Volitox Ignis
Hazard to Self

Posts: 53
Registered: 28-1-2016
Member Is Offline
Mood: No Mood
|
|
Questionable Synth:Sodium Metasilicate
I have been looking around on the Internet for any information on how to make white phosphorus (I've never seen it burn firsthand,only on video),and
stumbled across this video:
https://www.youtube.com/watch?v=mibM4WUx74Q and parts two and three. Firstly,I think that the amounts of each chemical were not stoichiometric,but
that is not my main concern.
I believe that the reaction occurring during the process to be:
24 Al + 2(NaPO3)6 --> 12 Al2O3 + 3 P4 + 12 Na
Since sodium reacts with water to produce sodium hydroxide,which can react with the phosphorus to produce toxic phosphine gas,this method is very
dangerous. I then thought that the sand added to the salt/sodium hexametaphosphate/aluminum reacts with the sodium and hexametaphosphate to produce
sodium metasilicate,thus preventing the production of phosphine. Are my assumptions correct? If so,what is the equation for the reaction that produces
sodium metasilicate?
Yes,I read the replies to my propellants thread,thanks for the help!
[Edited on 31-1-2016 by Volitox Ignis]
|
|
blogfast25
International Hazard
   
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
You'll find the answers in the sticky phosphorus thread.
|
|
BromicAcid
International Hazard
   
Posts: 3272
Registered: 13-7-2003
Location: Wisconsin
Member Is Offline
Mood: Rock n' Roll
|
|
Start by reading my primer:
https://www.sciencemadness.org/whisper/viewthread.php?tid=20...
Spoiler Alert - See Sodium Aluminate
[Edited on 1/31/2016 by BromicAcid]
|
|
Volitox Ignis
Hazard to Self

Posts: 53
Registered: 28-1-2016
Member Is Offline
Mood: No Mood
|
|
After reading around on the Phosphorus thread and some reworking, the equation came out as:
2 (NaPO3)6+ 20 Al + 6 SiO2 --> 6 Na2SiO3 + 10 Al2O3 + 3 P4
-From BromicAcid's PDF
Assuming no losses,this should result in a 30% yield of phosphorus based on sodium hexametaphosphate, am I right?
[Edited on 31-1-2016 by Volitox Ignis]
[Edited on 1-2-2016 by Volitox Ignis]
|
|
blogfast25
International Hazard
   
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by Volitox Ignis  | After reading around on the Phosphorus thread and some reworking, the equation came out as:
2 (NaPO3)6+ 20 Al + 6 SiO2 --> 6 Na2SiO3 + 10 Al2O3 + 3 P4
-From BromicAcid's PDF
Assuming no losses,this should result in a 39% yield based on sodium hexametaphosphate, am I right?
|
Yield of what?
|
|
Volitox Ignis
Hazard to Self

Posts: 53
Registered: 28-1-2016
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by blogfast25  | Quote: Originally posted by Volitox Ignis  | After reading around on the Phosphorus thread and some reworking, the equation came out as:
2 (NaPO3)6+ 20 Al + 6 SiO2 --> 6 Na2SiO3 + 10 Al2O3 + 3 P4
-From BromicAcid's PDF
Assuming no losses,this should result in a 39% yield based on sodium hexametaphosphate, am I right?
|
Yield of what? |
Ah,sorry for not writing it: 30% yield of phosphorus. I fixed my post now.
[Edited on 31-1-2016 by Volitox Ignis]
[Edited on 1-2-2016 by Volitox Ignis]
|
|
BromicAcid
International Hazard
   
Posts: 3272
Registered: 13-7-2003
Location: Wisconsin
Member Is Offline
Mood: Rock n' Roll
|
|
Reaction scheme is balanced, check.
The reaction of 2 mols of sodium hexametaphosphate (1223.54 g) should yield 3 mol of P4 (the exact allotrope does not matter, as distilling you will
get P2 as well, molecular weight either way is 371.64 g).
371.64 g phosphorus / 1223.54 g sodium hexametaphosphate x 100 = 30.37%
Is that what you are going for? Essentially if all your phosphorus is available you're hexametaphosphate is 30.37% phosphorus by weight which would
be the maximum theoretical yield (in practice it is about half of that IIRC). Versus your reaction mixture, your reaction mixture should give a
18.54% mass yield of phosphorus.
|
|
blogfast25
International Hazard
   
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
Sodium hexametaphosphate contains 30.4 w% of P. Is that what you mean?
To calculate an actual reaction yield you would need to know how much P was obtained from how much sodium hexametaphosphate.
[Edited on 1-2-2016 by blogfast25]
|
|