TEFLON (PTFE) beaker users? Chinese products???
I have been seeing (relatively!) cheap Chinese made? PTFE beakers showing up on eBay recently-
I've never used one. I do understand the need for non reactive beakers with such things as hydroflouric acid and extremely basic materials.
Has anyone used these items? Are they made properly...
(Flagrant racial stereotype driven idiocy on Bert's part removed here)
TEFLON structural materials are fabricated by a powder pressing and sintering process, as far as I recall. I would assume porosity could be a
problem?
If you use such equipment- What do you think of them? And what am I not thinking of, both in terms of real world need for this type of material in lab
processes, and what the drawbacks of these cheap tools may be?
[Edited on 10-4-2014 by Bert]
[Edited on 13-4-2014 by Bert]
Rapopart’s Rules for critical commentary:
1. Attempt to re-express your target’s position so clearly, vividly and fairly that your target says: “Thanks, I wish I’d thought of putting it
that way.”
2. List any points of agreement (especially if they are not matters of general or widespread agreement).
3. Mention anything you have learned from your target.
4. Only then are you permitted to say so much as a word of rebuttal or criticism.
Anatol Rapoport was a Russian-born American mathematical psychologist (1911-2007).
|
|
Zyklon-A
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1547
Registered: 26-11-2013
Member Is Offline
Mood: Fluorine radical
|
|
The first link doesn't work for me, it just sends me to eBay.com. No, I haven't bought one, but I might.
|
|
Varmint
Hazard to Others
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 264
Registered: 30-5-2013
Location: Near Atlanta, GA
Member Is Offline
Mood: No Mood
|
|
My first concern would be thermal conductivity, in both directions.
1). You need a reaction that takes place at an elevated temperature (or are heating up for evaporation), the lower thermal conductivity can present a
problem.
2). You are doing an exothermic reation where you would normally count on an ice bath (or indeed just plain air) to control the temperature. Again,
but in the opposite direction, thermal conductivity can present a problem.
Given those limitations, I'm hard-pressed to think of an application where they would fit my needs. That doesn't mean there aren't any, just that I
don't see it right off the bat.
The presumed immunity to breakage under typical conditions IS attractive, but I'm not sure what kind of premium I'd be willing to pay over
borosilicate for the limited number of applications where the drawbacks don't come into play.
DAS
|
|
Chemosynthesis
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1071
Registered: 26-9-2013
Member Is Offline
Mood: No Mood
|
|
I have seen Teflon used in some pressure applications such as hydrogenation work, digest bombs, autoclaves, and even microwave reactions. I'm not
sure why microwave reactions might prefer Teflon, or why beakers outside the cases you have mentioned, as the microwave accelerated reaction system
and my limited but interesting microwave synthesis days always used glass vessels.
edit- just thought of one possible use, though I know there are others I can't explain... there are microwave digestion bomb methodologies I have
never seen used.
I always thought most uses for non-glass lab ware, outside of HF, was to save money by making it hard to break by dropping, reducing replacement
costs.
[Edited on 10-4-2014 by Chemosynthesis]
|
|
macckone
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2165
Registered: 1-3-2013
Location: Over a mile high
Member Is Offline
Mood: Electrical
|
|
PTFE is not resistant to concentrated hot NaOH. It strips the fluorine
off the polymer leaving a tacky mess of the coating. PTFE will also absorb
HF. But doesn't seem degraded by it. Stainless 316 is better for NaOH.
And nickel is the preferred material for HF. Or at least that is what is
used industrially.
|
|
blogfast25
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
Try and get reasonably priced, smallish size nickelware though...
|
|
macckone
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2165
Registered: 1-3-2013
Location: Over a mile high
Member Is Offline
Mood: Electrical
|
|
Yes, nickle crucibles, 50ml run about $35.
|
|
deltaH
Dangerous source of unreferenced speculation
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 1663
Registered: 30-9-2013
Location: South Africa
Member Is Offline
Mood: Heavily protonated
|
|
On the topic of crucibles, I used to do sodium peroxide fusions of mineral samples for metal assays in zirconium crucibles over a decade ago. They
were tough as nails but cost a pretty penny back then!
Before that we were doing HF digestions, initially in pyrex (simply sacrificing the beakers after a few uses) then later in teflon bombs, but we had
to switch over to the peroxide fusions to quantitatively dissolve up some tougher ore components like chromite if I remember correctly.
For the 'wet' digestions, the Pyrex was suprisingly tough even to the HF, though the beakers were consumables in that lab.
[Edited on 13-4-2014 by deltaH]
|
|
Bert
Super Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2821
Registered: 12-3-2004
Member Is Offline
Mood: " I think we are all going to die. I think that love is an illusion. We are flawed, my darling".
|
|
Thanks everyone, I've learned a few things from this-
Not going to need the PTFE equipment anytime soon, hydroflouric acid is not on my list of reagents I'll be needing for any planned projects.
Rapopart’s Rules for critical commentary:
1. Attempt to re-express your target’s position so clearly, vividly and fairly that your target says: “Thanks, I wish I’d thought of putting it
that way.”
