Author: Subject: Tin Refining/Purification
DeIonizedPlasma
Harmless
*




Posts: 21
Registered: 28-9-2014
Member Is Offline

Mood: No Mood

[*] posted on 18-2-2015 at 17:27
Tin Refining/Purification


So I recently gained access to a copy of the CRC (88th) and had fun looking through the ridiculously specific information (Did you know that the earth loses 10^23 J/Century through radiation of heat into space?). Anyways, I happened to come across a list of low melting point alloys, one of which is Ga-Sn-Zn.

I already have two of these, but tin is something that I don't currently have in the lab. I was unable to find anything referencing the refining of tin here, and the only resource I found was a patent on a method of electrorefining that I would rather not spend the time to build. In this case, is there any way to make or obtain relatively pure tin at home? I don't have any tin cans, and I would think that they aren't pure enough anyways. Any ideas for a starting point that might contain tin in any form would be helpful.
View user's profile View All Posts By User
WGTR
National Hazard
****




Posts: 972
Registered: 29-9-2013
Location: Online
Member Is Offline

Mood: Outline

[*] posted on 18-2-2015 at 18:05


Lead-free solder is mostly tin, with either 5% antimony or 3% silver, etc. Get the stuff that is solid wire, without the flux inside. Find it in your favourite hardware store, it's used for plumbing.
View user's profile View All Posts By User
Metacelsus
International Hazard
*****




Posts: 2543
Registered: 26-12-2012
Location: Boston, MA
Member Is Offline

Mood: Double, double, toil and trouble

[*] posted on 18-2-2015 at 18:10


You can buy tin ingots online (I bought an 8 oz. one once). Tin is easy to melt down, and can be granulated by dripping small drops into water.



As below, so above.

My blog: https://denovo.substack.com
View user's profile View All Posts By User
Magpie
lab constructor
*****




Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline

Mood: Chemistry: the subtle science.

[*] posted on 18-2-2015 at 18:34


I have bought ingot tin and bismuth off eBay from which I made a low temperature melting eutectic alloy. My purpose was to have a heating bath that could go higher in temperature than silicone oil. It must have been cheaper than Wood's metal or I would have bought that.



The single most important condition for a successful synthesis is good mixing - Nicodem
View user's profile View All Posts By User
gdflp
Super Moderator
*******




Posts: 1320
Registered: 14-2-2014
Location: NY, USA
Member Is Offline

Mood: Staring at code

[*] posted on 18-2-2015 at 18:41


Quote: Originally posted by Magpie  
I have bought ingot tin and bismuth off eBay from which I made a low temperature melting eutectic alloy. My purpose was to have a heating bath that could go higher in temperature than silicone oil.


That's a very intriguing idea. Have you ever had any issues cleaning the outside of the flask afterwards, or does the alloy not wet glass at all?

[Edited on 2-19-2015 by gdflp]
View user's profile View All Posts By User
Magpie
lab constructor
*****




Posts: 5939
Registered: 1-11-2003
Location: USA
Member Is Offline

Mood: Chemistry: the subtle science.

[*] posted on 18-2-2015 at 18:58


I never used it with a glass vessel so can't say. The picture below shows the bath on the left with the alloy in it. The middle ss vessel was used in the bath for making molten NaOH. The copper crucible was made for the same purpose but I haven't got around to using it yet. Both of the crucibles were silver soldered.

The ss vessels were both made from a martini shaker put to a higher use. ;)

Sn-Bi bath + metal crucibles.jpg - 106kB




The single most important condition for a successful synthesis is good mixing - Nicodem
View user's profile View All Posts By User
vmelkon
National Hazard
****




Posts: 669
Registered: 25-11-2011
Location: Canada
Member Is Offline

Mood: autoerotic asphyxiation

[*] posted on 20-2-2015 at 04:07


I think certain ornaments are made of pure tin. I have one at home but I never tested it to see what it is made of.

I suppose you can buy lead-tin solder (60%-40%).
Dissolve in nitric acid. I assume this makes Sn(2+).
Lead of course will become Pb(2+).
Add a chloride salt like NaCl and PbCl2 precipitates.
You should be able to get tin metal as needle crystals by dunking in a copper wire.




Signature ==== Is this my youtube page? https://www.youtube.com/watch?v=tA5PYtul5aU
We must attach the electrodes of knowledge to the nipples of ignorance and give a few good jolts.
Yes my evolutionary friends. We are all homos here.
View user's profile View All Posts By User
Bert
Super Administrator
*********




Posts: 2821
Registered: 12-3-2004
Member Is Offline

Mood: " I think we are all going to die. I think that love is an illusion. We are flawed, my darling".

