How much does light penetrate through a solid material in microns.
How much does light penetrate through a solid material in microns.
There more than a million atoms in the width of a human hair, so with...light shining on the hair how many single atoms in a line, would the light
traverse through, or maybe the better word to use is scatter through.
The light is getting absorbed by the electron, and emission-ed, but some light is getting through the solid material, but by how much.
Thank you for your help, anything helps even a few words.
|
|
Etaoin Shrdlu
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 724
Registered: 25-12-2013
Location: Wisconsin
Member Is Offline
Mood: Insufferable
|
|
Define "light."
What solid material? Lead? Glass?
|
|
careysub
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1339
Registered: 4-8-2014
Location: Coastal Sage Scrub Biome
Member Is Offline
Mood: Lowest quantum state
|
|
About half of visible light is absorbed passing through 5 nm layer of aluminum.
|
|
Texium
|
Thread Moved 25-3-2016 at 19:47 |
unionised
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 5109
Registered: 1-11-2003
Location: UK
Member Is Offline
Mood: No Mood
|
|
If your material is an optical fibre, and the light is near 1550nm (Infra red- but the idea is still pretty much the same as visible light) then about
half the light will penetrate roughly 15 kilometres.
That's 15,000,000,000 microns.
|
|