methyl methacrylate
I have got about 1 l of methyl methacrylate and is there any interesing use of it or I should get rid of it?
sorry for my English it is pretty bad
|
|
Nicodem
|
Thread Moved 16-11-2015 at 10:33 |
zed
International Hazard
   
Posts: 2285
Registered: 6-9-2008
Location: Great State of Jefferson, City of Portland
Member Is Offline
Mood: Semi-repentant Sith Lord
|
|
Methyl Methacrylate is an interesting reagent. I don't need it, but somebody might.
I had a Kilo or so, a while back. When I moved, I think I accidentally left if in my basement.
Might be sitting there still, but after all these years, it has probably slowly polymerized, to become a liter bottle full of solid plexiglass (AKA
lucite).
[Edited on 18-11-2015 by zed]
[Edited on 18-11-2015 by zed]
|
|
CuReUS
National Hazard
  
Posts: 928
Registered: 9-9-2014
Member Is Offline
Mood: No Mood
|
|
Is there a Kharasch reaction type modification for a freidel craft alkylation (i.e. the primary carbocation formed from the double bond of methyl
methacrylate attacks the aromatic ring instead of it rearranging to secondary carbocation and then attacking ? )
|
|
zed
International Hazard
   
Posts: 2285
Registered: 6-9-2008
Location: Great State of Jefferson, City of Portland
Member Is Offline
Mood: Semi-repentant Sith Lord
|
|
Ummm. Alkylations of the Indole 3 position, via refluxing Indole with Acetic Anhydride, and materials structurally similar to Methyl-Methacrylate,
are known. This is a special case. The 3 site is unusually reactive.
Likewise, Alkylations via the coupling of Methyl Methacrylate with diazonium salts may be achieved.
Direct Alkylation of an aromatic ring, via Methyl-Methacrylate? I dunno.
Are you suggesting halogenation of Methyl-Methacrylate, followed by the resulting Alkyl Halide, attacking an aromatic ring?
[Edited on 25-11-2015 by zed]
|
|
innervision
Harmless
Posts: 49
Registered: 6-2-2006
Member Is Offline
Mood: eh.
|
|
Make custom fit prosthetic teeth/fangs for Halloween. That's what I did with mine after distilling plexiglass.
It also makes for a very sturdy finish for wood if you polymerize it directly on the wood, then sand and polish.
|
|
zed
International Hazard
   
Posts: 2285
Registered: 6-9-2008
Location: Great State of Jefferson, City of Portland
Member Is Offline
Mood: Semi-repentant Sith Lord
|
|
How did you polymerize the material. Also, how serious a lachrymator is this stuff?
One equals terrible.........10 equals eye transplant. I've owned it before. I just never opened the bottle.
|
|
CuReUS
National Hazard
  
Posts: 928
Registered: 9-9-2014
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by zed  |
Direct Alkylation of an aromatic ring, via Methyl-Methacrylate? I dunno.
Are you suggesting halogenation of Methyl-Methacrylate, followed by the resulting Alkyl Halide, attacking an aromatic ring?
|
Not quite.
Alkenes can be reacted with aromatic rings in a friedel craft reactions using polyphosphoric acid.
|
|
innervision
Harmless
Posts: 49
Registered: 6-2-2006
Member Is Offline
Mood: eh.
|
|
Since I distilled Plexiglas for it, it is obviously a "heat cure" monomer as opposed to the easily cured "cold cure" that's available from dental
suppliers.
What I did was stirred monomer with some finely powdered acrylic polymer until starting to get thick then poured it into my bottom mold, pressed the
top mold in place, weighted the top and gave it a half hour to set. I then finished the polymerization submerged in sub-boiling water in a crock pot.
Ideally it is cured under water in a pressure pot. That forces any bubbles that formed from the mixing of monomer and polymer to disappear. I don't
have a pressure pot and couldn't justify buying one. It took a couple tries to get one without a bubble hole at the tip of a front fang or two.
Interestingly, the bottle with loose-fitting lid that I stored the (inhibitorless) monomer in, stayed liquid for a couple months before it finally
polymerized.
As for the smell... it's not a lachrymator, but I'm not sure I've smelled (been nasally abused by) anything so strong. You will want a respirator.
|
|