CHRIS25
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 951
Registered: 6-4-2012
Location: Ireland
Member Is Offline
Mood: No Mood
|
|
Lead impurities
While there is info on the web about impurities in lead I am unable to find any leads (no pun intended) as to the following question:
Needing to make lead nitrate: I am using lab grade nitric acid, but using a lead bullet from 1830 that has been in the ocean for probably same amount
of time. At the moment the lead nitrate solution is milk white, not what I expected, I expected dirty brown, or dirty yellow before filtering . Has
anyone any ideas as to what significant impurity might be causing this?
‘Calcination… is such a Separation of Bodies by Fire, as makes ‘em easily reducible into Powder; and for that reason ‘tis call’d by some
Chymical Pulverization.’ (John Friend, Chymical Lectures London, 1712)
Right is right, even if everyone is against it, and wrong is wrong, even if everyone is for it. (William Penn 1644-1718)
The very nature of Random, Chance development precludes the existence of Order - strange that our organic and inorganic world is so well defined by
precision and law. (me)
|
|
gdflp
Super Moderator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1320
Registered: 14-2-2014
Location: NY, USA
Member Is Offline
Mood: Staring at code
|
|
Most likely, it is tin content in the bullet. Tin doesn't dissolve in nitric acid, it simply oxidizes to insoluble tin oxides. Filtering should
remove this just fine.
|
|
CHRIS25
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 951
Registered: 6-4-2012
Location: Ireland
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by gdflp ![](images/xpblue/lastpost.gif) | Most likely, it is tin content in the bullet. Tin doesn't dissolve in nitric acid, it simply oxidizes to insoluble tin oxides. Filtering should
remove this just fine. |
Ok I never knew that they added Tin to lead when casting the civil war type bullets, (that's what these are), I will do some testing.
‘Calcination… is such a Separation of Bodies by Fire, as makes ‘em easily reducible into Powder; and for that reason ‘tis call’d by some
Chymical Pulverization.’ (John Friend, Chymical Lectures London, 1712)
Right is right, even if everyone is against it, and wrong is wrong, even if everyone is for it. (William Penn 1644-1718)
The very nature of Random, Chance development precludes the existence of Order - strange that our organic and inorganic world is so well defined by
precision and law. (me)
|
|
MrHomeScientist
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1806
Registered: 24-10-2010
Location: Flerovium
Member Is Offline
Mood: No Mood
|
|
Seems a shame to destroy bits of history for chemistry! I think wheel weights are the usual go-to source for lead. I bought an ingot of 99.9% Pb on
eBay.
I think gdflp is correct for the identity of the impurity. Antimony is another common additive, and I believe that also will oxidize to insoluble
oxides. Filter and you should be good to go.
Edit: You should try the golden rain demo with your lead nitrate! It's one of the most beautiful experiments I've ever done.
[Edited on 11-14-2014 by MrHomeScientist]
|
|
CHRIS25
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 951
Registered: 6-4-2012
Location: Ireland
Member Is Offline
Mood: No Mood
|
|
Well I found about 300 of these bullets and just used two that were crushed, so no tears there. Yes, I will to do that golden rain experiment.
Thanks for the pointer.
‘Calcination… is such a Separation of Bodies by Fire, as makes ‘em easily reducible into Powder; and for that reason ‘tis call’d by some
Chymical Pulverization.’ (John Friend, Chymical Lectures London, 1712)
Right is right, even if everyone is against it, and wrong is wrong, even if everyone is for it. (William Penn 1644-1718)
The very nature of Random, Chance development precludes the existence of Order - strange that our organic and inorganic world is so well defined by
precision and law. (me)
|
|
diddi
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 723
Registered: 23-9-2014
Location: Victoria, Australia
Member Is Offline
Mood: Fluorescent
|
|
also consider antimony and bismuth in your list of impurities.
|
|
CHRIS25
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 951
Registered: 6-4-2012
Location: Ireland
Member Is Offline
Mood: No Mood
|
|
Filtering achieved nothing, there was is a fair amount of Tin Oxide layered on the filter paper, but solution is still milk. Plan "B" Take one of my
lead ingots from the beach and re-smelt, and ladle off smaller portions, this stuff has to be better, I already skimmed off much of the impurities
first time round. I don't need pure lead, so 0.5% impurities won't matter for end use.
