antimon
Harmless
Posts: 33
Registered: 24-6-2015
Member Is Offline
Mood: No Mood
|
|
Anybody know of colloidal magnet?
I saw a patent on a permanent magnet motor that used a solution of colloidal neodynium magnet in the design.
Have i gotten this backwards, or did the motor benefit from the liquid magnet solution?
|
|
j_sum1
Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 6256
Registered: 4-10-2014
Location: Unmoved
Member Is Offline
Mood: Organised
|
|
Can you link to the patent?
|
|
antimon
Harmless
Posts: 33
Registered: 24-6-2015
Member Is Offline
Mood: No Mood
|
|
Sorry it took so long. I don´t have a link to the patent, but here is the place i read it.
http://www.free-energy-info.co.uk/Chapter1.pdf
Thanks for the interest.
|
|
MrHomeScientist
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1806
Registered: 24-10-2010
Location: Flerovium
Member Is Offline
Mood: No Mood
|
|
This almost certainly refers to ferrofluid, not a "suspension of magnets".
It also almost certainly is complete nonsense. If the URL didn't give it away, on the first page it states that a magnet "polarises the quantum
environment surrounding it". Throw enough big words around and people will believe anything.
|
|
IrC
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2710
Registered: 7-3-2005
Location: Eureka
Member Is Offline
Mood: Discovering
|
|
The PDF you provided is one chapter from a book found using a simple search as PJKbook.pdf, “Practical Guide to Free-Energy Devices”. It is a
compilation of many devices by various inventors. Having never seen the fluid you describe, from the description it is not a Ferrofluid, but rather a
colloidal suspension of small crystal units of NdFeB material which was never subjected to a magnetic pulse common to typical magnets constructed of
such material, then broken up into particles in suspension in nonpolar fluids. Ferrofluid differs in that Fe particles are used instead of NdFeB
crystal units.
In any case the file you uploaded speaks of "ShenHe Wang’s Permanent Magnet Motor", then provides little further information on it. Followed by
going into some conspiracy theory issues followed by listing several magnetic devices unrelated to anything created by ShenHe Wang. Simple searching
reveals ShenHe Wang's patent as CN1218329. Interestingly the patent does not mention the OP's thread title material, using instead terms like
Ferro-Liquid, vibrating fluid, bowl of water. Many discrepancies in the OP's and other descriptions abound, all in all rather confusing to analyze.
Attachment: CN1218329A.pdf (417kB) This file has been downloaded 474 times
For those unable to read the patent:
Attachment: Wang.pdf (3.2MB) This file has been downloaded 559 times
http://rexresearch.com/wang/wang.htm
https://www.youtube.com/watch?v=YiHw-KphoIM
I should add just google “Practical Guide to Free-Energy Devices pdf”. As it was around 49.4 mb I cannot add it here.
[Edited on 1-9-2016 by IrC]
"Science is the belief in the ignorance of the experts" Richard Feynman
|
|
IrC
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2710
Registered: 7-3-2005
Location: Eureka
Member Is Offline
Mood: Discovering
|
|
If you want to study interesting magnetic properties and unusual motors, check out the metal Gadolinium. I was experimenting with various dopants in
glow powders a few years ago and obtained a quantity greater than needed since it is always good to buy too much when it is a great deal. So the bulk
of it sat in storage until I wandered across a video that seemed too oddly curious to not investigate. I had studied its properties but never thought
about a thermal motor. Check it out:
https://www.youtube.com/watch?v=VonUp5Wicwk&feature=play...
I doubt it will ever equal a well designed motor but surely it would make a nice classroom demonstration of a seldom seen magnetic effect.
MAGNETIC GADOLINIUM PROPULSION GENERATOR
Attachment: US20150295469A1.pdf (95kB) This file has been downloaded 421 times
https://en.wikipedia.org/wiki/Gadolinium
Thinking of building a DCM free drinking bird.
https://en.wikipedia.org/wiki/Drinking_bird
![220px-Sipping_Bird.jpg - 12kB 220px-Sipping_Bird.jpg - 12kB](http://www.sciencemadness.org/talk/files.php?pid=434955&aid=47218)
"Science is the belief in the ignorance of the experts" Richard Feynman
|
|
Texium
|
Thread Moved 22-11-2023 at 20:00 |