Author: Subject: Pressing powders into a pellet: how it works
Metallus
Hazard to Others
***




Posts: 116
Registered: 16-5-2013
Member Is Offline

Mood: No Mood

[*] posted on 10-11-2015 at 08:42
Pressing powders into a pellet: how it works


Hi there

This is more of a doubt I have concerning "how" the particles stick together in the pellet/platelet you make when you press a powdered solid.

From what I understood, when you grind a solid (eg: KBr, Al2O3, ZrB2) into a fine powder of an average particle size of 1-5 μm, and then you press said powder into a small platelet, what happens is that you stack all those small particles in a small volume, while still keeping their microscopic size (so the particles don't actually fuse together to give e.g 500μm particle size, but just stick together because reasons)

What is the force that keeps the pellet/platelet together? Is it just weak interactions? Because afterall the pellet is still very fragile and can be more or less easily broken and pulverized.

Also, in the case of KBr, you can actually make a perfectly transparent platelet starting from a white powder. A professor of mine told me that you actually melt the material together when pressing, but that explanation seemed a bit "odd" to me. Did he mean "you locally melt the particles because with an high surface area the melting point is lower"? Still, I never noticed a change in temperature whatsoever, so when he told me this I was a bit like "is he BSing me?".

I also know that in order to actually "fuse" the particles together, there is a process called sintering (like HP) during which you heat at high temperatures (even >2k°C) and press the material together, so I'm somewhat sure you don't actually fuse the particles together when you press them for 5min at RT, but more like "stack them together for a while".

I hope you can solve this little doubt of mine. If I got it right, it's just a difference between microscopic and macroscopic changes.

Thanks for your attention

View user's profile View All Posts By User
aga
Forum Drunkard
*****




Posts: 7030
Registered: 25-3-2014
Member Is Offline


[*] posted on 10-11-2015 at 09:10


Dunno about powders, but squashing stuff at high mechanically-induced pressures certainly causes localised heating.

The Krone system for telephone wires is basically ramming a copper wire between two blades.

The heating at the blade edge causes a 'microweld' between the copper wire and the blades.




View user's profile View All Posts By User
Bert
Super Administrator
Thread Moved
10-11-2015 at 09:18
Detonationology
Hazard to Others
***




Posts: 362
Registered: 5-5-2015
Location: Deep South
Member Is Offline

Mood: Electrophillic

[*] posted on 10-11-2015 at 09:21


Quote: Originally posted by aga  
Dunno about powders, but squashing stuff at high mechanically-induced pressures certainly causes localised heating.

I too don't have any practical experience with metal powders, but this reminds me of explosion welding (without the explosion). I assume that when powdered, particles can make better contact, but high temperature and pressure seems to be necessary across the board.




“There are no differences but differences of degree between different degrees of difference and no difference.” ― William James
View user's profile View All Posts By User
Bert
Super Administrator
*********




Posts: 2821
Registered: 12-3-2004
Member Is Offline

Mood: " I think we are all going to die. I think that love is an illusion. We are flawed, my darling".

[*] posted on 10-11-2015 at 09:35



Quote:

(so the particles don't actually fuse together to give e.g 500μm particle size, but just stick together because reasons)


Um, what? "because reasons"?!

Lots of different physical and chemical mechanisms may be in play, depending on the materials being pressed and conditions.

Got a specific question?




Rapopart’s Rules for critical commentary:

1. Attempt to re-express your target’s position so clearly, vividly and fairly that your target says: “Thanks, I wish I’d thought of putting it that way.”
2. List any points of agreement (especially if they are not matters of general or widespread agreement).
3. Mention anything you have learned from your target.
4. Only then are you permitted to say so much as a word of rebuttal or criticism.

Anatol Rapoport was a Russian-born American mathematical psychologist (1911-2007).

View user's profile View All Posts By User
annaandherdad
Hazard to Others
***




Posts: 387
Registered: 17-9-2011
Member Is Offline

Mood: No Mood

[*] posted on 10-11-2015 at 10:38


If two perfectly clean surfaces are pressed together, I find myself wondering why they would *not* weld.

One reason would be that neither surface is a perfect plane, or even if they are (because they are crystals cleaved along a plane of the lattice), the two planes cannot be made adjacent because of bumps elsewhere on the surface, or even if they can be made adjacent, the crystal lattices would not be aligned. But pressure would overcome misalignment, and the pressure is magnified at small points of contact. And a misalignment of crystals is no worse than what happens at domain boundaries.

I'm just speculating, I have no official knowledge. Of course, it could be that the surfaces are not perfectly clean.





Any other SF Bay chemists?
View user's profile View All Posts By User
phlogiston
International Hazard
*****




Posts: 1377
Registered: 26-4-2008
Location: Neon Thorium Erbium Lanthanum Neodymium Sulphur
Member Is Offline

Mood: pyrophoric

[*] posted on 10-11-2015 at 12:19


I suspect van der Waals forces are a big part of the answer.

Lots of substances undergo phase transitions when pressure changes. Possibly, KBr melts, but not because heat is generated when you apply pressure, but rather because at the high pressure and room temperature, KBr is a liquid. (However, googling for a few minutes I can't find a reliable references quickly that supports that KBr actually melts. Some sites say that it becomes plastic) so whether that is really true in the case of KBr I am not sure (but it is certainly possible for other solid substances).

Similarly, you can boil water at room temperature if you lower the pressure. You can melt ice at well below 0 deg C if you apply pressure. You can compress gasses to store them as liquids at room temperature. Look up pressure-temperature phase diagrams to find out more.




-----
"If a rocket goes up, who cares where it comes down, that's not my concern said Wernher von Braun" - Tom Lehrer
View user's profile View All Posts By User
careysub
International Hazard
*****




Posts: 1339
Registered: 4-8-2014
Location: Coastal Sage Scrub Biome
Member Is Offline

Mood: Lowest quantum state

[*] posted on 10-11-2015 at 15:12


Quote: Originally posted by phlogiston  
...
Lots of substances undergo phase transitions when pressure changes. Possibly, KBr melts, but not because heat is generated when you apply pressure, but rather because at the high pressure and room temperature, KBr is a liquid. (However, googling for a few minutes I can't find a reliable references quickly that supports that KBr actually melts. Some sites say that it becomes plastic) so whether that is really true in the case of KBr I am not sure (but it is certainly possible for other solid substances).
...


I believe the phenomenon you are looking for is plastic deformation - the pressure exceeds the yield point for the substance and it flows, even though it is still fully solid.