Electrolysis of Sodium chlorde with aluminum electrodes


I did an electrolysis of saltwith aluminum electrodes with a 9-volt battery and I got a white powdery substance on the negate electrode and at the bottom of the vessel in which I performed the electrolysis, is that aluminum hydroxide or aluminum oxide?

[Edited on 30-11-2013 by shaheerniazi]
View user's profile Visit user's homepage View All Posts By User
bismuthate
National Hazard
****




Posts: 803
Registered: 28-9-2013
Location: the island of stability
Member Is Offline

Mood: self reacting

[*] posted on 30-11-2013 at 05:04


Was it molten?



I'm not a liar, I'm just an enthusiastic celebrant of opposite day.
I post pictures of chemistry on instagram as bismuthate. http://iconosquare.com/bismuthate
or this viewer if you don't have an instagram (it sucks though) http://web.stagram.com/n/bismuthate
View user's profile Visit user's homepage View All Posts By User
shaheerniazi
Hazard to Self
**




Posts: 70
Registered: 25-11-2013
Location: Pakistan
Member Is Offline

Mood: radioactive

[*] posted on 30-11-2013 at 05:15


Oops Sorry! forgot to mention it was a solution.
View user's profile Visit user's homepage View All Posts By User
bismuthate
National Hazard
****




Posts: 803
Registered: 28-9-2013
Location: the island of stability
Member Is Offline

Mood: self reacting

[*] posted on 30-11-2013 at 05:32


It might be sodium aluminate formed by the reaction of (NaOH) with Al

[Edited on 30-11-2013 by bismuthate]




I'm not a liar, I'm just an enthusiastic celebrant of opposite day.
I post pictures of chemistry on instagram as bismuthate. http://iconosquare.com/bismuthate
or this viewer if you don't have an instagram (it sucks though) http://web.stagram.com/n/bismuthate
View user's profile Visit user's homepage View All Posts By User
shaheerniazi
Hazard to Self
**




Posts: 70
Registered: 25-11-2013
Location: Pakistan
Member Is Offline

Mood: radioactive

[*] posted on 30-11-2013 at 05:38


It has a grayish wight colour
View user's profile Visit user's homepage View All Posts By User
shaheerniazi
Hazard to Self
**




Posts: 70
Registered: 25-11-2013
Location: Pakistan
Member Is Offline

Mood: radioactive

[*] posted on 30-11-2013 at 05:40


Wikipedia says it is soluble in water and my powder is making a suspension in water.
View user's profile Visit user's homepage View All Posts By User
homeIandsecurity
Banned: Another incarnation of PhDChemist





Posts: 11
Registered: 30-11-2013
Member Is Offline

Mood: ready to put somebody in jail today

[*] posted on 30-11-2013 at 06:03




It is Aluminium Hydroxide, with Al metal impurities.

[Edited on 30-11-2013 by homeIandsecurity]




HOMELANDSECURITY@INTERPOL.US
View user's profile View All Posts By User
bismuthate
National Hazard
****




Posts: 803
Registered: 28-9-2013
Location: the island of stability
Member Is Offline

Mood: self reacting

[*] posted on 30-11-2013 at 06:04


Ahh it's insoluble. I suspect impurities..
homeland security, wouldn't Al(OH)3 be attacked by the NaOH produced?

[Edited on 30-11-2013 by bismuthate]




I'm not a liar, I'm just an enthusiastic celebrant of opposite day.
I post pictures of chemistry on instagram as bismuthate. http://iconosquare.com/bismuthate
or this viewer if you don't have an instagram (it sucks though) http://web.stagram.com/n/bismuthate
View user's profile Visit user's homepage View All Posts By User
homeIandsecurity
Banned: Another incarnation of PhDChemist





Posts: 11
Registered: 30-11-2013
Member Is Offline

Mood: ready to put somebody in jail today

[*] posted on 30-11-2013 at 06:07


Quote: Originally posted by bismuthate  
Ahh it's insoluble. I suspect impurities..


It can't be aluminate...because it only occurs in basic solution...but Sodium Chloride in his case did not smell like Chlorine, meaning did not release any Chlorine.

Sodium Chloride isn't involved in any reaction there. Only water - Hydrogen hydroxide reacts with Al.
Only this:
H+ -> (H)
Al -> Al(3+)

[Edited on 30-11-2013 by homeIandsecurity]




HOMELANDSECURITY@INTERPOL.US
View user's profile View All Posts By User
shaheerniazi
Hazard to Self
**




Posts: 70
Registered: 25-11-2013
Location: Pakistan
Member Is Offline

Mood: radioactive

[*] posted on 30-11-2013 at 06:37


Thanks guys! I am now labeling i with surety!
View user's profile Visit user's homepage View All Posts By User
homeIandsecurity
Banned: Another incarnation of PhDChemist





Posts: 11
Registered: 30-11-2013
Member Is Offline

Mood: ready to put somebody in jail today

[*] posted on 30-11-2013 at 06:42


Quote: Originally posted by shaheerniazi  
Thanks guys! I am now labeling i with surety!


Just filter that powder to separate all soluble chemicals and dry. Then, put it in HCl acid for test. If releases even one small bubble, you can be sure impurity is Al metal.