2. List any points of agreement (especially if they are not matters of general or widespread agreement).
3. Mention anything you have learned from your target.
4. Only then are you permitted to say so much as a word of rebuttal or criticism.
Anatol Rapoport was a Russian-born American mathematical psychologist (1911-2007).
|
|
Bert
Super Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2821
Registered: 12-3-2004
Member Is Offline
Mood: " I think we are all going to die. I think that love is an illusion. We are flawed, my darling".
|
|
I am pretty happy with the information on less reactive/non glassware vessels this thread generated.
Thanks again, everyone!
If their is an additional side discussion of interest to the members on the intersection of laboratory GLASS, quality control, marketing
practices, societal or cultural perceptions vs. actual norms- AND IF IT's RELEVANT TO AMATEUR CHEMISTRY- Let's start that up on Legal &
Societal.
If it goes there, Keep it clean, stick to personal experience & verifiable incidents and no ad hominem...
Rapopart’s Rules for critical commentary:
1. Attempt to re-express your target’s position so clearly, vividly and fairly that your target says: “Thanks, I wish I’d thought of putting it
that way.”
2. List any points of agreement (especially if they are not matters of general or widespread agreement).
3. Mention anything you have learned from your target.
4. Only then are you permitted to say so much as a word of rebuttal or criticism.
Anatol Rapoport was a Russian-born American mathematical psychologist (1911-2007).
|
|
blogfast25
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by Bert ![](images/xpblue/lastpost.gif) | If their is an additional side discussion of interest to the members on the intersection of laboratory GLASS, quality control, marketing practices,
societal or cultural perceptions vs. actual norms- AND IF IT's RELEVANT TO AMATEUR CHEMISTRY- Let's start that up on Legal & Societal.
If it goes there, Keep it clean, stick to personal experience & verifiable incidents and no ad hominem... |
That could be useful, as well as interesting.
[Edited on 13-4-2014 by blogfast25]
|
|
Bert
Super Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2821
Registered: 12-3-2004
Member Is Offline
Mood: " I think we are all going to die. I think that love is an illusion. We are flawed, my darling".
|
|
I removed whatever seemed not relevant to the discussion of PTFE and other non glass containers and their uses.
Their will be an even handed, documented fact & evidence based discussion on Legal & Societal regarding equipment sources and quality control
issues.
Rapopart’s Rules for critical commentary:
1. Attempt to re-express your target’s position so clearly, vividly and fairly that your target says: “Thanks, I wish I’d thought of putting it
that way.”
2. List any points of agreement (especially if they are not matters of general or widespread agreement).
3. Mention anything you have learned from your target.
4. Only then are you permitted to say so much as a word of rebuttal or criticism.
Anatol Rapoport was a Russian-born American mathematical psychologist (1911-2007).
|
|
blogfast25
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by Bert ![](images/xpblue/lastpost.gif) | I removed whatever seemed not relevant to the discussion of PTFE and other non glass containers and their uses.
|
I'm not sure blatantly removing people's posts (or parts of it) is going to please many: they put work into putting those texts up. Surgical removal
to 'Detritus' is the usual procedure for stuff that is deemed irrelevant/unsuitable to a thread.
|
|
Bert
Super Administrator
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2821
Registered: 12-3-2004
Member Is Offline
Mood: " I think we are all going to die. I think that love is an illusion. We are flawed, my darling".
|
|
I watched a thread deteriorate into a borderline flame war, with several who should know better spending a lot of words on having the last
word, regardless of the thread's original purpose. The only thing being learned was that smart people will get stupid and argue on the
internet.
Tried offering an alternative to this sideshow, in an appropriate place for the derail's subject. Got no traction, you may have missed a few things I
deleted. I certainly hope you did.
People may hate me if they feel slighted by my actions in maintaining what semblence of order I can here. I will just have to deal with that somehow.
Look at the history of active moderation here, and quality of threads generated vs. level of scrutiny and moderator activity. Would you rather there
was none?
I will leave any answer you care to make here and say no more. As a peace offering, please have the last word.
Rapopart’s Rules for critical commentary:
1. Attempt to re-express your target’s position so clearly, vividly and fairly that your target says: “Thanks, I wish I’d thought of putting it
that way.”
2. List any points of agreement (especially if they are not matters of general or widespread agreement).
3. Mention anything you have learned from your target.
4. Only then are you permitted to say so much as a word of rebuttal or criticism.
Anatol Rapoport was a Russian-born American mathematical psychologist (1911-2007).
|
|
macckone
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 2165
Registered: 1-3-2013
Location: Over a mile high
Member Is Offline
Mood: Electrical
|
|
As a last word from a post that was removed.
Everyone should be cautious with pyrex branded beakers.
Some are borosilicate, some are not.
And this is legitimate pyrex trademarked ware.
After corning sold off the brand name the new
maker no longer uses borosilicate for most products.
http://www.snopes.com/food/warnings/pyrex.asp
|
|
blogfast25
International Hazard
![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif) ![*](images/xpblue/star.gif)
Posts: 10562
Registered: 3-2-2008
Location: Neverland
Member Is Offline
Mood: No Mood
|
|
Quote: Originally posted by Bert ![](images/xpblue/lastpost.gif) |
Look at the history of active moderation here, and quality of threads generated vs. level of scrutiny and moderator activity. Would you rather there
was none?
|
My point was merely that posts are rarely deleted, rather they are usually moved to detritus. Nothing else. I have no problem with moderation per se.
|
|