fused mass.


I didn't. About 73 % yield, one nice roundish regulus of metal. It does require slight heat boosting (KNO3+Al, KClO3+Al or even K2Cr2O7+Al) and slag fluidiser (CaF2).




View user's profile View All Posts By User
S.C. Wack
bibliomaster
*****




Posts: 2419
Registered: 7-5-2004
Location: Cornworld, Central USA
Member Is Offline

Mood: Enhanced

[*] posted on 7-4-2016 at 18:13


Sulfuric acid will dissolve the oxide under certain conditions, such as when everything is mixed with "permanganic acid" for a second or two. Will dissolve a fair amount or none at all, because the reagents much less the conditions were not exactly nailed down. This particular permanganic acid was most reliably made from KMnO4, but MnO2 sometimes works...perhaps that depends on the exact nature of the "MnO2".



"You're going to be all right, kid...Everything's under control." Yossarian, to Snowden
View user's profile Visit user's homepage View All Posts By User
Mabus
Wiki Master
***




Posts: 238
Registered: 3-11-2013
Member Is Offline

Mood: Energetic

[*] posted on 8-4-2016 at 08:42


Uugh the pottery grade Cr2O3 I have it's very inert: No acid I used affected it, and when I tried to fuse it with KNO3 all I got was a brown-red insoluble mass, with some deep blue spots, which also seems to be pretty inert (no reaction with bleach or other acids). I have a feeling it's not just Cr2O3 in the pigment.



View user's profile View All Posts By User
Velzee
Hazard to Others
***




Posts: 381
Registered: 19-8-2015
Location: New York
Member Is Offline

Mood: Taking it easy

[*] posted on 8-4-2016 at 10:49


Quote: Originally posted by Mabus  
Uugh the pottery grade Cr2O3 I have it's very inert: No acid I used affected it, and when I tried to fuse it with KNO3 all I got was a brown-red insoluble mass, with some deep blue spots, which also seems to be pretty inert (no reaction with bleach or other acids). I have a feeling it's not just Cr2O3 in the pigment.


I got my Cr2O3 from US Pigments, if that makes any difference




Check out the ScienceMadness Wiki: http://www.sciencemadness.org/smwiki/index.php/Main_Page

"All truth passes through three stages. First, it is ridiculed. Second, it is violently opposed. Third, it is accepted as being self-evident."
—Arthur Schopenhauer

"¡Vivá Cristo Rey!"
—Saint José Sánchez del Río
View user's profile View All Posts By User
Velzee
Hazard to Others
***




Posts: 381
Registered: 19-8-2015
Location: New York
Member Is Offline

Mood: Taking it easy

[*] posted on 24-4-2016 at 10:01


Quote: Originally posted by blogfast25  
If your pottery Cr2O3 is anything like mine it won't even be affected by fusing with KOH!

I ended up fusing it with KNO3 which converts it (with very high yield) to K2Cr2O7.

[Edited on 7-4-2016 by blogfast25]



So, how exactly would I go about fusing them?




Check out the ScienceMadness Wiki: http://www.sciencemadness.org/smwiki/index.php/Main_Page

"All truth passes through three stages. First, it is ridiculed. Second, it is violently opposed. Third, it is accepted as being self-evident."
—Arthur Schopenhauer

"¡Vivá Cristo Rey!"
—Saint José Sánchez del Río
View user's profile View All Posts By User
macckone
Dispenser of practical lab wisdom
*****




Posts: 2168
Registered: 1-3-2013
Location: Over a mile high
Member Is Offline

Mood: Electrical

[*] posted on 24-4-2016 at 19:23


Grind the really fine, mix thoroughly and heat above the potassium nitrate decomposition point.
View user's profile View All Posts By User
Velzee
Hazard to Others
***




Posts: 381
Registered: 19-8-2015
Location: New York
Member Is Offline

Mood: Taking it easy

[*] posted on 15-7-2016 at 14:50


I wound up attempting to fuse ~15 grams of Cr2O3 with a little over 15 grams of NaOH in order to see if any reaction would occur. To my surprise, although all I could see was the green Cr2O3, after washing with water, I was left with a very small amount of a yellow solution, which presumably had a lot of NaOH in it.

I attempted another go, this time with an arbitrary amount of both reactants. Here's the result:

Tmizt07.jpg - 793kB

I may heat it up again, because I think I see some NaOH left over. What do you guys thing?