HOMELANDSECURITY@INTERPOL.US
View user's profile View All Posts By User
shaheerniazi
Hazard to Self
**




Posts: 70
Registered: 25-11-2013
Location: Pakistan
Member Is Offline

Mood: radioactive

[*] posted on 30-11-2013 at 06:52


Yes! when I did the electrolysis small flakes of aluminium foil did some contamination of it.
View user's profile Visit user's homepage View All Posts By User
homeIandsecurity
Banned: Another incarnation of PhDChemist





Posts: 11
Registered: 30-11-2013
Member Is Offline

Mood: ready to put somebody in jail today

[*] posted on 30-11-2013 at 06:57


Have you noticed this...VERY INTERESTING!

Your foil will be transparent on some parts after electrolysis. I always thought, that is some thin plastic over it...like nylon...but guess what is it?




HOMELANDSECURITY@INTERPOL.US
View user's profile View All Posts By User
shaheerniazi
Hazard to Self
**




Posts: 70
Registered: 25-11-2013
Location: Pakistan
Member Is Offline

Mood: radioactive

[*] posted on 30-11-2013 at 07:11


Hmm, You tell, I have no idea.
View user's profile Visit user's homepage View All Posts By User
homeIandsecurity
Banned: Another incarnation of PhDChemist





Posts: 11
Registered: 30-11-2013
Member Is Offline

Mood: ready to put somebody in jail today

[*] posted on 30-11-2013 at 07:20


TRANSPARENT OR INVISIBLE ALUMINIUM.

I am right now doing electrolysis and will post a new thread called TRANSPARENT/INVISIBLE ALUMINIUM with picture in beginnings!




HOMELANDSECURITY@INTERPOL.US
View user's profile View All Posts By User
shaheerniazi
Hazard to Self
**




Posts: 70
Registered: 25-11-2013
Location: Pakistan
Member Is Offline

Mood: radioactive

[*] posted on 30-11-2013 at 07:27


Cool, but This never happened to my alluminum, will it work with water electrolysis with aluminum electrodes?
View user's profile Visit user's homepage View All Posts By User
shaheerniazi
Hazard to Self
**




Posts: 70
Registered: 25-11-2013
Location: Pakistan
Member Is Offline

Mood: radioactive

[*] posted on 30-11-2013 at 07:29


In the internet it says its aluminium oxynitride?
View user's profile Visit user's homepage View All Posts By User
homeIandsecurity
Banned: Another incarnation of PhDChemist





Posts: 11
Registered: 30-11-2013
Member Is Offline

Mood: ready to put somebody in jail today

[*] posted on 30-11-2013 at 08:11


Yes...it must be foil (even from chocolate is possible).

You must have sodium chloride...water alone doesn't work.

No, Al oxynitride is formed when burning aluminium in air.




HOMELANDSECURITY@INTERPOL.US
View user's profile View All Posts By User
shaheerniazi
Hazard to Self
**




Posts: 70
Registered: 25-11-2013
Location: Pakistan
Member Is Offline

Mood: radioactive

[*] posted on 30-11-2013 at 08:17


When I burn it in air then it forms a white powder which is aluminium oxide, and I used the aluminium foil from the kitchen which is used for packing and when I did it then it formed a white crystaline powder on my foil, let me show you wait.
View user's profile Visit user's homepage View All Posts By User
shaheerniazi
Hazard to Self
**




Posts: 70
Registered: 25-11-2013
Location: Pakistan
Member Is Offline

Mood: radioactive

[*] posted on 30-11-2013 at 08:26



View user's profile Visit user's homepage View All Posts By User
homeIandsecurity
Banned: Another incarnation of PhDChemist





Posts: 11
Registered: 30-11-2013
Member Is Offline

Mood: ready to put somebody in jail today

[*] posted on 30-11-2013 at 08:55


Yes.
Al oxynitride is formed only when burning it in limited amount of air. Here is how to test: Just put it in water...if it smells like ammonia gas then you have some nitride also.

Did you burn it in stove or just with flame?




HOMELANDSECURITY@INTERPOL.US
View user's profile View All Posts By User
shaheerniazi
Hazard to Self
**




Posts: 70
Registered: 25-11-2013
Location: Pakistan
Member Is Offline

Mood: radioactive

[*] posted on 30-11-2013 at 09:11


I used a stove.
View user's profile Visit user's homepage View All Posts By User
bfesser
Resident Wikipedian
*****




Posts: 2114
Registered: 29-1-2008
Member Is Offline

Mood: No Mood

[*] posted on 30-11-2013 at 10:22


Quote: Originally posted by homeIandsecurity  
Yes...it must be foil (even from chocolate is possible).
It's plastic (or another non-metallic thin film coating on the foil)! <img src="http://clipartist.info/Art/April/facepalm_facepalm-999px.png" width="14" alt="facepalm" />

[Edited on 30.11.13 by bfesser]




View user's profile View All Posts By User
woelen
Super Administrator
*********




Posts: 7988
Registered: 20-8-2005
Location: Netherlands
Member Is Offline

Mood: interested

[*] posted on 30-11-2013 at 12:32


@shaheerniazi: Do not reply to homeIandsecurity anymore. He is fooling you into all kind of stupid things and has fun of your confusion. He is a troll.




The art of wondering makes life worth living...
Want to wonder? Look at https://woelen.homescience.net
View user's profile Visit user's homepage View All Posts By User
Zyklon-A
International Hazard
*****




Posts: 1547
Registered: 26-11-2013
Member Is Offline

Mood: Fluorine radical

[*] posted on 30-11-2013 at 13:13


Quote: Originally posted by bismuthate  
Was it molten?

If NaCl was molten the aluminum would also melt.