Author: Subject: 10 nm silicon nanoparticles for making hydrogen
vmelkon
National Hazard
****




Posts: 669
Registered: 25-11-2011
Location: Canada
Member Is Offline

Mood: autoerotic asphyxiation

[*] posted on 25-6-2014 at 17:43
10 nm silicon nanoparticles for making hydrogen


http://phys.org/news/2013-01-nanosilicon-rapidly-electricity...

Each mol of silicon should produce 2 mol of H2 but the article says they obtained 2.58 mol. How is that possible?




Signature ==== Is this my youtube page? https://www.youtube.com/watch?v=tA5PYtul5aU
We must attach the electrodes of knowledge to the nipples of ignorance and give a few good jolts.
Yes my evolutionary friends. We are all homos here.
View user's profile View All Posts By User
TheChemiKid
Hazard to Others
***




Posts: 493
Registered: 5-8-2013
Location: ̿̿ ̿̿ ̿'̿'̵͇̿̿з=༼ ▀̿̿Ĺ̯̿̿▀̿ ̿ ༽
Member Is Offline

Mood: No Mood

[*] posted on 25-6-2014 at 17:57


I'm not sure how that is possible, I think it might be a mistake, but this is really interesting.



When the police come


\( * O * )/ ̿̿ ̿̿ ̿'̿'̵͇̿̿з=༼ ▀̿̿Ĺ̯̿̿▀̿ ̿ ༽
View user's profile View All Posts By User
Zyklon-A
International Hazard
*****




Posts: 1547
Registered: 26-11-2013
Member Is Offline

Mood: Fluorine radical

[*] posted on 26-6-2014 at 09:28


Weird. Perhaps more than one reaction is occurring [giving rise to different oxidation states or silicon hydroxides, thus a different stoichiometry is involved] - to small extents of course.
It seems like a decent idea, but nano-silicon particles are far too expensive to make for the energy you get out of the cell.
I like the idea of adding a few % of lithium or sodium hydride to catalyze the reaction. That seems beneficial.
Perhaps there would be no need for the particles to be that small if alloyed with alkali hydrides. >100-nm silicon nanoparticles, mixed with 2-5% hydride ions would likely react as fast as the 10-nm pure silicon nanoparticles. [Just a thought]
[EDIT] Never mind, silicon cannot have a higher oxidation state than 4+, so there must be some mistake.




[Edited on 26-6-2014 by Zyklon-A]




View user's profile View All Posts By User
Artemus Gordon
Hazard to Others
***




Posts: 178
Registered: 1-8-2013
Member Is Offline

Mood: No Mood

[*] posted on 26-6-2014 at 12:18


Since Oxygen binds with itself during electrolysis, I'm guessing they are getting some O2 in addition to SiO2.
View user's profile View All Posts By User
blogfast25
International Hazard
*****




Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline

Mood: No Mood

[*] posted on 26-6-2014 at 13:13


Quote: Originally posted by vmelkon  
http://phys.org/news/2013-01-nanosilicon-rapidly-electricity...

Each mol of silicon should produce 2 mol of H2 but the article says they obtained 2.58 mol. How is that possible?


Well spotted. It does seem to be a mistake: Si can never generate more than 2 mol of H2 per mol of Si, no matter what the source of hydrogen is... unless the reaction product behaves catalytically for the splitting of water.




View user's profile View All Posts By User
Morgan
International Hazard
*****




Posts: 1727
Registered: 28-12-2010
Member Is Offline

Mood: No Mood

[*] posted on 26-6-2014 at 17:23


The explanation is somewhat vague to me. Had some of the remaining Si formed a hydride? Or are they saying it was just a bunch of bubbles that weren't dislodged at the initial start of the measurements, giving the experiment a head start so to speak? Or as mentioned is it implying a catalytic bonus? Or was it that the way the nano silicon was manufactured that it contained residual hydrogen that is first released/driven off before the water starts breaking down? There is this chart.
http://bioage.typepad.com/.a/6a00d8341c4fbe53ef017d402119299...
"In addition, the hydrogen generated from the 10 nm silicon exceeds the expected 2 mols of H2 per mole of silicon. They attributed this to to the presence of hydrogen on the surface of the particles remaining from their production in a hydrogen rich environment."
http://www.greencarcongress.com/2013/01/ergbogbo-20130118.ht...

[Edited on 27-6-2014 by Morgan]
View user's profile View All Posts By User

  Go To Top