Ps, don't you guys mean Tin Dioxide, not the SnO?
[Edited on 15-11-2014 by CHRIS25]
‘Calcination… is such a Separation of Bodies by Fire, as makes ‘em easily reducible into Powder; and for that reason ‘tis call’d by some
Chymical Pulverization.’ (John Friend, Chymical Lectures London, 1712)
Right is right, even if everyone is against it, and wrong is wrong, even if everyone is for it. (William Penn 1644-1718)
The very nature of Random, Chance development precludes the existence of Order - strange that our organic and inorganic world is so well defined by
precision and law. (me)
|
|
blogfast25
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by CHRIS25 ![](images/xpblue/lastpost.gif) | Filtering achieved nothing, there was is a fair amount of Tin Oxide layered on the filter paper, but solution is still milk. Plan "B" Take one of my
lead ingots from the beach and re-smelt, and ladle off smaller portions, this stuff has to be better, I already skimmed off much of the impurities
first time round. I don't need pure lead, so 0.5% impurities won't matter for end use.
Ps, don't you guys mean Tin Dioxide, not the SnO?
[Edited on 15-11-2014 by CHRIS25] |
That is a clear indication that it is indeed SnO2 (or at least in part). SnO2 has a tendency to peptise, in plain English: to run through a filter,
especially when freshly prepared. So your tin dioxide is only partly retained on the filter.
You could just let that decant for several days of course: SnO2 is a dense material and will eventually sink to the bottom.
All kinds of impurities in lead artefacts are a common problem for preparing relatively pure lead compounds from them, as others correctly pointed
out. Tin and antimony form their insoluble oxide on treatment with nitric acid, so these have been eliminated mostly. Bismuth does dissolve in nitric
acid, so if there's any there it will be in your solution. Very old lead objects may also contain small amounts of silver, because the two often
accompany each other in ores. If any, it will be in solution.
[Edited on 15-11-2014 by blogfast25]
|
|
CHRIS25
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 951
Registered: 6-4-2012
Location: Ireland
Member Is Offline
Mood: No Mood
|
|
Hallo, good, so I have begun a new reaction with some purified lead (by double refinement). this is not from the bullets, more modern scrap stuff
found on beaches. The tin dioxide is an unexpected pleasure since I have a use for this. Though I am surprised at the amount. 15.6g from 26g of
Lead? So I did three tests:
It is Insoluble in Alcohol
Insoluble in NaOH
InSoluble in water.
Tin Dioxide should have dissolved in the sodium hydroxide but did not.
[Edited on 15-11-2014 by CHRIS25]
‘Calcination… is such a Separation of Bodies by Fire, as makes ‘em easily reducible into Powder; and for that reason ‘tis call’d by some
Chymical Pulverization.’ (John Friend, Chymical Lectures London, 1712)
Right is right, even if everyone is against it, and wrong is wrong, even if everyone is for it. (William Penn 1644-1718)
The very nature of Random, Chance development precludes the existence of Order - strange that our organic and inorganic world is so well defined by
precision and law. (me)
|
|
blogfast25
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
I presume that by 'sodium hydroxide' you mean sodium hydroxide solution?
Whether or not a tin dioxide will dissolve in such a solution is not as straightforward a question as you make out. It depends on:
* age of the Sn(OH)4/SnO2. It ages very quickly and then becomes insoluble in even the strongest NaOH solutions (or strong acids, for that matter).
* How it was prepared (related to the point above). Freshly prepared Sn(OH)4 from acidic SnCl4 solution and ammonia will be reasonably soluble in NaOH
solutions (as well as strong acid solutions).
* SnO2 prepared from treating tin metal with nitric acid is quite inert (insoluble in alkali/acids) in my experience.