[*] posted on 20-2-2015 at 05:32


Rotometals is about as good a deal as you will find for small quantities of 99.9% pure Tin- Prices on most items INCLUDE shipping if order is over $99.00.

http://www.rotometals.com/Tin-Ingot-s/27.htm

They also sell several low melting alloys:

http://www.rotometals.com/Low-Melting-Fusible-Alloys-s/21.ht...

[Edited on 20-2-2015 by Bert]




Rapopart’s Rules for critical commentary:

1. Attempt to re-express your target’s position so clearly, vividly and fairly that your target says: “Thanks, I wish I’d thought of putting it that way.”
2. List any points of agreement (especially if they are not matters of general or widespread agreement).
3. Mention anything you have learned from your target.
4. Only then are you permitted to say so much as a word of rebuttal or criticism.

Anatol Rapoport was a Russian-born American mathematical psychologist (1911-2007).

View user's profile View All Posts By User
papaya
National Hazard
****




Posts: 615
Registered: 4-4-2013
Member Is Offline

Mood: reactive

[*] posted on 20-2-2015 at 06:24


Quote: Originally posted by vmelkon  
I


Dissolve in nitric acid. I assume this makes Sn(2+).

Don't advice things you're not sure!
View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 20-2-2015 at 06:46


Chemical separation of tin and antimony can be achieved as follows.

Dissolve the Sn/Sb alloy in (weakish) Aqua Regia. It dissolves the metals to H<sub>2</sub>SnCl<sub>6</sub> and HSbCl<sub>6</sub>.

Add KCl to the hot solution, dissolve, then allow to cool. K<sub>2</sub>SnCl<sub>6</sub> crystallises out but KSbCl<sub>6</sub> is far too soluble and stays in solution.

From that same mixed solution Sb can also be separated out fom Sn because copper plates out the Sb but not the Sn.




View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 20-2-2015 at 06:51


Quote: Originally posted by vmelkon  
Dissolve in nitric acid. I assume this makes Sn(2+).


It doesn't dissolve in nitric acid: it forms insoluble SnO<sub>2</sub>. It needs HNO3 + HCl. And then it forms hexachloro stannic acid.




View user's profile View All Posts By User
careysub
International Hazard
*****




Posts: 1339
Registered: 4-8-2014
Location: Coastal Sage Scrub Biome
Member Is Offline

Mood: Lowest quantum state

[*] posted on 20-2-2015 at 08:16


Quote: Originally posted by Bert  
Rotometals is about as good a deal as you will find for small quantities of 99.9% pure Tin- Prices on most items INCLUDE shipping if order is over $99.00.

http://www.rotometals.com/Tin-Ingot-s/27.htm

They also sell several low melting alloys:

http://www.rotometals.com/Low-Melting-Fusible-Alloys-s/21.ht...

[Edited on 20-2-2015 by Bert]


They also have "popcorn" tin flake for $20/lb, which should be convenient for doing tin reductions (or for melting into an alloy composition).

http://www.rotometals.com/product-p/tinflakes.htm
View user's profile View All Posts By User
Sulaiman
International Hazard
*****




Posts: 3778
Registered: 8-2-2015
Member Is Offline


[*] posted on 20-2-2015 at 19:32


for me, a cheap source of tin is used lead-free Pewter flatware items (plates, saucers etc.) via eBay.
There may be a few percent Cu and Sb.
Selangor pewter is about 97.5% Sn, 1.5% Sb and 1% Cu.

For 'pure' tin I bought 5 oz. of 99.9% tin for GBP 7.49 incl. p&p via eBay.
Search your local eBay for 'tin 99' or 'tin 99.9'

[Edited on 21-2-2015 by Sulaiman]
View user's profile View All Posts By User
IrC
International Hazard
*****




Posts: 2710
Registered: 7-3-2005
Location: Eureka
Member Is Offline

Mood: Discovering

[*] posted on 20-2-2015 at 22:11


Quote: Originally posted by Magpie  
I have bought ingot tin and bismuth off eBay from which I made a low temperature melting eutectic alloy. My purpose was to have a heating bath that could go higher in temperature than silicone oil. It must have been cheaper than Wood's metal or I would have bought that.


Stick with what you made as Wood's metal is an extremely bad choice for a heating bath. 26.7 % Pb is bad enough as far as toxicity goes. The 10 % Cadmium metal (itself toxic) which will form the very toxic oxide upon heating adds a whole new level of risk.

On the subject of the OP, Sn is so cheap at decent purity on ebay I do not see why one would wish to deal with purifying solder or some other alloy or mix. Just buy the pure metal.

http://www.ebay.com/itm/1-Pound-TIN-metal-Ingot-99-98-pure-B...

One pound for $18.99 with $5.99 shipping.




"Science is the belief in the ignorance of the experts" Richard Feynman
View user's profile View All Posts By User