[Edited on 7/15/2016 by Velzee]

Tmizt07.jpg - 793kB




Check out the ScienceMadness Wiki: http://www.sciencemadness.org/smwiki/index.php/Main_Page

"All truth passes through three stages. First, it is ridiculed. Second, it is violently opposed. Third, it is accepted as being self-evident."
—Arthur Schopenhauer

"¡Vivá Cristo Rey!"
—Saint José Sánchez del Río
View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 15-7-2016 at 16:23


Quote: Originally posted by Velzee  
What do you guys thing?



With mine fused with KOH I got no reaction whatsoever. And I mean N-O-T-H-I-N-G.

But with 20 % stoichio excess of KNO3 the conversion to K2Cr2O7 is essentially 100 %.




View user's profile View All Posts By User
Bert
Super Administrator
*********




Posts: 2821
Registered: 12-3-2004
Member Is Offline

Mood: " I think we are all going to die. I think that love is an illusion. We are flawed, my darling".

[*] posted on 16-7-2016 at 12:27


Quote: Originally posted by blogfast25  
I didn't. About 73 % yield, one nice roundish regulus of metal. It does require slight heat boosting (KNO3+Al, KClO3+Al or even K2Cr2O7+Al) and slag fluidiser (CaF2).


Anyone tried the synthetic cryolite (Na3AlF6) used as a flux in Aluminum production, rather than Calcium fluoride as a flux/"slag fluidizer" for this or similar processes? I have cryolite on hand, it was used as a non hygroscopic yellow flame colorant in some pyrotechnic mixtures. No Calcium flouride, except a cute little crystaline mineral specimen I would not choose to sacrifice in an experiment.

MP of cryolite is around 1,000 C, BP not listed, said to decompose rather than vaporize. Decomposition temperature I have not yet found given anywhere-

Calcium flouride MP 1,408 C, BP 2,533 C.




Rapopart’s Rules for critical commentary:

1. Attempt to re-express your target’s position so clearly, vividly and fairly that your target says: “Thanks, I wish I’d thought of putting it that way.”
2. List any points of agreement (especially if they are not matters of general or widespread agreement).
3. Mention anything you have learned from your target.
4. Only then are you permitted to say so much as a word of rebuttal or criticism.

Anatol Rapoport was a Russian-born American mathematical psychologist (1911-2007).

View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 16-7-2016 at 13:25


Quote: Originally posted by Bert  

Anyone tried the synthetic cryolite (Na3AlF6) used as a flux in Aluminum production, rather than Calcium fluoride as a flux/"slag fluidizer" for this or similar processes? I have cryolite on hand, it was used as a non hygroscopic yellow flame colorant in some pyrotechnic mixtures. No Calcium flouride, except a cute little crystaline mineral specimen I would not choose to sacrifice in an experiment.

MP of cryolite is around 1,000 C, BP not listed, said to decompose rather than vaporize. Decomposition temperature I have not yet found given anywhere-

Calcium flouride MP 1,408 C, BP 2,533 C.


I've contemplated it because I have some too but I'm pretty sure it decomposes well below the minimum 2500 C needed for good slag/metal separation, acc.:

Na3AlF6 === > 3 NaF + AlF3

(The pyrolysis of (NH4)3AlF6 is a route to anhydrous AlF3, see e.g. Brauer)

BP NaF = 1700 C
BP AlF3 = not known but sublimes, almost certainly below 2500 C.

CaF2 really just hits the sweet spot, Bert.
<hr>
One should consider also CaO as a melt fluidiser, which forms a series of low melting a aluminates with alumina. A single test with MnO2 was very promising.


[Edited on 16-7-2016 by blogfast25]




View user's profile View All Posts By User
Velzee
Hazard to Others
***




Posts: 381
Registered: 19-8-2015
Location: New York
Member Is Offline

Mood: Taking it easy

[*] posted on 24-8-2016 at 07:32


These crystals formed from the solution after a few weeks. They're probably heavily contaminated with NaCl.

image.jpeg - 1.2MB




Check out the ScienceMadness Wiki: http://www.sciencemadness.org/smwiki/index.php/Main_Page

"All truth passes through three stages. First, it is ridiculed. Second, it is violently opposed. Third, it is accepted as being self-evident."
—Arthur Schopenhauer

"¡Vivá Cristo Rey!"
—Saint José Sánchez del Río
View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 24-8-2016 at 15:42


Quote: Originally posted by Velzee  
These crystals formed from the solution after a few weeks. They're probably heavily contaminated with NaCl.


Which experiment does this now refer to, Velzee? :)