So solubility in NaOH solutions is a very, very poor identifier for Sn(OH)4/SnO2.
All SnO2 can be 'dissolved' in molten NaOH, forming sodium stannate. From very alkaline solutions this can be crystallised as
Na<sub>2</sub>Sn(OH)<sub>6</sub> (sodium stannate).
The quantity you're finding seems too high though. But maybe it was effectively a tin/lead alloy?
[Edited on 15-11-2014 by blogfast25]
|
|
CHRIS25
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 951
Registered: 6-4-2012
Location: Ireland
Member Is Offline
Mood: No Mood
|
|
The new batch, (not complete yet), has a crystal clear layer of solution on top of the precipitate, which is brilliant white, still with plenty of
undissolved lead. So this is a good indication of my original refining of the raw lead. Great, at least I am assured of lead nitrate. Since Lead
nitrate is soluble in water but insoluble in nitric acid I think that too much nitric acid evaporated as nitrous oxide and left me with not enough
nitric acid to dissolve the lead even though I added 1 mole of acid to 0.4 moles of lead all in a 7M concentration.
I did some research on an american civil war site but could only find vague references to them casting lead bullets with tin, no percentages given.
But I would, out of sheer curiosity, like to be able to discover the amount of tin/lead ratio that has been used. I could find no references to what
might have been used back in 1860. Although these bullets actually date from 1835 Liverpool England, (long story here).
Working backwards from knowing 15g of tin dioxide, is it possible to calculate amount of tin in this? If tin is 118g/mol and the dioxide is 151g/mol:
15g = 0.1 mol ; therefore 0.1 mol of 118g = 11g tin? but I anticipate my logic to be wrong. This kind of calculating is something I am unfamiliar
with.
‘Calcination… is such a Separation of Bodies by Fire, as makes ‘em easily reducible into Powder; and for that reason ‘tis call’d by some
Chymical Pulverization.’ (John Friend, Chymical Lectures London, 1712)
Right is right, even if everyone is against it, and wrong is wrong, even if everyone is for it. (William Penn 1644-1718)
The very nature of Random, Chance development precludes the existence of Order - strange that our organic and inorganic world is so well defined by
precision and law. (me)
|
|
blogfast25
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by CHRIS25 ![](images/xpblue/lastpost.gif) |
Working backwards from knowing 15g of tin dioxide, is it possible to calculate amount of tin in this? If tin is 118g/mol and the dioxide is 151g/mol:
15g = 0.1 mol ; therefore 0.1 mol of 118g = 11g tin? but I anticipate my logic to be wrong. This kind of calculating is something I am unfamiliar
with.
|
No, the reasoning is correct and would indicate approx. 11/26 x 100 w% = 42 w% tin in your bullet.
Bear in mind that what you did wasn't a precise chemical analysis, so that number is approximate at best. Oxides in analytical chemistry usually
require high temperature glowing to drive off the last bits of moisture for instance.
You seem rather pleased with the SnO2, are you planning to use it for something?
|
|
CHRIS25
National Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 951
Registered: 6-4-2012
Location: Ireland
Member Is Offline
Mood: No Mood
|
|
Ah, a bit of a relief there then, I recognise that it is approximate - but nevertheless a good guide, thanks for the feedback. I am interested in
creating something new involving combining cyanotype and watercolour, but I want to create the pigments myself, I can't let go of the chemistry and
buy them, this would ruin my self imposed insanity; besides this would upset the creative ideas that are brewing. So the tin dioxide and the lead
nitrate are both ingredients in different yellows.
‘Calcination… is such a Separation of Bodies by Fire, as makes ‘em easily reducible into Powder; and for that reason ‘tis call’d by some
Chymical Pulverization.’ (John Friend, Chymical Lectures London, 1712)
Right is right, even if everyone is against it, and wrong is wrong, even if everyone is for it. (William Penn 1644-1718)
The very nature of Random, Chance development precludes the existence of Order - strange that our organic and inorganic world is so well defined by
precision and law. (me)
|
|